Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Open Research DataThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 10Na2O–60P2O5–30CaO glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 10Na2O–60P2O5–30CaO glass was measured by impedance spectroscopy method.
-
Linear impedance of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 1SiO2–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 1SiO2–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 35P2O5-30Fe2O3-20Nb2O5-15TiO2
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and...
-
Linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Open Research DataThe electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2 (≥99.9%, anatase...
-
Linear impedance of 40Na2O-20CaO-40P2O5 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 40Na2O-20CaO-40P2O5 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at low temperatures
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.