Wyniki wyszukiwania dla: SOFC
-
The SEM images of LSCNT reduced at 800 degrees C under H2
Dane BadawczeThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 800oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1W0.45Mo0.45O3-s precursor calcined under air atmosphere
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1W0.45Mo0.45O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder calcined at 1100oC in air
Dane BadawczeThe dataset includes XRD patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.5Mo0.5O6 powder calcined at 1100oC in air
Dane BadawczeThe dataset includes XRD patterns of Sr1.9Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The SEM images of Ce0.8La0.2O2 nanopowder prepared using soft template method
Dane BadawczeThe dataset includes SEM images of Ce0.8La0.2O2-s nanopowder (nanoparticles) prepared using soft template method. CTAB was used as a micelle-based templating agent. The powder was precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitate was heated up to 90oC, centrifuged and washed...
-
The XPS spectra of Ce0.8Ni0.2O2 prepared using microemulsion method
Dane BadawczeThe dataset includes XPS spectra of Ce0.8Ni0.2O2-s sintered under air atmosphere. Samples were produced using aqueous soft chemistry methods (microemulsion). The XPS spectra were collected for all species.
-
The XRD diffraction patterns of Ce0.8La0.2O2/Ni prepared using soft template method and impregnation
Dane BadawczeThe dataset includes XRD patterns of Ce0.8La0.2O2-s nanopowders (nanoparticles,nanocatalyst) prepared using soft template method and further impregnated with 10wt.%Ni using aqueous nitrate solution.
-
FTIR spectra of gas mixtures from the process of biogas dry reforming using CLO/Cu catalyst
Dane BadawczeThe dataset contains the FTIR spectra collected during the catalytic measurements of dry reforming of biogas (60/40 CH4-CO2) using Ce0.8La0.2O2+10wt.%Cu nanocatalyst. The specatra were collected every 1 minute.
-
The SEM images of CeO2 nanopowder prepared using soft template method
Dane BadawczeThe dataset includes SEM images of CeO2-s nanopowder (nanoparticles) prepared using soft template method. CTAB was used as a micelle-based templating agent. The powder was precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitate was heated up to 90oC, centrifuged and washed several...
-
FTIR spectra of gas mixtures from the process of biogas dry reforming using CeO2/Cu catalyst
Dane BadawczeThe dataset contains the FTIR spectra collected during the catalytic measurements of dry reforming of biogas (60/40 CH4-CO2) using CeO2+10wt.%Cu nanocatalyst. The specatra were collected every 1 minute.
-
The SEM images of LSCNT reduced at 1000 degrees C under H2
Dane BadawczeThe dataset includes SEM images of La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s sintered at 1200oC under air atmosphere for 12 h and reduced at 1000oC under H2 for 10 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The XRD diffraction patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder calcined at 1200oC in air
Dane BadawczeThe dataset includes XRD patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The SEM images of Ce0.8La0.2O2 nanocatalyst infiltrated with 10wt.% Ni prepared using soft template method
Dane BadawczeThe dataset includes SEM images of Ce0.8La0.2O2-s nanopowder (nanoparticles) prepared using soft template method and infiltrated to 10wt.% Ni in the catalyst. CTAB was used as a micelle-based templating agent. The powder was precipitated from aqueous nitrate solution using NaOH solution and 250xCMC (critcal micelle concentration) of CTAB. Precipitate...
-
The XRD diffraction patterns of Ce(Gd,Pr)O2-s samples
Dane BadawczeThe dataset includes XRD diffraction patterns of Ce0.8Gd0.2O2-s and Ce0.8Pr0.2O2-s sintered at 600oC under air atmosphere for 4 h. Samples were produced using aqueous soft chemistry methods (Pechini).
-
The XRD diffraction patterns of Sr1.9Fe1.5Mo0.5O6 powder calcined at 1200oC in air
Dane BadawczeThe dataset includes XRD patterns of Sr1.9Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XPS spectra of Ce0.8Cu0.2O2 prepared using microemulsion method
Dane BadawczeThe dataset includes XPS spectra of Ce0.8Cu0.2O2-s sintered under air atmosphere. Samples were produced using aqueous soft chemistry methods (microemulsion). The XPS spectra were collected for all species.
-
The XRD diffraction patterns of La0.3Sr2Al0.1FeMoO6 powder calcined at 1200oC in air
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr2Al0.1FeMoO6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of Sr2Al0.1Fe1.4Mo0.5O6 powder calcined at 1100oC in air
Dane BadawczeThe dataset includes XRD patterns of Sr2Al0.1Fe1.4Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder calcined at 1100oC in air
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder calcined at 800oC in air
Dane BadawczeThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 800oC for 12 h in air.