ISSN:
eISSN:
Publisher:
Disciplines
(Field of Science):
- biomedical engineering (Engineering and Technology)
- chemical engineering (Engineering and Technology)
- civil engineering, geodesy and transport (Engineering and Technology)
- materials engineering (Engineering and Technology)
- mechanical engineering (Engineering and Technology)
- pharmacology and pharmacy (Medical and Health Sciences )
- chemical sciences (Natural sciences)
(Field of Science)
Ministry points: Help
Year | Points | List |
---|---|---|
Year 2024 | 40 | Ministry scored journals list 2024 |
Year | Points | List |
---|---|---|
2024 | 40 | Ministry scored journals list 2024 |
2023 | 70 | Ministry Scored Journals List |
2022 | 40 | Ministry Scored Journals List 2019-2022 |
2021 | 40 | Ministry Scored Journals List 2019-2022 |
2020 | 40 | Ministry Scored Journals List 2019-2022 |
2019 | 40 | Ministry Scored Journals List 2019-2022 |
2018 | 11 | B |
2017 | 11 | B |
2016 | 11 | B |
2015 | 11 | B |
2014 | 9 | B |
2013 | 9 | B |
2012 | 6 | B |
2011 | 6 | B |
2010 | 6 | B |
Model:
Impact Factor:
Publishing policy:
- License
- open in new tab
- Information on publishing policy
- https://content.sciendo.com/view/journals/adms/adms-overview.xml open in new tab
- Information on the conditions of self-archiving
- Included in license
- Is self-archiving allowed by the journal?
- Yes - with restrictions
- Information on research data policy
- n/a
- Months of embargo
- no embargo
- Additional information
-
Must link to journal homepage with DOI.
Self-archiving policy for article versions based on the Sherpa Romeo database.
Papers published in journal
Filters
total: 135
Catalog Journals
Year 2007
-
Hardness measurements for assessment of cavitation intensity
PublicationArtykuł opisuje możliwość zastosowania pomiarów teardości erodowanego materiału do oceny natężenia zjawiska kawitacji. Proponowana metoda zakłada, że cała energia implodujących pęcherzyków kawitacyjnych zamieniana jest na przyrost twardości warstwy wierzchniej materiału
-
High temperature corrosion of evaporator tubes in low-emission steam boilers
PublicationW artykule opisano zjawisko korozji wysokotemperaturowej rur ekranowych kotłów parowych niskoemisyjnych. Przeprowadzono badania rur po eksploatacji. Wykonano badania składu chemicznego zgorzelin. Stwierdzono, że główną przyczyną pocienienia rur na wyższych poziomach jest korozja siarkowa, natomiast na poziomach niższych oddziaływanie stopionych soli.
-
High temperature corrosion of the cobalt base clad layers
PublicationNapawane warstwy wykonane ze stopu kobaltu poddano utlenianiu w temperaturach 650 stopni C i 750 stopni C oraz korozji w spalinach. Proces utleniania był prowadzony 2 sposobami, izotermicznie przez 100 godzin i cyklicznie pzez 200 godzin. Korozja w spalinach przebiegała cyklicznie przez 200 godzin w temperaturze 650stopni C. Warstwy napawano metodą laserową i plazmową (PTA). Badano stabilność termiczną procesu utleniania warstw...
-
Hydrogen degradation of high strength weldable steels
PublicationW pracy przedstawiono wyniki badań podatności stali spawalnych o wysokiej wytrzymałości na niszczenie wodorowe. Badano dwa gatunki stali S690Q i ich złącza spawane. Ocenę podatności na niszczenie wodorowe wykonano w oparciu o próbę rozciągania z małą prędkością odkształcania w powietrzu i środowisku wody morskiej przy polaryzacji katodowej. Przedstawiono model niszczenia wodorowego badanych stali i ich złączy spawanych.
-
Hydrogen permeation through welded joints of S690QL steels at cathodic polarisation in sea water in the presence of SRB
PublicationPrezentowane są wyniki badan metodą Devanathana- Stachurskyego przenikania wodoru w wodzie morskiej w obecności bakterii redukujących siarczany i w warunkach sterylnych. Badania wykonano na stali S690QL poddanej symulowanym obróbkom cieplnym prowadzącym do struktur modelujących strefy wpływu ciepła. Stwierdzono dodatni wpływ obecności bakterii na przenikanie wodoru. Różnice między poszczególnymi próbkami były minimalne.
