XRD-TiO2 heat-treated at 400-600oC in Ar or H2
Dane BadawczeThese data contain XRD patterns of TiO2 heat-treated at 400-600oC in Ar or H2. Two pases of TiO2 were identified: anatase and rutile.
-
The morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with AFM
Dane BadawczeThe morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses was measured with the use of atomic force microscope.
-
The dataset of coupling coefficients for rotating receiver of multicoil dynamic wireless power transfer system
Dane BadawczeThe provided dataset is part of the simulation results shown in related journal paper "Optimal Rotating Receiver Angles Estimation for Multicoil Dynamic Wireless Power Transfer".
-
Measurements of the heat of hydration released by concrete specimens cured under adiabatic conditions
Dane BadawczeThe DataSet contains measurements of heat of hydartion of concrete cubes (150 x 150 x 150 mm) cured under adiabatic conditions. The specimens were moulded from six types of concrete mixtures produced in the laboratory conditions. Mix #1: Portland cement CEM I 42.5R and gravel aggregate, mix #2: CEM I 42.5R and basalt aggregate, mix#3: Portland-composite...
-
The topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope
Dane BadawczeThe topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope.
-
The dataset of simulations for optimal and non-optimal rotating receiver angles of multicoil dynamic wireless power transfer system
Dane BadawczeThe provided dataset is part of the simulation results shown in related journal paper "Optimal Rotating Receiver Angles Estimation for Multicoil Dynamic Wireless Power Transfer".
-
The topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with AFM
Dane BadawczeThe topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with AFM.
-
The topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with confocal microscope
Dane BadawczeThe topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with confocal microscope.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at low temperatures
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Effect of particle size of aluminosilicate microspheres on the change of hydration heat of cement mortars and selected physical, chemical, and mechanical properties.
Dane BadawczeThis subject of the work is the study of selected properties of cement mortars containing two fractions of aluminosilicate microspheres with grain size in the range of 125 to 250 μm and from 250 to 500 μm. Mortar mixtures with ordinary Portland cement (OPC 42.5R) and three substitution rates of cement by microspheres, 1.5%, 3.5%, and 5.0%, were investigated....
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at 273 K
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 613 K was measured by impedance spectroscopy method.