Experimental tuning of AuAg nanoalloy plasmon resonances assisted by machine learning method
PublikacjaPlasmonic nanostructures based on AuAg nanoalloys were fabricated by thermal annealing of metallic films in an argon atmosphere. The nanoalloys were chosen because they can extend the wavelength range in which plasmon resonance occurs and thus allow the design of plasmonic platforms with the desired parameters. The influence of initial fabrication parameters and experimental conditions on the formation of nanostructures was investigated....
-
Measurements of AuAg nanostructures
Dane BadawczeExtensive UV-vis measurements of AuAg alloyed nanostructures created from thin films. Plasmonic band position dependence on fabrication parameters.
-
Processed measurements of AuAg nanostructures
Dane BadawczeExtensive processed UV-vis measurements of AuAg alloyed nanostructures created from thin films. Plasmonic band position dependence on fabrication parameters.
-
Raw data of AuAg nanoalloy plasmon resonances used for machine learning method
Dane BadawczeRaw data used for machine learning process. UV-vis measurements of AuAg alloyed nanostructures created from thin films. Plasmonic band position dependence on fabrication parameters. Small presentation reviewing achieved structures and their properties.
-
TEM imaging of Ag-Au nanoalloys
Dane BadawczeThe nanostructures of AuAg nanoalloys were prepared by sequential sputtering of metal thin layers (Au/Ag or Ag/Au) followed by annealing under 550 Celsius degree in an argon atmosphere. The basic single layer thickness was usually ca. 3 nm. For investigations two samples wih 50% Au and 50% Ag were selected and samples 1/3 Ag - 2/3 Au and 2/3 Ag - 1/3...
-
Chemical analysis of the Au-Ag nanoaloys
Dane BadawczeThe nanostructures of AuAg nanoalloys were prepared by sequential sputtering of gold and silver thin films. Single layer thickness was usually 2.8 nm were deosted by magnetron sputtering method in a Ar plasma. As deposited layers were annealed in Ar atmosphere at 550 degress for 15 minutes. For XPS measurements five samples were selected: pure gold...