Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 4.03 mm was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 4.03 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 2.91 mm was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.91 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at 273 K
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of as-quenched 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 annealed glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm (after second heat-treatment at 913 K) was measured at high temperature range with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm (after second heat-treatment at 913 K) was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 fully crystallized glass at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 partially crystallized glass at 613 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 partially crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 593 K was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage and temperature for Bi2VO5.5 ceramic of thickness 2.52 mm (after first heat-treatment at 913 K) was measured at different frequencies with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 473 K for 3 h measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 473 K for 3h was measured by impedance spectroscopy method.
-
Electrochemical Impedance Spectroscopy data of PDA-modified TiO2 nanotubes
Dane BadawczeThis dataset contains Electrochemical Impedance Spectroscopy data of the samples from TiO2 nanotubes modified with polydopamine. The studies were presented as a part of the research on "Band Gap Engineering toward Semimetallic Character of Quinone-Rich Polydopamine" (DOI: 10.1021/acs.jpcc.2c08804).
-
Impedance spectroscopy of the lithium titanate doped by copper thin films
Dane BadawczeLithium titanate doped by copper thin films were derived by sol-gel method. Prepared gel was deposited by spin-coating technique. Samples with various content of Cu were measured by impedance spectroscopy method in a wide range of temperature, from -120 up to 150 deg.
-
Linear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glass-ceramics containing BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
The electrochemical impedance spectroscopy studies of cataphoretic-grown epoxy-based coatings
Dane BadawczeThe dataset contains electrochemical impedance spectroscopy spectra collected for epoxy-based cataphoretic coatings in order to determine the offered anti-corrosion protection. Particular spectra pertain to the coatings applied for the different magnitude of polarization potential imposed, namely 10V, 20V and 30V. The results were obtained within the...
-
Thermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with DSC
Dane BadawczeThermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by DSC.
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-35Nb2O5 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH) and Nb2O5 (≥99.9%, PLUKA AG) were...
-
Model dynamic electrochemical impedance spectroscopy (DEIS) results obtained with various DC polarization rates
Dane BadawczeThe dataset contains results of model dynamic electrochemical impedance spectroscopy studies carried out on a setup of 10 diodes in series, which were connected in parallel with a condenser. The impedance data were acquired every 1 s (the analytic window length for Fourier Transform was 1 s). The model system was polarized between 0 and +8 V with DEIS...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
Influence of sintering temperature of porous SrTi0.30Fe0.70O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Influence of sintering temperature of porous SrTi0.50Fe0.50O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Influence of sintering temperature of porous SrTi0.65Fe0.35O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
The voltage across and current through the RC model object tested using pulse excitation in impedance spectroscopy measurement method
Dane BadawczeThe raw data (voltage across and current through RC model object ) obtained using pulse excitation EIS impedance spectroscopy measurement method. The data was acquired using 12-bit ADC (LTC1420) with sampling frequency changed in time segments. The 1V voltage pulse excitation duration was set to 0.1s and the total acqusition time was set to 1000s. For...
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.50Fe0.50O3-d oxygen electrode sintered at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.65Fe0.35O3-d oxygen electrode sintered at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrode sintered at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 800 °C and 15% oxygen partial pressure
Dane BadawczeThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 100% oxygen partial pressure
Dane BadawczeThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 100% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 20% oxygen partial pressure
Dane BadawczeThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 20% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 5% oxygen partial pressure
Dane BadawczeThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 5% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included. Results...
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 600 °C and 15% oxygen partial pressure
Dane BadawczeThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 600 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included. Results converted...
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 15% oxygen partial pressure
Dane BadawczeThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Nonlinear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...