The XRD diffraction patterns of as-prepared (La0.3Sr0.6Ce0.1)0.9FexMeyTi(1-x-y)O3-δ materials (Me=Ni,Co)
Dane BadawczeThe (La0.3Sr0.6Ce0.1)0.9FexMeyTi(1-x-y)O3-δ materials (Me=Ni,Co) were synthesized via the Pechini method. First, the reagents in the form of nitrates were weighed and dissolved in DI water. In another beaker, a stoichiometric amount of titanium (IV) butoxide (Ti(OBu)4) was mixed together with reagent-grade ethylene glycol (EG), and citric acid (CA)...
-
The 2p XPS spectra of transition metals in Ce0.9M0.1O2
Dane BadawczeThe dataset consists of 2p XPS spectra of transition metals in Ce0.9M0.1O2 where (M=Mn, Fe, Co, Ni, Cu). X-ray Photoelectron Spectroscopy analysis (XPS) was performed using X-ray photoelectron spectrometer Omnicron NanoTechnology with 128-channel collector. XPS measurements were undertaken in ultra-high vacuum conditions, below 1.1x10-8 mbar. Photoelectrons...
-
The XRD diffraction patterns of annealed Ce0.9M0.1O2 powders prepared using the reverse microemulsion method
Dane BadawczeThe dataset includes XRD patterns of Ce0.9M0.1O2 (where M=Mn, Fe, Co, Ni, Cu) nanopowders prepared using the reverse microemulsion method. The powders were precipitated from organic-based solution of nitrates using TMAOH. The sediment was cetrifuged and rinsed with alcohol several times. Powders were dried and calcinated at 500 degrees for 2 h, followed...
-
FTIR spectra of gas mixtures from the process of biogas dry reforming using CLO catalyst
Dane BadawczeThe dataset contains the FTIR spectra collected during the catalytic measurements of dry reforming of biogas (60/40 CH4-CO2) using Ce0.8La0.2O2 nanocatalyst. The specatra were collected every 1 minute.
-
The SEM images of LSCNT reduced at 900 degrees C under H2
Dane BadawczeThe dataset includes SEM image of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 900oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The TEC measurement of LSCNT (dilatometry) in air
Dane BadawczeThe dataset includes dilatometry results for La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s measured in air from 100 to 800C using Netzsch DIL 402 PC.
-
The SEM images of LSCNT sintered at 1200 degrees C in air
Dane BadawczeThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h. Samples were produced using aqueous soft chemistry methods (Pechini). The grain structure can be seen on higher resolution image.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1W0.9O3-s precursor calcined under air atmosphere
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1W0.9O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
FTIR spectra of gas mixtures from the process of biogas dry reforming using alumina catalyst - blank
Dane BadawczeThe dataset contains the FTIR spectra collected during the catalytic measurements of blank sample Al2O3 for dry reforming of biogas (60/40 CH4-CO2). The specatra were collected every 1 minute.
-
The XRD diffraction patterns of reduced LSCNT prepared using two methods and two sintering temperatures
Dane BadawczeThe dataset includes XRD diffraction patterns of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s produced using two methods, namely organic (citrate assisted) and Pechini sintered at 1000 or 1200oC under air atmosphere and reduced at 900 for 12 h in wet H2.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s precursor calcined under air atmosphere
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
The XRD diffraction patterns of Ce0.8La0.2O2 and CeO2 prepared using soft template method
Dane BadawczeThe dataset includes XRD patterns of Ce0.8La0.2O2-s and CeO2-s nanopowders (nanoparticles) prepared using soft template method. CTAB was used as a micelle-based templating agent. The powders were precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitates were heated up to 90oC, centrifuged...
-
The XRD diffraction patterns of LSCNT of different A site nonstoichiometry
Dane BadawczeThe dataset includes XRD diffraction patterns of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s and La0.3Sr0.6Ce0.1Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The SEM images of LSCNT reduced at 800 degrees C under H2
Dane BadawczeThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 800oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1W0.45Mo0.45O3-s precursor calcined under air atmosphere
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1W0.45Mo0.45O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
The SEM images of Ce0.8La0.2O2 nanopowder prepared using soft template method
Dane BadawczeThe dataset includes SEM images of Ce0.8La0.2O2-s nanopowder (nanoparticles) prepared using soft template method. CTAB was used as a micelle-based templating agent. The powder was precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitate was heated up to 90oC, centrifuged and washed...
-
The XPS spectra of Ce0.8Ni0.2O2 prepared using microemulsion method
Dane BadawczeThe dataset includes XPS spectra of Ce0.8Ni0.2O2-s sintered under air atmosphere. Samples were produced using aqueous soft chemistry methods (microemulsion). The XPS spectra were collected for all species.
-
The XRD diffraction patterns of Ce0.8La0.2O2/Ni prepared using soft template method and impregnation
Dane BadawczeThe dataset includes XRD patterns of Ce0.8La0.2O2-s nanopowders (nanoparticles,nanocatalyst) prepared using soft template method and further impregnated with 10wt.%Ni using aqueous nitrate solution.
-
FTIR spectra of gas mixtures from the process of biogas dry reforming using CLO/Cu catalyst
Dane BadawczeThe dataset contains the FTIR spectra collected during the catalytic measurements of dry reforming of biogas (60/40 CH4-CO2) using Ce0.8La0.2O2+10wt.%Cu nanocatalyst. The specatra were collected every 1 minute.
-
The SEM images of CeO2 nanopowder prepared using soft template method
Dane BadawczeThe dataset includes SEM images of CeO2-s nanopowder (nanoparticles) prepared using soft template method. CTAB was used as a micelle-based templating agent. The powder was precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitate was heated up to 90oC, centrifuged and washed several...