Filters
total: 44
filtered: 37
Chosen catalog filters
Search results for: nanoindentation
-
Nanoindentation tests titanium alloy Ti-6Al-4V after interference laser treatment
PublicationThe study aimed was to assess selected mechanical properties of surface layers obtained after interference laser treatment – DLIL of titanium alloy Ti-6Al-4V used for implants. The samples were melted in still air at room temperature, for this purpose Nd:YAG laser was used, the number of laser shots was variable. Next, nanoindentation tests were performed, based on which Young’s modulus and nanohardness in the obtained surface...
-
Application of the nanoindentation method in assessing of properties of cement composites modified with silica-magnetite nanostructures
Publication -
Mechanical Properties and Wear Susceptibility Determined by Nanoindentation Technique of Ti13Nb13Zr Titanium Alloy after “Direct Laser Writing”
PublicationLaser treatment has often been applied to rebuild the surface layer of titanium and its alloys destined for long-term implants. Such treatment has always been associated with forming melted and re-solidified thin surface layers. The process parameters of such laser treatment can be different, including the patterning of a surface by so-called direct writing. In this research, pulse laser treatment was performed on the Ti13Nb13Zr...
-
Microstructure and mechanical properties of laser surface-treated Ti13nb13zr alloy with MWCNTs coatings
PublicationLaser surface modification of titanium alloys is one of the main methods of improving the properties of titanium alloys used in implantology. This study investigates the microstructural morphology of a laser-modified surface layer on a Ti13Nb13Zr alloy with and without a carbon nanotube coating deposited by electrophoretic deposition. Laser modification was performed for samples with and without carbon nanotube coating for two...
-
The Influence of Nanometals, Dispersed in the Electrophoretic Nanohydroxyapatite Coatings on the Ti13Zr13Nb Alloy, on Their Morphology and Mechanical Properties
PublicationIn this work, nanohydroxyapatite coatings with nanosilver and nanocopper have been fabricated and studied. The presented results concern coatings with a chemical composition that has never been proposed before. The present research aims to characterize the effects of nanosilver and nanocopper, dispersed in nanohydroxyapatite coatings and deposited on a new, non-toxic Ti13Zr13Nb alloy, on the physical and mechanical properties of...
-
Influence of Surface Laser Treatment on Mechanical Properties and Residual Stresses of Titanium and its Alloys
PublicationSurface modification of the titanium and its alloys used in implantology with a long-pulse laser can change the surface topography, but it also leads to changes in the stress sign and magnitude in the resulting subsurface layer. The presented research was aimed at evaluating the state of stress after laser remelting with the Nd:YAG laser of pre-etched titanium alloys Ti6Al4V and Ti13Nb13Zr and pure titanium. The obtained surface...
-
Study of nanomechanical properties of (1-y)BST-yMgO thin films
PublicationIn the present study thin films of MgO – modified Ba0.6Sr0.4TiO3 (BST60/40) solid solution were prepared by the sol-gel-type chemical solution deposition method on stainless steel substrates. A multilayer spin-coating approach was utilized for the Ba0.6Sr0.4TiO3-MgO thin film deposition with subsequent thermal annealing at T=650-750C. Dried BST60/40-MgO gel powders were studied with thermogravimetric and differential thermal analysis...
-
Effects of electrophoretic deposition times and nanotubular oxide surfaces on properties of the nanohydroxyapatite/nanocopper coating on the Ti13Zr13Nb alloy
PublicationLoad-bearing implants are developed with a particular emphasis placed on an application of ceramic hydroxyapatite coatings in order, to enhance the bioactivity of titanium implants and to shorten the healing time. Therefore, thin, fully crystalline coatings that are, highly adhesive, hydrophilic and demonstrating antibacterial properties are ly looked for. The aim of this research was to develop and characterize the properties...
-
Hydrogen Embrittlement and Oxide Layer E ect in the Cathodically Charged Zircaloy-2
PublicationThe present paper is aimed at determining the less investigated effects of hydrogen uptake on the microstructure and the mechanical behavior of the oxidized Zircaloy-2 alloy. The specimens were oxidized and charged with hydrogen. The different oxidation temperatures and cathodic current densities were applied. The scanning electron microscopy, X-ray electron diffraction spectroscopy, hydrogen absorption assessment, tensile, and...
-
The Influence of the Depth of Cut in Single-Pass Grinding on the Microstructure and Properties of the C45 Steel Surface Layer
PublicationThe paper contains the results of a metallographic examination and nanoindentation test conducted for the medium carbon structural steel with low content of Mn, Si, Cu, Cr, and Ni after its grinding to a depth ranging from 2 μm to 20 μm, at constant cutting speed (peripheral speed) of vs = 25 ms−1 and constant feed rate of vft = 1 m/min. Applied grinding parameters did not cause the surface layer hardening, which could generate...
