Search results for: perovskite
-
Oxygen partial pressure and temperature dependence of low frequency resistance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of low frequency resistance at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Oxygen partial pressure and temperature dependence of series resistance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of series resistance (R) at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Oxygen partial pressure and temperature dependence of middle frequency resistance of symmetrical porous Sr0.86Ti0.65Fe0.35O3 electrode on CGO substrate
Open Research DataThis dataset contains values of middle frequency resistance at different temperatures (800 °C, 750 °C, 700 °C, 650 °C and 600 °C) and oxygen partial pressures (20%, 10%, 5%, 1%, 0.1% and 0.01% pO2) of symmetrical Sr0.86Ti0.65Fe0.35O3 electrode sintered at 1000 °C. This values were obtained by fitting each measured impedance spectra by electrical equivalent...
-
Series resistance (at 800 °C - 500 °C) of the Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes sintered at different temperatures
Open Research DataIn this dataset are presented results of the ohmic contribution of differently sintered Sr0.86Ti0.65Fe0.35O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C, 1000 °C and 1050 °C. The measurement temperature range was between 800 °C and 500 °C in stationary air. Results converted to electrode surfaces area.
-
Impact of strontium non-stoichiometry of SrxTi0.3Fe0.7O3-δ on structural, electrical, and electrochemical properties for potential oxygen electrode of intermediate temperature solid oxide cells
PublicationThis work presents the results of a comprehensive study on the impact of the A-site non-stoichiometry of SrxTi0.3Fe0.7O3-δ (x = 0.90, 0.95, 1.00, 1.05) ceramics on their physicochemical properties. The materials were fabricated by the conventional solid-state reaction method and their structure was determined by X-ray diffractometry, X-ray photoelectron spectroscopy and electron microscopy. Their sintering and thermal expansion...
-
Structural and electrical properties of Cr-doped SrTiO 3 porous materials
PublicationSeries of single-phase materials with assumed formula SrTi1−xCrxO3 (where x = 0, 1, 4, 6 mol.%) were obtained by sol-gel method. The structure and microstructure of materials were characterised by X-ray diffraction and scanning electron microscopy methods. Moreover, the study of electrical properties and evaluation of chemical stability in CO2/H2O atmosphere was performed by electrochemical impedance spectroscopy and thermogravimery...
-
Electrochemical properties of porous Sr0.86Ti0.65Fe0.35O3 oxygen electrodes in solid oxide cells: Impedance study of symmetrical electrodes
PublicationThis work evaluates porous Sr0.86Ti0.65Fe0.35O3 (STF35) as a possible oxygen electrode material for Solid Oxide Cells. The powder synthesis was performed by solid state method. Characterization included DC electrical conductivity study of sintered bulk samples and impedance spectroscopy study of symmetrical electrodes deposited on gadolinium doped ceria substrates. Measurements were carried out in atmospheres with different pO2...
-
Correlation between structural and electrical properties in highly porous (Y,Sr)(Ti,Nb)O3-delta SOFC anodes
PublicationIn order to find a relationship between structural and electrical properties, niobium and yttrium doped SrTiO3 ceramics were prepared via solid-state reaction. The samples were sintered in hydrogen and air conditions. The samples were also fabricated with a pore-former to obtain highly porous specimens. The electrical properties of Nb-doped SrTiO3 samples and yttrium and niobium co-doped SrTiO3 were compared. The comparable electrical...
-
Thin LSFO films for bolometers
PublicationPrzedstawiono metodę produkcji oraz temperaturowe zależności rezystancji cienkich warstw niestechiometrycznych tlenków (La,Sr)FeO3 (LSFO) przeznaczonych do zastosowań na detektory podczerwieni
-
Emisyjność warstw tlenków lantanowo-strontowo-kobaltowych LSCO i lantanowo-strontowo-żelazowych LSFO praeznaczonych na bolometry
PublicationPrzedstawiono metodę pomiaru oraz wyniki pomiarów emisyjności grubych warstw niestechiometrycznych tlenków LSFO i LSCO. Duża emisyjność jest korzystna przy zastosowaniu tych warstw na detektory IR.
