Wyniki wyszukiwania dla: FATIGUE FRACTURE
-
Experimental study of the impact of notches and holes made in the front edge of adherends on the properties of static and fatigue strength of adhesive joints
PublikacjaThe paper presents the results of experimental studies aimed at determining the effect of holes and notches at the front edge of adherends on the strength of adhesive joints. Single-lap joints made of S235JR steel sheets joined with Araldite 2014-2 epoxy adhesive were tested. Comparative tests of static strength in the shear test as well as high-cycle fatigue strength tests were carried out. Joints with three holes with a diameter...
-
The effect of elevated temperature on LCF damage growth in 2024AA – Experiment and modeling
PublikacjaThis paper presents the results of experimental low-cycle fatigue (LCF) tests conducted on EN-AW 2024 alloy in T3511 temper at 100 ◦C, 200 ◦C and 300 ◦C. The material’s basic fatigue characteristics were determined, such as fatigue life curve and cyclic strain curve. Both the hysteresis loop and nature of fracture surfaces obtained in macro- and microscopic observations (scanning electron microscope, SEM) were accounted for. The...
-
The effect of preliminary creep-strain on material behavior under LCF tension/compression and pure torsion regimes
PublikacjaThis paper presents the results of experimental tests of monotonic tension and torsion, creep-rupture and preliminary creep at 200C and 300C, as well as low-cycle fatigue of 2024 T3511 aluminum alloy. The fatigue process was conducted at room temperature for uniaxial tension/compression and torsion. The as-received material and pre-deformed material were also investigated during creep at elevated temperature. Basic monotonic,...
-
Analysis of Ceramic Elements with Ring-Crack Defects in Lubricated Rolling Contact
PublikacjaThe properties of ceramics, specifically low density, high hardness, high temperature capability and low coefficient of thermal expansion are of most interest to rolling element manufacturers. Surface ring cracks on lubricating rolling contact fatigue failure has been studied using numerical fracture analysis. Such cracks are very often found on ceramic bearing balls and decrease fatigue life rapidly. The numerical calculations...
-
On the durability of the hydraulic satellite motor working mechanism in overload condition
PublikacjaThe paper presents the newest construction of the hydraulic satellite pump/motor. In this study, the fracture of the hydraulic satellite motor working mechanism is investigated. Factors influencing the durability of satellite working mechanism have been described. The durability of the hydraulic satellite motor working mechanism at a load, corresponding to a pressure of 15 MPa supplied with refined rapeseed oil is very low. Analyses...
-
Numerical analysis of crack propagation in silicone nitride
PublikacjaThe properties of ceramics, specifically low density, high hardness, high temperature capability and low coefficient of thermal expansion are of most interest to rolling element manufacturers. The influence of ring crack size on rolling contact fatigue failure has been studied using numerical fracture analysis. Such cracks are very often found on ceramic bearing balls and decrease fatigue life rapidly. The numerical calculation...
-
Mechanical properties of VL E27 steel for shipbuilding – fracture documentation (test in -20°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture documentation (test in +20°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture documentation (test in 0°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical Properties of Additively Manufactured Polymeric Materials—PLA and PETG—For Biomechanical Applications
PublikacjaThe study presented herein concerns the mechanical properties of two common polymers for potential biomedical applications, PLA and PETG, processed through fused filament fabrication (FFF)—Material Extrusion (ME). For the uniaxial tension tests carried out, two printing orientations—XY (Horizontal, H) and YZ (Vertical, V)—were considered according to the general principles for part positioning, coordinates, and orientation typically...
-
LCF behavior of 2024AA under uni- and biaxial loading taking into account creep pre-deformation
PublikacjaThis study presents the results of experimental low-cycle fatigue (LCF) tests of aluminum 2024 alloy T3511 temper in uni- and biaxial loading states. Tests were carried out on both the as-received material (hardened extruded rods) and material with different pre-deformation histories. These deformations were carried out in the creep process at 200 °C and 300 °C for two different levels of at each temperature. The pre-deformed material’s...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - tensile test record
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - 3D fracture scan
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - Charpy impact test reslut in vary tempetatures
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 60 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
Effect of austempering temperature on microstructure and cyclic deformation behaviour of multiphase low-carbon steel
PublikacjaThis paper examined the cyclic deformation behaviour of multiphase low-carbon steel that was subjected to austempering heat treatments at four temperatures (190 °C, 230 °C, 275 °C, and 315 °C) below the martensite start temperature (Ms = 353 °C). The tests were conducted at room temperature, under fully reversed strain-controlled conditions, with strain amplitudes in the range 0.5–1.0%. The microstructure was observed by transmission...
-
Application of Structural Control Systems for the Cables of Cable-Stayed Bridges: State-of-the-Art and State-of-the-Practice
PublikacjaStay cables are one of the key elements of cable-stayed bridges and are characterized by lightweight, low inherent damping, and high flexibility. They are continuously subjected to small-to large-amplitude vibrations due to various types of dynamic loads that may, in the long term, cause fatigue and fracture problems for the cable system, and may eventually compromise the safety of cable-stayed bridges. Thus, several countermeasures...
-
Fatigue Bending of V-Notched Cold-Sprayed FeCoCrNiMn Coatings
PublikacjaCold-spray coatings were produced by FeCoCrNiMn high-entropy alloy powders deposited on carbon steel substrate. The coatings were realized at intermediate temperature and high pressure (at 1100 °C and 7 MPa). The coating microstructure was characterized by scanning electron microscopy and X-ray diffraction, revealing a very dense deposition and high flattening ratio of the splatted particles. This had a large influence on the...
-
Effect of processing parameters on the cyclic behaviour of aluminium friction stir welded to spark plasma sintered aluminium matrix composites with bimodal micro-and nano-sized reinforcing alumina particles
PublikacjaUnderstanding the cyclic behaviour of Alumina reinforced Aluminium composites (Al-A2O3) was of critical importance, for their further application in the different industrial sectors. The present study is focussing on the cyclic behaviour of the Al-Alumina nanocomposite produced through the combination of spark plasma sintering (SPS) method and friction stir welding (FSW). The added Alumina with total content of 10% is the combination...
-
The energy approach to fatigue crack growth of S355 steel welded specimens subjected to bending
PublikacjaThe study presents the results of the research on the rate of fatigue crack growth subjected to bending in the ferritic-pearlitic structure. The studies were carried out at a constant amplitude of the moment and at various values of the load ratios R and at the operating frequency of the machine of 28.4 Hz. Flat specimens made of S355 steel and with fillet welds and with double-sided blunt external notches as well as concave...