Filtry
wszystkich: 566
wybranych: 9
Wyniki wyszukiwania dla: punching shear
-
Determination of changes in viscosity of hydrogel depending on shear rate (1.1 to 55 s-1).
Dane BadawczeThe rheological characteristics of hydrogel were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 25 spindle and shear rates from 1.1 to 55 s-1.
-
Determination of changes in viscosity of hydrogel depending on shear rate (1.7 to 34 s-1).
Dane BadawczeThe rheological characteristics of hydrogel were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 27 spindle and shear rates from 1.7 to 34 s-1.
-
Determination of changes in viscosity of hydrogel depending on shear rate (6.6 to 330 s-1).
Dane BadawczeThe rheological characteristics of hydrogel were made on the basis of a viscosity measurement using a Brookfield viscometer, using LV SC4 - 18 spindle and shear rates from 6.6 to 330 s-1.
-
Determination of changes in viscosity of refined oil depending on the temperature (19-96 Celsius degrees).
Dane BadawczeThe rheological characteristics of the refined oil were made on the basis of the viscosity assessment using a Brookfield viscometer with an LV SC4 - 18 spindle and a shear rate of 52.8 s-1 in from temperature 19-96 °C.
-
XRD, DTA and luminescence measurements of B2O3-Bi2O3-AlF3 glasses doped with Eu3+, Tb3+ and Tm3+ ions
Dane BadawczeThe DataSet contains the XRD,DTA and luminescence measurements for the B2O3-Bi2O3-AlF3 glass system. Samples were prepared by the conventional melt quenching technique. Starting materials were melted in porcelain crucibles at 950 oC for 20 min. XRD and DTA data were collected for 50B2O3-50Bi2O3,45B2O3-45Bi2O3+10AlF3 and 40B2O3-40Bi2O3+20AlF3 glasses....
-
Fresh properties of concrete mixes M0-M100 concrete mixes
Dane BadawczeDataset of fresh properties of concretes containing different amount of magnetite aggregate (M0-M100) mixes.*. ODS - open-source spreadsheet file file consists results of:
-
The luminescence study of SrAl11.88−xGaxO19:0.12Cr3+ coumpounds.
Dane BadawczePortable near-infrared (NIR) light sources are in high demand for applications in spectroscopy, night vision, bioimaging, and many others. Typical phosphor designs feature isolated Cr3+ ion centers, and it is challenging to design broadband NIR phosphors based on Cr3+–Cr3+ pairs. Here, we explore the solid-solution series SrAl11.88–xGaxO19:0.12Cr3+...
-
Hemocompatibility of nanocrystalline diamond layers
Dane BadawczeThe biocompatibility of the diamond films were investigated with whole human blood samples. Blood used in this study was drawn from 10 healthy human patients of different age, sex, and blood group. A 2 ml samples were collected into standard tubes with EDTA anticoagulation agent. Blood was used within 6 hours from the collection time. A reference blood...
-
Nonlinear impedance as a function of A.C. voltage for glass 40Bi2VO5.5-60SrB4O7 annealed at 473 K for 3h and next fully crystallized measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties as a function of A.C. voltage for annealed at 473 K for 3h and next fully crystallized 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.