Filtry
wszystkich: 26
Wyniki wyszukiwania dla: DISSIMILAR WELDING
-
Laser Dissimilar Welding of AISI 430F and AISI 304 Stainless Steels
PublikacjaA dissimilar autogenous laser welded joint of AISI 430F (X12CrMoS17) martensitic stainless steel and AISI 304 (X5CrNi18-10) austenitic stainless steel was manufactured. The welded joint was examined by non-destructive visual testing and destructive testing by macro- and microscopic examination and hardness measurements. With reference to the ISO 13919-1 standard the welded joint was characterized by C level, due to the gas pores...
-
Dissimilar underwater wet welding of HSLA steels
PublikacjaThe high-strength low-alloy S460ML and S460N steels were chosen for underwater wet welding of dissimilar T-joints using covered electrodes. For improving the quality of joints, the temper bead welding (TBW) method was used. The application of TBW in pad welding conditions has been investigated earlier but the possibility of usage of this technique in welded joints was not analyzed. The main aim of the study was to check the influence...
-
The influence of welding heat input on the quality and properties of high strength low-alloy dissimilar steel butt joints
PublikacjaThe paper presents the results of non-destructive and destructive tests of dissimilar highstrength low-alloy S460ML and S460N steel butt joints. These steels are characterized by similar mechanical properties, but their carbon equivalent CeIIW values are much different. The joints were made using different values of heat input for each welding bead. They were tested by non-destructive methods: visual, penetrant, radiographic and...
-
Induction Assisted Hybrid Friction Stir Welding of Dissimilar Materials AA5052 Aluminium Alloy and X12Cr13 Stainless Steel
PublikacjaThis research aimed to study the induction in-situ heated hybrid friction stir welding (IAFSW) method to join AA5052 aluminium alloy with X12Cr13 stainless steel (SS) to enhance joint strength. The potency of this method on the mechanical properties and microstructural characterizations were also investigated. The results show that the transverse tensile strength gained was 94% of the AA5052 base metal that is 229.5 MPa. This superior...
-
Review on friction stir welding of dissimilar magnesium and aluminum alloys: Scientometric analysis and strategies for achieving high-quality joints
PublikacjaMagnesium and aluminum alloys continually attract interest as lightweight structural materials for transport applications. However, joining these dissimilar alloys is very challenging. The main obstacle that hinders progress in dissimilar Mg-Al joining is the formation of brittle intermetallic compounds (IMCs). As a solid-state joining technique, FSW is an excellent candidate to attenuate the deleterious IMC effects in dissimilar...
-
Investigation of the Effects of Tool Positioning Factors on Peak Temperature in Dissimilar Friction Stir Welding of AA6061-T6 and AA7075-T6 Aluminum Alloys
PublikacjaAmong the emerging new welding techniques, friction stir welding (FSW) is used frequently for welding high-strength aluminum alloys that are difficult to weld by conventional fusion-welding techniques. This paper investigated the effects of tool-positioning factors on the maximum temperature generated in the dissimilar FSW joint of AA6061-T6 and AA7075-T6 aluminum alloys. Three factors of plunge depth, tool offset, and tilt angle...
-
Jacek Tomków dr hab. inż.
OsobyWykształcenie:1. 2018 r.Doktor inżynier - Politechnika Gdańska, Wydział Mechaniczny, Inżynieria Materiałowa,rozprawa doktorska: Wpływ warunków spawania pod wodą na skłonność do tworzenia pęknięć zimnych w stalach o podwyższonej wytrzymałości 2. 2012 r.Magister inżynier - Politechnika Gdańska, Wydział Mechaniczny, Mechanika i Budowa Maszyn, specjalność: Technologia Maszyn i Komputerowe Wspomaganie Produkcji,praca magisterska: Badania...
-
Study on Microstructure and Mechanical Properties of Laser Welded Dissimilar Joint of P91 Steel and INCOLOY 800HT Nickel Alloy
PublikacjaThis investigation attempts to explore the weld characteristics of a laser welded dissimilar joint of ferritic/martensitic 9Cr-1Mo-V-Nb (P91) steel and Incoloy 800HT austenitic nickel alloy. This dissimilar joint is essential in power generating nuclear and thermal plants operating at 600–650 °C. In such critical operating conditions, it is essential for a dissimilar joint to preserve its characteristics and be free from any kind...
-
Corrosion Properties of Dissimilar AA6082/AA6060 Friction Stir Welded Butt Joints in Different NaCl Concentrations
PublikacjaA solid-state friction stir welding method which is increasingly used in the marine and shipbuilding industry, has been developed to produce welds with high mechanical properties. In seawater, the oxide layer of aluminium is attacked by Cl− ions resulting in its disruption and formation of pitting corrosion. It is particularly important to determine the electrochemical properties of the produced welds and to evaluate the efect...