-
Influence of H2S on degradation of 9Cr-1Mo steel in advanced stage of metal dusting process
PublicationPrzedstawiono wyniki badań stali 9Cr-1Mo w zaawansowanym stadium procesu pylenia metalu po 10 latach eksploatacji w piecu rafineryjnej instalacji platformingu CCR, przeprowadzonych w celu podjęcia decyzji o dozowaniu związków siarki do wsadu instalacji. Na podstawie długotrwałej ekspozycji próbek stali w 600C w mieszaninie wodoru i siarkowodoru wykazano, że siarka może być powodem procesów wpływających niekorzystnie na stan materiału...
-
Influence of the heat treatment on corrosion characteristics of the Superston alloy
PublicationW artykule przedstawiono wpływ hartowania i odpuszczania na twardość i właściwości korozyjne stopu Superston, stosowanego na śruby okrętowe. Stwierdzono, iż hartowanie z temperatury 900 st.C i odpuszczanie w temperaturze 550 st.C znacząco podwyższa odporność na korozję stopu Superston w 3% roztworze NaCl w porownaniu ze stanem odlanym.
-
Microstructural aspects of corrosion of the SUPERSTON alloy after laser treatment
PublicationW artykule przedstawiono rezultaty obróbki laserowej stopu SUPERSTON w warunkach kriogenicznych i jej wpływ na mikrostrukturę i odporność korozyjną. Badania korozyjne zostały zrealizowane metodą potencjostatyczną w 3% NaCl, odporność korozyjna stopu zmieniała się wraz ze zmianą parametrów nadtapiania laserowego.
-
New laser-enhanced surface treatment of Ti bioalloy
PublicationPrzedstawiono wyniki badan mikrostruktury i korozji w roztworze Ringera stopu Ti6Al4V, który był poddawany nadtapianiu laserem CO2 w powietrzu, wodzie i ciekłym azocie. Stwierdzono znaczący wpływ warunków obróbki na mikrostrukturę, mikrotwardość i głębokość zmodyfikowanej warstwy wierzchniej.
-
The use of nitriding as a prevention method against hydrogen degradation of high-strength steels
PublicationPrzedstawiono badania wpływu warstw azotowanych jarzeniowo na stali 34CrAlNi7-10 na jej podatność na niszczenie wodorowe. Wytworzono warstwy azotowane w atmosferach technologicznych o różnym udziale wodoru. Próbki materiału rodzimego i z warstwami azotowanymi poddano próbie rozciągania z małą prędkością odkształcania w środowisku 0,01 N kwasu siarkowego przy polaryzcaji katodowej. Względny spadek plastyczności i charakter przełomu...
Year 2008
-
Analisys of the failure of fixator used in bone surgery
PublicationThe Gamma nail (fixator) made of stainless steel, which has broken in the body, was subjected to examination. The fixator was removed from the patient femur. The fracture occurred in the area of the nail hole after two months' stay in the organism. The research included chemical composition, hardness of the Gamma nail material and the observation and analysis of the type of fracture. The research showed the fatigue failure of the...
-
Assessment of cavitation erosion damage of laser remelted the SUPERSTON alloy
PublicationW artykule przedstawiono wpływ obróbki laserowej w warunkach kriogenicznych na mikrostrukturę stopu SUPERSTON po badaniach kawitacyjnych. Badania odporności kawitacyjnej przeprowadzono na stanowisku z wirującą tarczą w IMP PAN Gdańsk. Określono kinetykę ubytku masy próbek podczas testu kawitacyjnego dla stopu odlanego i nadtopionego laserowo.
-
Assessment of evaporator tubes corrosion in low-emission steam boilers
PublicationW artykule przedstawiono wyniki badań rur ekranowych(16Mo3) kotła niskoemisyjnego po jednym roku i dwóch latach eksploatacji. Powierzchnie rur pokryte zostały warstwami natryskiwanymi cieplne - pojedynczą ze stopu 70%Ni 30%Cr i podwójną Ni-30Cr /Al2O3. Rury bez powłok natryskiwanych wykazywały pocienienie ze względu na działanie korozji siarkowej oraz korozyjnego oddziaływania warstwy stopionych soli. Pojedyncza warstwa 70%Ni 30%Cr...