-
Filip Kaźmierczak
People -
SEM images of symmetrical cell interface with Sr1.05Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at 800 °C, 900 °C and 1000 °C
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with Sr1.05Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at three different temperatures 800 °C, 900 °C and 1000 °C. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating...
-
Impact of strontium non-stoichiometry of SrxTi0.3Fe0.7O3-δ
Open Research DataThis dataset contains results of the research on the basis of which the Figures presented in the manuscript entitled "Impact of strontium non-stoichiometry of SrxTi0.3Fe0.7O3-δ on structural, electrical, and electrochemical properties for potential oxygen electrode of intermediate temperature Solid Oxide Cells" were prepared. A detailed description...
-
SEM images of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen
Open Research DataThe dataset presents SEM images of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen. The powders were synthesized via the Pechini method. The reduction was performed in order to force the exsolution process of metallic nanoparticles.
-
Thermogravimetric analysis (TGA) of the SrxTi0.30Fe0.70O3-d materials
Open Research DataThis dataset contains results of thermogravimetric analysis (TGA) fot SrxTi0.30Fe0.70O3-d materials (x=0.90, 0.95, 1.00 and 1.05). The TGA experiments were carried out using a microbalance (CI Precision MK5) in the temperature range between 900 °C and 200 °C. During the whole measurement procedure, air was fed to the furnace chamber at a flow rate of...
-
The XRD diffraction patterns of as-prepared (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Fe, Ni) materials
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Fe, Ni) materials were synthesized via the Pechini method. First, the reagents in the form of nitrates were weighed and dissolved in DI water. In another beaker, a stoichiometric amount of titanium (IV) butoxide (Ti(OBu)4) was mixed together with reagent-grade ethylene glycol (EG), and citric acid (CA)...
-
SEM images of Solid Oxide Fuel Cell interface with La0.6Sr0.4Co0.2Fe0.8O3-δ oxygen electrodes sintered at 1050 °C before and after test
Open Research DataThis dataset contains cross section SEM images of Solid Oxide Fuel Cell interface with La0.6Sr0.4Co0.2Fe0.8O3-δ oxygen electrode sintered at 1050 °C before and after test. The cell was tested using Open Flanges™ test Set-up at 700 °C. During the test, the cell was aged for approximately 120 hours at a load of 0.5 A/cm^2. Images were obtained using...
-
SEM images of (La0.3Sr0.6Ce0.1)0.9(Me1Me2Ti)O3-δ (Me1,Me2=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen
Open Research DataThe dataset presents SEM images of (La0.3Sr0.6Ce0.1)0.9(Me1Me2Ti)O3-δ (Me1,Me2=Co, Fe, Ni) powder materials after reduction at 1000 deg.C in hydrogen. The powders were synthesized via the Pechini method. The reduction was performed to force the exsolution process of bimetallic nanoparticles.
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 1000 deg.C in hydrogen
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
The XRD diffraction patterns of as-prepared (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials synthesized via the solid state reaction method
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
SEM images of symmetrical cell interface with Sr0.90Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at 800 °C, 900 °C and 1000 °C
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with Sr0.90Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at three different temperatures 800 °C, 900 °C and 1000 °C. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating...
-
SEM images of Solid Oxide Fuel Cell interface with Sr0.95Ti0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C before and after test
Open Research DataThis dataset contains cross section SEM images of Solid Oxide Fuel Cell interface with Sr0.95Ti0.30Fe0.70O3-d oxygen electrode sintered at 800 °C before and after test. The cell was tested using Open Flanges™ test Set-up at 700 °C. During the test, the cell was aged for approximately 120 hours at a load of 0.5 A/cm^2. Images were obtained using a FEI...