-
Physicochemical and Mechanical Performance of Freestanding Boron-Doped Diamond Nanosheets Coated with C:H:N:O Plasma Polymer
PublicationThe physicochemical and mechanical properties of thin and freestanding heavy boron-doped diamond (BDD) nanosheets coated with a thin C:H:N:O plasma polymer were studied. First, diamond nanosheets were grown and doped with boron on a Ta substrate using the microwave plasma-enhanced chemical vapor deposition technique (MPECVD). Next, the BDD/Ta samples were covered with nylon 6.6 to improve their stability in harsh environments and...
-
Effects of solution composition and electrophoretic deposition voltage on various properties of nanohydroxyapatite coatings on the Ti13Zr13Nb alloy
PublicationThe purpose of the research was to establish the influence of the solution composition and the electrophoretic deposition voltage on the coating homogeneity and thickness, nanohardness, adhesion, corrosion resistance and wettability. The Ti13Zr13Nb alloy was coated by the electrophoretic technique with hydroxyapatite in a solution containing 0.1, 0.2 or 0.5 g nanoHAp in 100 mL of suspension and at voltage 15, 30 or 50 V. The scanning...
-
The Influence of Laser Alloying of Ti13Nb13Zr on Surface Topography and Properties
PublicationThe laser alloying is a continually developing surface treatment because of its significant and specific structuration of a surface. In particular, it is applied for Ti alloys, being now the most essential biomaterials` group for load-bearing implants. The present research was performed on the Ti13Nb13Zr alloy subject to laser modification in order to determine the treatment effects on surface topography and its some mechanical...
-
Biological and mechanical research of titanium implants covered with bactericidal coating
PublicationThe paper concerns the biological and mechanical properties of titanium implants with an antibacterial coating. The Ti13Zr13Nb alloy samples were coated with hydroxyapatite (HAp) coatings using the electrophoretic deposition technique (EPD). Subsequently, the surface of the samples was modified with silver, copper, and nickel nanoparticles by the immersion method. Different titanium sample types (i.e. HAp-only and nanometals-enriched...
-
Effect of MAO coatings on cavitation erosion and tribological properties of 5056 and 7075 aluminum alloys
PublicationTwo ceramic coatings have been applied on 5056 and 7075 aluminum alloy by microarc oxidation (MAO) technology. The mass losses, surface morphologies and the phase constituents of the MAO coatings before and after cavitation tests were examined by means of digital scales, scanning electron microscopy (SEM) and X-ray diffraction (XRD), respectively. In order to assess the impact of the mechanical properties of the surface layer on...
-
Nanotubular oxide layers and hydroxyapatite coatings on ‘Ti–13Zr–13Nb’ alloy
PublicationThe presented research was aimed to determine the mechanical properties of the nanotubular oxide layer covered with hydroxyapatite coating. The Ti–13Zr–13Nb alloy was oxidised in 1M phosphoric acid with an addition of 0?5% HF for HF solution at 20 V voltage. The electrochemically assisted deposition of hydroxyapatite was performed at cyclic polarisation in NH4H2PO4 and CaCl2 solution at 80uC. The mechanical properties were determined...
-
Effect of plasma sprayed and laser re-melted Al2O3 coatings on hardness and wear properties of stainless steel
PublicationCommercially available austenic stainless steel substrate was coated with commercially available, raw Al2O3 powder applied by means of plasma spraying method and then re-melted with CO2 laser beam of various parameters. Tribological and mechanical properties of the 120 J/mm and 160 J/mm laser re-melted coatings were compared with the tribological and mechanical properties of the “as-sprayed” coating. The influence of the laser...
-
Prototype design and development of low-load-roof photovoltaic modules for applications in on-grid systems
PublicationFour prototypes of lightweight photovoltaic modules for applications in on-grid systems have been designed, developed, manufactured and tested for compliance with relevant IEC standards. Selected, commercially available materials characterized by thermogravimetry, differential scanning calorimetry, dilatometry, scanning electron microscopy and nanoindentation technique were used in frameless, adhesively-bonded sandwich-structures...
-
Mechanical Behavior of Bi-Layer and Dispersion Coatings Composed of Several Nanostructures on Ti Substrate
PublicationThree coatings suitable for biomedical applications, including the dispersion coating composed of multi-wall carbon nanotubes (MWCNTs), MWCNTs/TiO2 bi-layer coating, and MWCNTs-Cu dispersion coating, were fabricated by electrophoretic deposition (EPD) on Ti Grade II substrate. Optical microscopy, scanning electron microscopy, energy-dispersive X-ray spectroscopy, and nanoindentation were applied to study topography, chemical, and...
-
Influence of Two-Stage Anodization on Properties of the Oxide Coatings on the Ti–13Nb–13Zr Alloy
PublicationThe increasing demand for titanium and its alloys used for implants results in need of such innovative surface treatment that may jointly increase corrosion resistance and biocompatibility, and demonstrate antibacterial protection at no cytotoxicity. The purpose of this research was to characterize the effect of two-stage anodization, performed for 30 min in phosphoric acid, at the presence of hydrofluoric acid in the second stage....