-
Cavitation erosion of X5CrNi18-10 austenitic stainless steel alloyed with TiC
PublicationPraca prezentuje zmianę odporności kawitacyjnej stali X5CrNi18-10 po laserowym stopowaniu jej warstwy wierzchniej węglikiem TiC. Laserowe stopowanie przeprowadzono dla 2 wariantów. W pierwszym przypadku stal stopowano do zawartości 1,55 TiC a w drugim do zawartości 3,97% TiC. Uzyskane rezultaty wskazują że przy zawartości 3,97 TiC nastopiło znaczące zwiększenie odporności na plastyczne odkszyałcenie warstwy wierzchniej pod wpływem...
-
Coatings in arthroplasty [online]
PublicationThe modern coatings used in arthroplasty for long term implants are reviewed. The phosphate coatingsare the most popular technique to improve the bone-implant interfacial strength and promote theosseointegration. The plasma spraying, electrophoretic precipitation, powder metallurgy, ion beamsputtering, high velocity oxy-fuel (HVOF) combustion spraying, sol-gel technique, biomimeticdeposition are mostly used to obtain the phosphate,...
-
Effects of the time and temperature on the oxide scale formed on the cobalt alloys
PublicationWarstwy wykonane za pomocą techniki PTA ze stopu kobaltu poddano utlenianiu w różnych temperaturach i w różnym czasie. Mikrostruktury otrzymane po utlenianiu wskazują na proces degradacji materiału. Proces ten prowadził do degradacji obszarów międzydendrytycznych napoiny. Skład chemiczny powstającej zgorzeliny byłzależny od temperatury utleniania, składu chemicznego stopu, ze szczegfólnym uwzględnieniem obecności małych ilości...
-
FEM approach to estimate the behaviour of biocomposite metal-surface coating system
PublicationA three dimensional (3D) model of biocomposite metal-surface coating system, which is influenced byknown external forces, is proposed. This model consists of the metallic substrate (Ti6Al4V) and thehydroxyapatite (HA) coating. Using FEM (finite element method), strain-stress maps of model weregenerated for investigating relations between the extreme stress of HA coating and the magnitude ofexternal force and the thickness of the...
-
Microbiological corossion of metallic products as a result of biofilm
PublicationWarunkiem do pojawienia się korozji mikrobiologicznej jest utworzenie na powierzchni metalu biofilmu. Zawiera on biologicznie czynne mikroorganizmy wraz z produktami ich przemian metabolicznych. Biofilm ogranicza dyfuzję produktów metabolizmu wytwarzanych przez poszczególne komórki mikrokolonii. Powoduje to, że produkty uboczne tych przemian gromadzą się w bezpośrednim sąsiedztwie metalu. Gdy powierzchnia metalu nie jest odporna...
-
Microstructure and corrosion properties of the (Mn-N-O-P) type layers created on aluminium alloys
PublicationPrzedstawiono mikrostrukturę i właściwości korozyjne warstw powierzchniowych typu (Mn-N-O-P) wytworzonych na stopach aluminium. Wykazano, iż warstwy (Mn-N-O-P) podwyższają wielokrotnie odporność korozyjną stopów aluminium i mogą być stosowane jako warstwy ochronne na tych materiałach.
-
Ocena wpływu parametrów nadtapiania laserowego w warunkach kriogenicznych na strukturę warstwy wierzchniej na stopie Ti-6Al-4V
PublicationW pracy zostały przedstawione efekty przetapiania laserowego w warunkach kriogenicznych stopu tytanu Ti-6Al-4V. W celu określenia wpływu obróbki laserowej wykonano analizę mikrostruktury (SEM), składu fazowego (XRD), oraz pomiary mikrotwardości uzyskanych warstw. Stwierdzono, że zmiany podstawowych parametrów przetapiania laserowego - mocy wiązki lasera i prędkości skanowania istotnie wpływają na grubość i mikrostrukturę otrzymanych...