The SEM images of Ce0.8La0.2O2 nanocatalyst infiltrated with 10wt.% Ni prepared using soft template method
Opis
The dataset includes SEM images of Ce0.8La0.2O2-s nanopowder (nanoparticles) prepared using soft template method and infiltrated to 10wt.% Ni in the catalyst. CTAB was used as a micelle-based templating agent. The powder was precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitate was heated up to 90oC, centrifuged and washed several times. The powders were calcined at 400oC. Powder was single-phase.
The Ni was introduced using nitrate solution (Ni(NO3)2*6H2O)) in water with the addition of beta-cyclodextrin.
Plik z danymi badawczymi
Ce0.8La0.2O2 SEM 10wt.%Ni.zip
16.9 MB,
S3 ETag
4e9c7321db53bb37bcb171e8cb08dbc1-1,
pobrań: 47
Hash pliku liczony jest ze wzoru
Przykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
hexmd5(md5(part1)+md5(part2)+...)-{parts_count}
gdzie pojedyncza część pliku jest wielkości 512 MBPrzykładowy skrypt do wyliczenia:
https://github.com/antespi/s3md5
Informacje szczegółowe o pliku
- Licencja:
-
otwiera się w nowej karcieCC BY-NCUżycie niekomercyjne
- Dane surowe:
- Dane zawarte w datasecie nie zostały w żaden sposób przetworzone.
Informacje szczegółowe
- Rok publikacji:
- 2021
- Data zatwierdzenia:
- 2021-06-10
- Data wytworzenia:
- 2020
- Język danych badawczych:
- angielski
- Dyscypliny:
-
- inżynieria materiałowa (Dziedzina nauk inżynieryjno-technicznych)
- DOI:
- Identyfikator DOI 10.34808/nm9t-f324 otwiera się w nowej karcie
- Finansowanie:
- Weryfikacja:
- Politechnika Gdańska
Słowa kluczowe
Powiązane zasoby
- dane badawcze The XRD diffraction patterns of Ce0.8La0.2O2/Ni prepared using soft template method and impregnation
Cytuj jako
Autorzy
wyświetlono 97 razy