-
Study on Microstructural Characterization, Mechanical Properties and Residual Stress of GTAW Dissimilar Joints of P91 and P22 Steels
PublikacjaThis article deals with the dissimilar joining of two different grade Cr-Mo steel (2.25Cr-1Mo: P22 and modified 9Cr-1Mo: P91) for power plant application. The dissimilar butt-welded joint was produced for conventional V groove design by using the gas tungsten arc welding (GTAW) process with the application of an ERNiCrMo-3 Ni-based super alloy filler. A microstructure characterization was performed to measure the inhomogeneity...
-
Creep rupture study of dissimilar welded joints of P92 and 304L steels
PublikacjaThe present work investigates the high-temperature tensile and creep properties of the dissimilar metal weld joints of 304L austenitic stainless steel (SS) and P92 creep strength-enhanced ferritic-martensitic (CSEF/M) steel under diferent testing condition. Thermanit MTS 616 fller rod (P92 fller) and the multi-pass tungsten inert gas (TIG) welding process were used to create the dissimilar weld connection. The ultimate tensile...
-
Autogenous Fiber Laser Welding of 316L Austenitic and 2304 Lean Duplex Stainless Steels
PublikacjaThis study presents results of experimental tests on quality of dissimilar welded joints between 316L austenitic and 2304 lean duplex stainless steels, welded without ceramic backing. Fiber laser welded butt joints at a thickness of 8 mm were subjected to non‐destructive testing (visual and penetrant), destructive testing (static tensile test, bending test, and microhardness measurements) and structure observations (macro‐ and...
-
Role of buttering layer composition on microstructural heterogeneity and mechanical properties of Alloy 617 and P92 steel dissimilar welded joints for future Indian AUSC program
PublikacjaRestrictive operating conditions (even exceeding 700 °C) of materials in advanced ultra super critical (AUSC) power plants and the need to minimize manufacturing and maintenance costs require the production of dissimilar metal welded joints (DMW). Significant differences in the physical and chemical properties of welded materials lead to phenomena that reduce the weldability of the metals used and force the search for solutions...
-
Influence of friction stir welding technological parameters on the properties of the joints of selected aluminum alloys
PublikacjaThe purpose of this dissertation was to determine the effect of friction stir welding technological parameters on the properties of selected aluminum alloy joints, with consideration of the residual stresses and dislocation density in the joints. The goal of the present work was also to produce defect-free joints with high mechanical and electrochemical properties. In the dissertation, similar welds of AA6082 alloy and dissimilar...
-
Study on Microstructure-Property Relationship of Inconel 617 Alloy/304L SS Steel Dissimilar Welds Joint
PublikacjaWelding of Inconel 617 (IN617) alloy and austenitic 304L SS steel has been attempted using the autogenous Laser Beam Welding (LBW) process. Characterization of dissimilar weldments was performed on either side of the fusion boundaries. The metallographic results showed that the inhomogeneous microstructure formation for weld metal contained columnar and cellular dendrites near the interface, whilst the columnar, cellular and equiaxed...
-
Microstructure and Mechanical Properties of Combined GTAW and SMAW Dissimilar Welded Joints between Inconel 718 and 304L Austenitic Stainless Steel
PublikacjaA dissimilar welded joint of Inconel 718 and 304L austenitic stainless steel was prepared using a combined procedure with the gas tungsten arc welding and shielded metal arc welding processes by employing the Ni-based fillers: ERNiCr-3 and ENiCrFe-3. The welded joints were investigated for metallographic testing and mechanical properties, and a relationship was established between the microstructure and the resultant mechanical...
-
Laser Welding of UNS S33207 Hyper-Duplex Stainless Steel to 6061 Aluminum Alloy Using High Entropy Alloy as a Filler Material
PublikacjaThe high entropy alloy (HEA) filler used during the fabrication method determines the reliability of HEAs for steel-aluminum dissimilar alloy configuration. HEAs have a direct impact on the formation of intermetallic compounds (IMC) formed by the interaction of iron (Fe) and aluminum (Al), and influence the size of the joint’s interaction zone. A novel welding process for Fe-Al alloy joints was developed to prevent the development...
