Filters
total: 1725
filtered: 172
-
Catalog
Chosen catalog filters
Search results for: SYNTHESIS
-
Studies on the building typology, Gdańsk-Wrzeszcz district case study, Kościuszki street, March 2020
Open Research DataThe data presents results of work within the studies on the building typology, Gdańsk-Wrzeszcz district case study, Kościuszki street, study proposal from March 2020. The goal of the process was to identify the basic types of urban structure of the area and to analyse them in terms of location, connections with the neighbourhood, basic and social functions,...
-
Studies on the building typology, Gdańsk-Wrzeszcz district case study, Matejki street, Wajdeloty street, Saperów street, March 2020
Open Research DataThe data presents results of work within the studies on the building typology, Gdańsk-Wrzeszcz district case study,Matejki street, Wajdeloty street, Saperów street, study proposal from March 2020. The goal of the process was to identify the basic types of urban structure of the area and to analyse them in terms of location, connections with the neighbourhood,...
-
Hydrogenation process ofTiO2/BiVO4/PEDOT:PSS observed by XPS method
Open Research DataTitania nanotubes synthesis was based on a two-stage anodization process at water/ethylene glycol (5%/95%) electrolyte containing 0.27 M NH4F and 1 M H3PO4 described previously. Anodization process was performed in two-electrode cell compartment using platinum mesh as a cathode. The distance between electrodes was about 2 cm. The anodization voltage...
-
Linear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Non-linear impedance of V2O5 nanorods obtained at 923K
Open Research DataThe DataSet contains the non-linear electrical properties of V2O5 nanorods which were measured by the impedance spectroscopy method. V2O5 nanorods were obtained by the sol-gel method. The information about xerogel powder synthesis is described in the Journal of Nanomaterials. The precursor powder was pressed into the disk-shaped pellets (12mm in diameter...
-
Depth chemical profile in a CeIr3 sample
Open Research DataThe polycrystalline sample of CeIr3 used in the present studies was synthesized by arc-melting cerium (4N) and iridium (3N5) in an arc furnace on a water-cooled copper hearth using a tungsten electrode under a high purity argon atmosphere. A piece of zirconium was used as an oxygen getter. First, a button of Ir was prepared by arc-melting the iridium...
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
The luminescence study of Sc2(1–x)Ga2xO3:Cr3+/4+ coumpounds
Open Research DataThe growing interest in the use of near-infrared (NIR) radiation for spectroscopy, optical communication, and medical applications spanning both NIR-I (700–900 nm) and NIR-II (900–1700 nm) has driven the need for new NIR light sources. NIR phosphor-converted light-emitting diodes (pc-LEDs) are expected to replace traditional lamps mainly due to their...
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
The XRD diffraction patterns of La0.3Sr1.7Fe1.5Mo0.5O6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr1.7Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1W0.9O3-s precursor calcined under air atmosphere
Open Research DataThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1W0.9O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s precursor calcined under air atmosphere
Open Research DataThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1W0.45Mo0.45O3-s precursor calcined under air atmosphere
Open Research DataThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1W0.45Mo0.45O3-s precursor gel prepared using wet chemistry methods, namely modified Pechini route. The powders were calcined at 550oC for 5 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.5Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.4Ni0.1Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of Sr1.9Fe1.5Mo0.5O6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of Sr1.9Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr2Al0.1FeMoO6 powder calcined at 1200oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr2Al0.1FeMoO6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1200oC for 12 h in air.
-
The XRD diffraction patterns of Sr2Al0.1Fe1.4Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of Sr2Al0.1Fe1.4Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder calcined at 1100oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr1.7Al0.1Fe1.5Mo0.5O6 powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 1100oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder calcined at 800oC in air
Open Research DataThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 800oC for 12 h in air.
-
The XRD diffraction patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder calcined at 800oC in H2
Open Research DataThe dataset includes XRD patterns of La0.3Sr0.6Ce0.1Ni0.1Mo0.9O3-s powder prepared using wet chemistry methods, namely modified Pechini route. The powders were sintered at 800oC for 12 h in H2. Pure perovskite phase was formed