Wyniki wyszukiwania dla: CHEMICAL COMPOSITION

  • X-Ray photoemission spectroscopy measurements of the Nb-V-Sr-O ceramics

    Dane Badawcze
    open access

    Niobium doped strontium vanadate based perovskite SrV1-xNbxO3-δ materials were prepared via conventional solid state reaction (SSR) method. For comparison, different samples with a various amount of niobium dopant in the structure were synthesized; x = 0; 0,2; 0,5; 0,8 and 1. Samples were sintered by two-steps: first under a pure hydrogen (purity >99.999%)...

  • XPS analysis of the GO based materials

    Dane Badawcze
    open access

    Graphene oxides samples were measured by XPS method. The X-ray photoemission spectroscopy measurements were carried out with Omicron NanoTechnology UHV equipment. The hemispherical spectrophotometer was equipped with a 128-channel collector. The XPS measurements were performed at room temperature at a pressure below 1.1 × 10−8 mBar. The photoelectrons...

  • Depth XPS profile of Fe-S layers on a titanium substrate

    Dane Badawcze
    open access

    Depth XPS profile of Fe-S layers on a titanium substrate was measured. Material was etched by Argon ion gun and measured by XPS method. For each sample, three times per 10 minutes each was sputtered.

  • Hydrogenation process ofTiO2/BiVO4/PEDOT:PSS observed by XPS method

    Dane Badawcze
    open access

    Titania nanotubes synthesis was based on a two-stage anodization process at water/ethylene glycol (5%/95%) electrolyte containing 0.27 M NH4F and 1 M H3PO4 described previously. Anodization process was performed in two-electrode cell compartment using platinum mesh as a cathode. The distance between electrodes was about 2 cm. The anodization voltage...

  • Detection of the Ag nanoparticles in Te-Bi-Ba-Oa glass

    Dane Badawcze
    open access

    The influence of the manufacturing parameters of tellurium-bismuth-barium glasses on the presence of silver nanoparticles was investigated. Glasses were annealed at 330, 335, 340, 345 and 350 degrees Celsius for 24 and 48 hours. Presence of the Ag nanoparticles was measured by XPS method. The growth of nanoparticles was observed along with the extension...