-
Dilatometry results of SrxTi0.30Fe0.70O3-d materials
Open Research DataThis dataset contains results of dilatometry measurements of SrxTi0.30Fe0.70O3-d (x=0.90, 0.95, 1.00 and 1.05) materials. The investigation of the linear thermal expansion was carried out using a Netzsch DIL402 dilatometer. The SrxTi0.30Fe0.70O3-d powder was formed into cylinders and heat up to 1100 °C with a heating rate of 5 °C min−1, dwelled for...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 1100 deg.C in hydrogen
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
The XRD diffraction patterns of as-prepared (La0.3Sr0.6Ce0.1)0.9Ni0.05Me0.05Ti0.9O3-δ (Me= Co, Fe, Cu) materials
Open Research DataThe ((La0.3Sr0.6Ce0.1)0.9Ni0.05Me0.05Ti0.9O3-δ (Me= Co, Fe, Cu) materials were synthesized via the Pechini method. First, the reagents in the form of nitrates were weighed and dissolved in DI water. In another beaker, a stoichiometric amount of titanium (IV) butoxide (Ti(OBu)4) was mixed together with reagent-grade ethylene glycol (EG), and citric acid...
-
SEM images of (La0.3Sr0.6Ce0.1)0.9FexTi(1-x)O3-δ (x=0.1, 0.2 and 0.3) materials after reduction at 900 deg.C in hydrogen
Open Research DataThe dataset presents SEM images of (La0.3Sr0.6Ce0.1)0.9FexTi(1-x)O3-δ (x=0.1, 0.2 and 0.3) powder materials synthesized via the Pechini method after reduction in hydrogen at 900C for 10h.
-
SEM images of symmetrical cell interface with Sr0.95Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at 800 °C, 900 °C and 1000 °C
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with Sr0.95Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at three different temperatures 800 °C, 900 °C and 1000 °C. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating...
-
X-ray diffraction patterns of BaCe0.6Zr0.2Y0.1M0.1O3-δ (M = Fe, Pr, Tb)
Open Research DataThe dataset consists of three raw X-ray diffraction (XRD) files collected using a Phillips X’Pert Pro diffractometer (CuKα radiation (𝜆 = 1.541 Å), under 40 kV and 30 mA). The diffraction patterns of BaCe0.6Zr0.2Y0.1Fe0.1O3-δ (BCZYFe), BaCe0.6Zr0.2Y0.1Pr0.1O3-δ (BCZYPr), and BaCe0.6Zr0.2Y0.1Tb0.1O3-δ (BCZYTb) were collected at room temperature. Collected...
-
SEM images of symmetrical cell interface with Sr1.00Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at 800 °C, 900 °C and 1000 °C
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with Sr1.00Ti0.30Fe0.70O3-d electrodes and CGO-20 substrate sintered at three different temperatures 800 °C, 900 °C and 1000 °C. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating...
-
SEM images of symmetrical cell interface with SrTi0.30Fe0.70O3-d electrode and CGO-20 substrate in function of sintering temperature
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.30Fe0.70O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
Area specific resistance (at 800 °C - 500 °C) of the SrTi0.50Fe0.50O3 porous oxygen electrodes sintered at different temperatures
Open Research DataIn this dataset are presented results of the polarization resistance of differently sintered SrTi0.50Fe0.50O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to...
-
SEM image and EDS map of SrTi0.50Fe0.50O3-d powder aglomerate
Open Research DataThis dataset contains image of the SrTi0.50Fe0.50O3-d powder aglomerate with EDS map analysis results. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 10 kV in a high vacuum mode. The chemical compositions of the investigated powder were determined...
-
SEM image and EDS map of SrTi0.65Fe0.35O3-d powder aglomerate
Open Research DataThis dataset contains image of the SrTi0.65Fe0.35O3-d powder aglomerate with EDS map analysis results. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 10 kV in a high vacuum mode. The chemical compositions of the investigated powder were determined...
-
SEM images of symmetrical cell interface with SrTi0.65Fe0.35O3-d electrode and CGO-20 substrate in function of sintering temperature
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.65Fe0.35O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
Distribution of Relaxation Times analysis results of impedance measured in function of temperature on porous SrTi0.50Fe0.50O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results of Distribution of Relaxation Times analysis (DRT) of impedance of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at 800 °C. Electrochemical impedance spectroscopy were measured at 800 °C; 750 °C and 700 °C (syntetic air). The DRTTools Matlab GUI, available from prof. Ciucci’s group, was used...
-
SEM images of symmetrical cell interface with SrTi1-xFexO3-d electrodes and CGO-20 substrate sintered at 800 °C
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi1-xFexO3-d (x=0.35; 0.50; 0..70) electrodes and CGO-20 substrate sintered at 800 °C. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage of 12 kV in a high vacuum...
