Wyniki wyszukiwania dla: SINTERING
-
SEM images of symmetrical cell interface with SrTi0.65Fe0.35O3-d electrode and CGO-20 substrate in function of sintering temperature
Dane BadawczeThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.65Fe0.35O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
SEM images of symmetrical cell interface with SrTi0.50Fe0.50O3-d electrode and CGO-20 substrate in function of sintering temperature
Dane BadawczeThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.50Fe0.50O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
Influence of sintering temperature of porous SrTi0.30Fe0.70O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Influence of sintering temperature of porous SrTi0.50Fe0.50O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Influence of sintering temperature of porous SrTi0.65Fe0.35O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Natalia Anna Wójcik dr hab. inż.
Osoby -
Fabrication and Study of BiNbO4 Ceramics
PublikacjaAim of the present research was to fabricate and study crystalline structure as well as dielectric properties of BiNbO4 ceramics. In the present study BiNbO4 ceramics was fabricated by solid state reaction from the mixture of simple oxides viz. Bi2O3, and Nb2O5. Stoichiometric mixture of the powders was thermally analyzed so parameters of the thermal treatment were determined. The EDS measurements proved conservation of the chemical...
-
Modification of Ground Tire Rubber—Promising Approach for Development of Green Composites
PublikacjaGround tire rubber (GTR) was mechano-chemically modified using a road bitumen 100/150 and two types of organic peroxides: di-(2-tert-butyl-peroxyisopropyl)-benzene (BIB) and dicumyl peroxide (DCP). The impact of used additives on reactive sintering efficiency and physico-mechanical properties of modified GTR was investigated using oscillating disc rheometer measurements, followed by tensile tests and swelling behavior studies....
-
X-RAY DIFFRACTION STUDY OF BISMUTH LAYER-STRUCTURED MULTIFERROIC CERAMICS
PublikacjaGoal of the present research was to apply a solid state reaction route to fabricate bismuth layer-structured multiferroic ceramics described with the formula Bi5FeTi3O15 and reveal the influence of processing conditions on its crystal structure and phase composition. Simple oxide powders Bi2O3, TiO2 and Fe2O3 were used to fabricate Aurivillius-type bismuth layer-structured ferroelectrics. Pressureless sintering in ambient air was...
-
CGO as a barrier layer between LSCF electrodes and YSZ electrolyte fabricated by spray pyrolysis for solid oxide fuel cells
PublikacjaPerovskite La0.6Sr0.4Co0.2Fe0.8O3 − δ (LSCF) is often used as a cathode material for solid oxide fuel cells (SOFC) due to high mixed ionic and electronic conductivity and good catalytic activity. Unfortunately, sintering of the LSCF cathode together with the yttria stabilized zirconia (YSZ) electrolyte, leads to formation of the La2Zr2O7 and SrZrO3 phases in the interface. These phases increase the resistance of the cell. To avoid...
-
Mg2+ Doping Effects on the Structural and Dielectric Properties of CaCu3Ti4O12 Ceramics Obtained by Mechanochemical Synthesis
PublikacjaIn this study, ceramic CaCu3Ti4O12 (CCTO) and CaCu3−xMgxTi4O12 solid solutions in which 0.1 ≤ x ≤ 0.5 were prepared by the mechanochemical method, realized by a high‐energy ball milling technique. The effects of the Mg2+ ion concentration and sintering time on the dielectric response in the prepared ceramics were investigated and discussed. It was demonstrated that, by the use of a sufficiently high energy of mechanochemical treatment,...
-
Series resistance (at 800 °C - 500 °C) of the Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the ohmic contribution of differently sintered Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C, 1000 °C and 1050 °C. The measurement temperature range was between 800 °C and 500 °C in stationary air. Results converted to electrode surfaces area.
-
Area specific resistance (at 800 °C - 500 °C) of the Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the polarization resistance of differently sintered Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C, 1000 °C and 1050 °C. The measurement temperature range was between 800 °C and 500 °C in stationary air. Results converted to electrode surfaces...
-
Series resistance (at 800 °C - 500 °C) of the SrTi0.50Fe0.50O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the ohmic contribution of differently sintered Sr0Ti0.50Fe0.50O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic ari flow (21% O2, 40 ml min-1). Results converted to electrode...
-
Series resistance (at 800 °C - 500 °C) of the SrTi0.30Fe0.70O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the ohmic contribution of differently sintered Sr0Ti0.30Fe0.70O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic ari flow (21% O2, 40 ml min-1). Results converted to electrode...
-
Series resistance (at 800 °C - 500 °C) of the SrTi0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the ohmic contribution of differently sintered Sr0Ti0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic ari flow (21% O2, 40 ml min-1). Results converted to electrode...
-
Area specific resistance (at 800 °C - 500 °C) of the SrTi0.50Fe0.50O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the polarization resistance of differently sintered SrTi0.50Fe0.50O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to...
-
Area specific resistance (at 800 °C - 500 °C) of the SrTi0.30Fe0.70O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the polarization resistance of differently sintered SrTi0.30Fe0.70O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to...
-
Area specific resistance (at 800 °C - 500 °C) of the SrTi0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Dane BadawczeIn this dataset are presented results of the polarization resistance of differently sintered SrTi0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to...
-
SEM images of symmetrical cell interface with Sr1.05Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at 800 °C, 900 °C and 1000 °C
Dane BadawczeThis dataset contains images of polished cross section of symmetrical cell interface with Sr1.05Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at three different temperatures 800 °C, 900 °C and 1000 °C. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating...