Filtry
wszystkich: 569
wybranych: 123
Wyniki wyszukiwania dla: NANOFLUIDS, PLATE HEAT EXCHANGER, WILSON METHOD
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at low temperatures
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at 273 K
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 613 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm (after second heat-treatment at 913 K) was measured at high temperature range with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm (after second heat-treatment at 913 K) was measured by impedance spectroscopy method.
-
Analytical and reliability data from the real-time simulator biogas plant
Dane BadawczeThe dataset represents the results of biogas plant simulation. The described plant is an agricultural biogas system, which can produce electrical energy with power estimated up to 1070 kW and heat energy that can reach 1200 kW simultaneously.
-
Testing an evaporator operation with a concave manifold, condenser temperature 30, evaporator temperature 70 and preheater temperature 60
Dane BadawczeThe experiment was conducted to test the evaporator operation. The heat exchanger was equipped with minigeometry (set of 50 parallel minichannels or single minigap). The studies were conducted for various mass flow rate of the working fluid and for various temperatures at the inlet of the evaporator. Accurate information about the test rig, the parameters...
-
Testing an evaporator operation with a bifurcation manifold, condenser temperature 20 and evaporator temperature 85
Dane BadawczeThe experiment was conducted to test the evaporator operation. The heat exchanger was equipped with minigeometry (set of 50 parallel minichannels or single minigap). The studies were conducted for various mass flow rate of the working fluid and for various temperatures at the inlet of the evaporator. Accurate information about the test rig, the parameters...