  • Results after grinding C45 steel

    The database contains results from nanoindenter, scanning microscope and also X-ray diffractometer. To determine the residual stresses and the size of the crystallites in the ferrite grains in the grinded surface layer, the Williamson Hall analysis of the X-ray diffraction patterns was performed. XRD diffraction patterns were also used to perform a...

  • Scanning electron microscopy studies of the weld decay on SS 304 of water supply pipeline

    Dane Badawcze
    open access

    This dataset contains micrographs made with scanning electron microscope (SEM) Hitachi S-3400N, of the weld decay for water supply system pipelines made of AISI 304 stainless steel. Within the dataset one can see the different corrosion mechanisms. The micrographs were made after the Strauss test (excluding pictures labeled as pits_in_HAZ, done without...

  • Maximum temperature of 0.5-W infrared laser-Illuminated gold nanorod platforms

    Dane Badawcze

    Data concern a system consisted of two pieces of borosilicate glass surrounded by air and joined together by a transparent glue, which is to serve as a thermal transducer. On the top and bottom sides of the smaller piece, gold nanorods are dislocated. Glass is prepared here due to its high transparency, facilitating heat to be produced within the system....

  • The morphology of vanadate glass-ceramics containing BaTiO3

    Dane Badawcze
    open access

    The morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...