mgr inż. Ariel Lenarciak
Zatrudnienie
-
High temperature linear impedance of 35P2O5-30Fe2O3-25Nb2O5-15TiO2
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%,...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-35Nb2O5 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH) and Nb2O5 (≥99.9%, PLUKA AG) were...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
High temperature linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
High temperature linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-20Nb2O5-15TiO2
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and...
-
Linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2 (≥99.9%, anatase...
-
Topography of iron-phosphate glasses doped with niobium and titanium tested by confocal microscope
Dane BadawczeThe topography of phosphate-iron glasses containing niobium and titanium were investigated with the use of confocal miscroscope. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5, 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 and 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents...
wyświetlono 1233 razy