-
Mechanical and Microstructural Characterization of TIG Welded Dissimilar Joints between 304L Austenitic Stainless Steel and Incoloy 800HT Nickel Alloy
PublikacjaIn this article, the mechanical properties and microstructure of 304L austenitic stainless steel/Incoloy 800HT nickel alloy dissimilar welded joints are investigated. The joints were made of 21.3 mm × 7.47 mm tubes using the TIG process with the use of S Ni 6082 nickel filler metal. No welding imperfections were found and high strength properties of joints were obtained, meeting the assumed acceptance criteria of the product’s...
-
Właściwości złączy różnoimiennych stopu niklu Incoloy 800H ze stalą odporną na korozję 316L
PublikacjaW artykule przedstawiono problemy związane z wykonywaniem połączeń różnoimiennych typu Incoloy 800HT – austenityczna stal odporna na korozję 316L. Wykonano badania nieniszczące oraz niszczące, których wyniki pozwoliły na weryfikacje jakości wykonanych złączy próbnych. Nie stwierdzono występowania niezgodności spawalniczych oraz uzyskano wysokie właściwości wytrzymałościowe złączy. Badania metalograficzne ujawniły poprawne struktury...
-
Advanced ultra super critical power plants: role of buttering layer
PublikacjaDissimilar metal welded (DMW) joint plays a crucial role in constructing and maintaining ultra-supercritical (USC) nuclear power plants while presenting noteworthy environmental implications. This research examines different welding techniques utilized in DMWJ, specifically emphasizing materials such as P91. The study investigates the mechanical properties of these materials, the impact of alloying elements, the notable difficulties...
-
Influence of the Tool Rotational Speed on Physical and Chemical Properties of Dissimilar Friction-Stir-Welded AA5083/AA6060 Joints
PublikacjaAluminum alloys have been successfully used in the railroad and automotive industries because of their potential to significantly reduce component weights, and their good mechanical and anti-corrosion properties. Problems with joining aluminum alloys are characterized by low weldability, which influences the need for studies focused on unconventional methods. The environmentally friendly and low-cost friction-stir-welding method...
-
P92 steel and inconel 617 alloy welds joint produced using ERNiCr-3 filler with GTAW process: Solidification mechanism, microstructure, mechanical properties and residual stresses
PublikacjaThe objective of the current study was to analyse the microstructure, mechanical characteristics, and residual stresses of a dissimilar welded joint (DWJ) made of P92 steel and the Inconel alloy 617 (IN617) using the gas tungsten arc welding (GTAW) method. The ERNiCr-3 filler was selected to produce the conventional V groove (VG) and narrow V groove (NVG) butt joint. The filler deficient zones in the weldments, such as the filler...
-
Dissimilar autogenous TIG joint of Alloy 617 and AISI 304H steel for AUSC application
PublikacjaTo reduce costs and improve high-temperature performance in Advanced Ultra Super Critical (AUSC) boilers, it is necessary to weld austenitic steel to Inconel alloy. In this study, the autogenous tungsten inert gas (TIG) welding process was used to join Alloy 617 and an austenitic AISI 304H steel plate of thickness 5 mm. Microstructural analysis showed that the microstructure formation was uneven along the weldments, with columnar...
-
A dissimilar welded joint of grade 92 steel and AISI 304L steel obtained using IN82 buttering and IN617 fller: relationship of microstructure and mechanical properties
PublikacjaUnfavourable operating conditions of equipment in the energy industry resulting from high-temperature loads determine the need to use special materials and technological solutions, including welding procedures. In this article, buttering using IN82 (ERNiCr-3) consumables was proposed as a method to improve the weldability of grade 92 steel joined by the gas tungsten arc welding (GTAW) process with AISI 304L (IN617 fller). The...
-
Effect of Tool Positioning Factors on the Strength of Dissimilar Friction Stir Welded Joints of AA7075-T6 and AA6061-T6
PublikacjaFriction Stir Welding (FSW) is a solid-state bonding technique. There are many direct and indirect factors affecting the mechanical and microstructural properties of the FSW joints. Tool offset, tilt angle, and plunge depth are determinative tool positioning in the FSW process. Investigating the effect of these factors simultaneously with other parameters such as process speeds (rotational speed and translational speed) and tool...
-
Microstructure and mechanical properties of a dissimilar metal welded joint of Inconel 617 and P92 steel with Inconel 82 buttering layer for AUSC boiler application
PublikacjaThe application of the novel dissimilar metal welded (DMW) joint, utilizing Inconel 617 and P92 steel, was showcased in the advanced ultra-supercritical (AUSC) boiler. The work has been performed to investigate the effect of Inconel 82 (ERNiCr-3) buttering layer on microstructure and mechanical properties (high-temperature tensile strength, impact strength and microhardness) of gas tungsten arc welded (GTAW) dissimilar joint between...