Technical fabrics sample 1
Dane BadawczeThe data presented here includes 3 videos of technical fabrics strength testing. The included movies are in .cine format, and an external program with a viewer for such movies is required.
-
Technical fabrics sample 2
Dane BadawczeThe data presented here includes 3 videos of technical fabrics strength testing. The included movies are in .cine format, and an external program with a viewer for such movies is required.
-
Mechanical durability and electroanalytical performance of 3D-printed multi-material sensors
Dane BadawczeThe data set consists tensile strength, electric resistance, electrochemical characteristics and physicochemical studies of multi-material 3D printed systems, including their sensing performance during detection of antibiotics in an industrial sewage. Additionally, contact angle measurements and SEM micrographs of the electrode surfaces were included.
-
The effect of wax foundation addition to PCL filaments on mechanical properties.
Dane BadawczeThe dataset includes the effect of wax foundation addition on the basic mechanical properties of the filaments. PCL and wax foundation addition at 10 and 15% were used for extrusion. The mechanical properties of the resulting filaments were evaluated by a double compression test using an Instron model 5543 universal testing machine. Parameters such...
-
Difficulties in financing innovation - research results
Dane BadawczeThe SME sector determines the strength of the Polish economy, still faces many barriers in running a business, they can be social and market barriers, for example: financial barriers, low employee mobility, or limited access to financing sources: legal barriers that result from economic policy difficult for the sector, or conservative economic policy.
-
Tensile curve of E grade steel for shipbuilding
Dane BadawczeIn the shipbuilding industry, the risk of brittle fractures developing in constructions is limited by employing certified materials of specific impact strength, determined using the Charpy method (for a given design temperature) and by exercising control over the welding processes (technology qualification, supervision of production, tests of non-destructive...
-
Opposite pressure impact on electron-phonon coupling in Eu2+ and Ce3+ doped AlN
Dane BadawczeThis data analyzes the influence of pressure on electron–lattice interactions in the 5d excited states of Ce3+ and Eu2+ in the AlN host based on pressure-dependent photoluminescence and photoluminescence excitation spectra. High-pressure measurements on AlN samples doped with Eu2+ and Ce3+ ions reveal that the Stokes shift increases with pressure for...
-
Measurements of radiation emission of a portable power bank with a capacity of 10400 mAh
Dane BadawczeThe dataset contains the emission measurement results that are part of comprehensive tests carried out for portable power banks with different capacities. The measurements were performed in the frequency range from 30 MHz to 3 GHz using a Gigahertz Transverse Electromagnetic (GTEM) cell (Fig. 1). The test setup was configured to measure a portable power...
-
The radiated immunity test of an astable multivibrator at over-normative field strengths
Dane BadawczeThe dataset presents a result of measurements that are a part of electromagnetic field immunity tests. The radiated, radio frequency, immunity tests were carried out for a typical astable electronic multivibrator. Tests of immunity of electronic systems to radiated radio frequency (RF) disturbances in the frequency range from 80 MHz to 1 GHz were performed...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 60mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 40mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - Charpy impact test reslut in vary tempetatures
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 40mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 50mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - tensile test record
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 50mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - 3D fracture scan
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 60 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
Measurements of radiation emission of a portable power bank with a capacity of 5200 mAh
Dane BadawczeThe dataset contains the emission measurement results that are part of comprehensive tests carried out for portable power banks with different capacities. The measurements were performed in the frequency range from 30 MHz to 3 GHz using a Gigahertz Transverse Electromagnetic (GTEM) cell. The test setup was configured to measure a portable power bank...
-
Measurements of radiation emission of a portable power bank with a capacity of 2600 mAh
Dane BadawczeThe dataset contains the emission measurement results that are part of comprehensive tests carried out for portable power banks with different capacities. The measurements were performed in the frequency range from 30 MHz to 3 GHz using a Gigahertz Transverse Electromagnetic (GTEM) cell. The test setup was configured to measure a portable power bank...
-
Areas of updraft air motion from WRF model simulations.
Dane BadawczePresented dataset is a part of numerical modelling study focusing on the analysis of sea ice floes size distribution (FSD) influence on the horizontal and vertical structure of convection in the atmosphere. The total area and spatial arrangement of the updrafts indicates that the FSD affects the total moisture content and the values of area averaged...
-
The magnetic field measurements in selected places of the industrial building
Dane BadawczeThe dataset is part of a comprehensive study on the assessment of the electromagnetic field intensity in a building of an operating industrial plant. Detailed results of magnetic field measurements, carried out in selected places of this building, are presented.
-
Electric field maps of an astable multivibrator in frequency range from 30 MHz to 3 GHz
Dane BadawczeThe data presents a result of near field measurements of electromagnetic emissions radiated from the PCB of a small electronic device. An efficient method of modelling the magnetic and electric field emissions is the measurements in the near field using electric and magnetic probes. The attached files contain electric field maps created on based measurements...
-
The radiated immunity test of an astable multivibrator for various supply voltages
Dane BadawczeThe dataset presents a result of measurements that are a part of electromagnetic field immunity tests. The radiated, radio frequency, immunity tests were carried out for a typical astable electronic multivibrator supplied from a power supply with an output voltage of 6V and 7.5 V. Tests of immunity of electronic systems to radiated radio frequency (RF)...
-
The radiated immunity test of an astable multivibrator in the frequency range from 100 MHz to 300 MHz
Dane BadawczeThe dataset presents a result of measurements that are a part of electromagnetic field immunity tests. The radiated, radio frequency, immunity tests were carried out for a typical astable electronic multivibrator. Tests of immunity of electronic systems to radiated radio frequency (RF) disturbances in the frequency range from 100 MHz to 300 MHz were...
-
Finite element models used in diagnostics of transverse cracks in bridge approach pavement
Dane BadawczeTransverse cracks in the asphalt pavement were observed on bridge structures next to single-module expansion joints with a 5 meter approach slab set at the depth of 1 m. The finite element (FE) models of the approach pavement were created to investigate the reasons of premature cracking and crack initiation mechanism over the back edge of the abutment...