Filters
total: 711
filtered: 169
Search results for: PLATE
-
Nonlinear impedance of vanadate glass-ceramics containing BaTiO3
Open Research DataThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
The structure of Bi2VO5.5 ceramic prepared by 3 different ways measured with X-ray diffraction
Open Research DataThe structure of Bi2VO5.5 ceramics was measured by XRD.
-
Thermal properties of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides measured with DSC method
Open Research DataThermal properties of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides was measured by DSC.
-
Thermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with DSC
Open Research DataThermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by DSC.
-
The morphology of lead-silicate glasses containing nanocrystallites of iron oxides
Open Research DataThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
The structure of lead-silicate glasses containing nanocrystallites of iron oxides
Open Research DataThe structure of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All samples were prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
The topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with SEM method
Open Research DataThe topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. was measured by SEM.
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-35Nb2O5 glass
Open Research DataThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH) and Nb2O5 (≥99.9%, PLUKA AG) were...
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 40Na2O-20CaO-40P2O5 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 40Na2O-20CaO-40P2O5 glass was measured by impedance spectroscopy method.
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Elastic wave propagation signals in concrete cube (experimental and calculated using discrete element method)
Open Research DataThe DataSet contains the results of the elastic wave propagation. Both experimental and numerical signals were obtained for the concrete cube with dimensions of 50 × 50 × 50 mm3. The specimen was made of concrete with called mortar concrete. The ingredients of the concrete mix were as follows: CEM I 42.5R (500 kg/m3), sand 0 – 2 (1500 kg/m3) and water...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 glass
Open Research DataThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
The structure of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides measured with X-ray diffraction method
Open Research DataThe structure of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides was measured by XRD.
-
The structure of strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with X-ray diffraction and SEM methods
Open Research DataThe structure of strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by XRD and SEM.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Open Research DataNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Electrical properties of nanostructures in lead-silicate glasses and nanocomposites doped with iron oxide
Open Research DataElectrical properties of iron oxide nanostructures observed in silicate glasses and glass-ceramics were studied. Two different sets of glass samples were prepared. The first group of samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO– xFe2O3, where x = 15, 20 and 25 (in mol%). Composition of the second group was 50SiO2–(50−x)PbO–xFe2O3, where...
-
Magnetic properties of of lead-silicate glasses and nanocomposites doped with iron oxide
Open Research DataMagnetic properties of iron-doped glasses and glass-ceramics were studied. Two different sets of glass samples were prepared. The first group of samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO– xFe2O3, where x = 15 and 20 (in mol%). Composition of the second group was 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All sampleswere...
-
Linear and nonlinear impedance of iron containing silicate glasses
Open Research DataThe linear and nonlinear impedance ofglasses doped with iron oxide were measured. Glass samples (50 SiO2-50-xPbO-xFe2O3 in mol%) were prepared by the conventional melt quenching technique. The substrates were powdered in a mortar and melted in Al2O3 crucibles. The melting was conducted in air at 1623K. The melts were poured out on plate heated up to...
-
Linear impedance of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Open Research DataNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 613 K was measured by impedance spectroscopy method.
-
Electrical properties of silicate-lead glasses containing nanostructures of iron oxides.
Open Research DataElectrical properties of silicate-lead glasses doped with different content of iron oxide was studied. The set of glass samples were prepared with the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in...
-
Linear impedance of 1SiO2–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 1SiO2–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Effects of liquid phase modification on the values of surface tension of trickling liquid
Open Research DataDataset presents the values of surface tension of trickling liquid sampled from three running biotrickling filters.
-
The topography of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides measured with SEM method
Open Research DataThe topography of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides was measured by SEM.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 annealed glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of as-quenched 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for fully crystallized 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for fully crystallized 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched glass 40Bi2VO5.5-60SrB4O7 after full crystallization was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of as-quenched glass 40Bi2VO5.5-60SrB4O7 afetr full crystallization was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 473 K for 3 h measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 473 K for 3h was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for annealed at 593 K and next fully crystallized 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of glass 40Bi2VO5.5-60SrB4O7 annealed at 473 K for 3h and next fully crystallized was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.