Filtry
wszystkich: 124
wybranych: 6
Filtry wybranego katalogu
Wyniki wyszukiwania dla: BATCH BLENDING CHAMBER SWIRLING DIFFUSER BLENDING TIME
-
Data from pizoelectric pressure sensor placed inside PWK pump chamber
Dane BadawczeThe dataset contains raw data acquired from a piezoelectric pressure sensor placed inside PWK pump chamber. Pumping pressure was 10MPa, displacement was set to 100%, oil temperature was 33C. Columns "Czas" stand for a time in seconds and milliseconds, "Napięcie" stands for Voltage in Volts
-
Kinetics of cyclohexane removal by Candida subhashii and Fusarium solani
Dane BadawczeDataset presents cyclohexane biodegradation in gas phase using two species of microorganisms: Candida Subhashii and Fusarium solani. Biodegradation was carried out in sealed chambers with a capacity of 1000 ml. In each of them there are two discs inhabited with microorganisms, made of polyurethane foam, 80 mm in diameter and 20 mm thick.
-
The experimental results of diesel fuel spray with marine engine injector
Dane BadawczeThe data set presents the measurement of the diesel fuel spray from with marine engine injector. The main target presents results is a study of the time course of macro parameters (spray tip penetration, spray cone angle) of fuel spray in the cylinder of marine diesel engine. The impact of ambient conditions and the geometrical parameters of the injector...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 4-8h.
Dane BadawczeWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 4-8h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h.
Dane BadawczeWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h. High frequency burst recording.
Dane BadawczeWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. High frequency burst recording.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21,...