-
SEM image and EDS map of SrTi0.50Fe0.50O3-d porous electrode sintered at 800 °C
Open Research DataThis dataset contains image of the SrTi0.50Fe0.50O3-d porous electrode sintered at 800 °C with EDS map analysis results. This study were performed for better understanding the chemical composition of flat like structures that occurs in electrode. Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope...
-
Series resistance (at 800 °C - 500 °C) of the SrTi0.50Fe0.50O3 porous oxygen electrodes sintered at different temperatures
Open Research DataIn this dataset are presented results of the ohmic contribution of differently sintered Sr0Ti0.50Fe0.50O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic ari flow (21% O2, 40 ml min-1). Results converted to electrode...
-
Influence of sintering temperature of porous SrTi0.30Fe0.70O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.50Fe0.50O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Distribution of Relaxation Times analysis results of impedance measured at 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures
Open Research DataThis dataset contains results of Distribution of Relaxation Times analysis (DRT) of impedance of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures (800 °C, 900 °C and 1000 °C). Electrochemical impedance spectroscopy were measured at 700 °C (syntetic air). The DRTTools Matlab GUI, available from prof....
-
Area specific resistance (at 800 °C - 500 °C) of the SrTi0.30Fe0.70O3 porous oxygen electrodes sintered at different temperatures
Open Research DataIn this dataset are presented results of the polarization resistance of differently sintered SrTi0.30Fe0.70O3 porous oxygen electrodes in symetrical cell. Applied sintering temperatures were 900 °C, 950 °C and 1000 °C. The measurement temperature range was between 800 °C and 500 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to...
-
Comparisson of area specific resistance of the SrTi1-xFexO3-d porous oxygen electrodes and state-of-the-art LSCF sintered at optimal conditions
Open Research DataIn this dataset are presented results of the polarization resistance of optimaly sintered SrTi1-xFexO3-d porous oxygen electrodes in symetrical cell (1000 °C; 800 °C and 800°C respectively x = 0.35; 0.50 and 0.70). For commparison were selected commercially avilable state-of-the-art LSCF (Europa) sintered at 1050 °C. The measurement temperature range...
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.65Fe0.35O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Electrical conductivity of the SrTi1-xFexO3-d pellets at 20% pO2
Open Research DataThis dataset contains results electrical conductivity measurements of dense SrTi1-xFexO3-d (x=0.35, 0.50, 0.70) pellets. DC electrical conductivity measurements were performed by the Van der Pauw method between 900 °C and 200 °C. Studies were performed at 20% of oxygen partial pressure under humidified (~4 vol%) gas flow rate of 50 ml min -1.
-
Distribution of Relaxation Times analysis results of impedance measured in function of temperature on porous SrTi0.30Fe0.70O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results of Distribution of Relaxation Times analysis (DRT) of impedance of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. Electrochemical impedance spectroscopy were measured at 800 °C; 750 °C and 700 °C (syntetic air). The DRTTools Matlab GUI, available from prof. Ciucci’s group, was used...
-
SEM images of symmetrical cell interface with SrTi0.50Fe0.50O3-d electrode and CGO-20 substrate in function of sintering temperature
Open Research DataThis dataset contains images of polished cross section of symmetrical cell interface with SrTi0.50Fe0.50O3-d electrode and CGO-20 substrate in function of sintering temperature (800 °C, 900°C and 1000 °C) . Images were obtained using a PhenomXL (Thermo Fisher Scientific, the Netherlands) scanning electron microscope (SEM) with an accelerating voltage...
-
Electrical conductivity of the (Ce0.80Gd0.20)O1.90 pellet at different oxygen partial pressures
Open Research DataThis dataset contains results electrical conductivity measurements of dense (Ce0.80Gd0.20)O1.90 (CGO-20) pellet. DC electrical conductivity measurements of CGO-20 were performed by the Van der Pauw method between 900 °C and 450 °C with 50 °C step. Studies were performed at different oxygen partial pressures (100%, 20% and 1%) under humidified (~4...
-
Influence of sintering temperature of porous SrTi0.50Fe0.50O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.