Linear impedance of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Force-deformation spectroscopy in contact mode
Open Research DataThe deformation-distance spectroscopic curve is obtained by registering the value of the probe cantilever deflection as a function of the elongation of the piezoelectric scanner. It assumes a simple relationship in the form of Hooke’s law, linking the deformation of the lever with the amount of its deflection caused by the proximity of the probe and...
-
Fourier transform infrared spectroscopy (FTIR) of pre- PXBS (0 h) and PXBS during the crosslinking process (24 h–288 h)
Open Research DataThe goal of this research was developing biodegradable and biocompatibile xylitol-based copolymers with improved mechanical properties, and investigating the change in their thermal and chemical properties withprogress of the cross-linking process. Using a raw material of natural origin such as xylitol, a prepolymer wasobtained by esterification and...
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Open Research DataThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 10Na2O–60P2O5–30CaO glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 10Na2O–60P2O5–30CaO glass was measured by impedance spectroscopy method.
-
Linear impedance of 1SiO2–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 1SiO2–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
SEM (Scanning Electron Microscopy) and SEM-EDS (Scanning Electron Microscopy with Energy Dispersive X-ray Spectroscopy) images of nickel (Ni) foam as received, after photocatalysis and after oxidation at 500_C.
Open Research DataThis dataset contains SEM (Scanning Electron Microscopy) and SEM-EDS (Scanning Electron Microscopy with Energy Dispersive X-ray Spectroscopy) images of Ni (nickel) foam as received from the supplier, after photocatalytic treatment and after oxidation at 500C. The detailed equipment and measurement data was described in "readme SEM.txt" file
-
Nonlinear impedance of as-quenched Bi2VO5.5 glass-ceramic was measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrical properties of as-quenched Bi2VO5.5 glass-ceramic was measured by impedance spectroscopy method.
-
Linear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 800 °C and 15% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....