Straightening of ship hull structure made of 316L stainless steel - microstructure of reference material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of reference material materia (transverse direction)
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of reference material materia (longitudinal direction)
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Rain Gardens LC_MS/MS analysis dataset
Dane BadawczeThis dataset contains the results of samples analysis (target analysis with certified reference materials) using ultra-high performance liquid chromatography tandem mass spectrometry (UHPLC-MS/MS, Shimadzu, Japan).
-
Refractive index measurement in the range of 1.3 – 1.5 for 1550 nm wavelength (2nd serie)
Dane BadawczeThe low-coherence refractive index measurements of certified liquid samples provided by Cargille Labs were performed. The measurement system consisted of a broadband light source (central wavelength of 1550 nm), an optical spectrum analyzer, a 2x1 fiber-optic coupler (50:50 power split), and single-mode telecommunication optical fibers. A micromechanical...
-
Refractive index measurement in the range of 1.3 – 1.5 for 1550 nm wavelength (1st serie)
Dane BadawczeThe low-coherence refractive index measurements of certified liquid samples provided by Cargille Labs were performed. The measurement system consisted of a broadband light source (central wavelength of 1550 nm), an optical spectrum analyzer, a 2x1 fiber-optic coupler (50:50 power split), and single-mode telecommunication optical fibers. A micromechanical...
-
Straightening of ship hull structure made of 316L stainless steel - microstructure of naturally colled material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - microstructure of water cooled material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of naturally cooled material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Paracetamol in Friction Ridge Skin Raman Spectra - Paracetamol Reference and from drugs 2023
Dane BadawczeRaman scatter spectra for paracetamol from different drugs and paracetamol reference.
-
Bio-based polyester polyols for polyurethane foams - chemical structure of reference sample
Dane BadawczePresented dataset includes the results of FTIR and H NMR spectroscopy of bio-based polyester polyol - poly(propylene succinate) (reference sample for materials obtained during MINIATURA 4 project realization).
-
3D knee model M with decreased material parameters of the cartilage and menisci - input text file for computation
Dane BadawczeThe finite element method was used to simulate the stance phase of the gait cycle. An intact knee model was prepared based on magnetic resonance scans of the left knee joint of a healthy volunteer. In the model M the material parameters of cartilage and menisci were reduced to simulate degenerative changes in the medial knee osteoarthritis. The file...
-
Deformation Sweep Test of Cement Bitumen Treated Material Mixture C3E5.5 (field obtained material; over 28 days of curing at 20C)
Dane BadawczeDataset presents data of results of deformation sweep test determined for cold recycled mixture – cement bitumen treated material mixture with following binding agents: 3% cement and 5.5% emulsion (C3E5.5). Mixture was designed according to Polish requirements for the base course of pavement. Mixture contains 60% of RAP material. Specimen size: f=100...
-
Acetaminophen in Friction Ridge Skin Raman Spectra - acetaminophen (paracetamol) Reference and from drugs 2023
Dane BadawczeRaman spectra for acetaminophen (paracetamol) from different drugs and paracetamol reference.
-
The effect of raw material type on endotoxin content .
Dane BadawczeThe datasets contain the results of determining the effect of raw material type on endotoxin content as well as the effect of purification methods. The endotoxin concentration was determined using the PyroGene Recombinant Factor C Endpoint Fluorescent Assay. Beckmann-Kenko sodium alginate and Chemat sodium salt of alginic acid were used for the assays....
-
Calculations of material factors for a set of 20 thermistors
Dane BadawczeThe presented data set is part of the research aimed at determining the actual characteristics of each thermistor in a package of twenty NTC10k type sensors.
-
Selection of material for infiltration of non-stoichiometric Sr0.95Ti0.3Fe0.7O3-δ
Dane BadawczeThe porous electrodes used for the infiltration were prepared from A-site non-stoichiometric Sr0.95Ti0.3Fe0.7O3-δ synthesized by the conventional solid state reaction method. Screen printed electrodes (0.5 cm2) on CGO-20 substrate, were fired at 800 °C for 2 hours in an air atmosphere. Infiltration of the scaffolds was performed by a water-based precursor...
-
Mechanical durability and electroanalytical performance of 3D-printed multi-material sensors
Dane BadawczeThe data set consists tensile strength, electric resistance, electrochemical characteristics and physicochemical studies of multi-material 3D printed systems, including their sensing performance during detection of antibiotics in an industrial sewage. Additionally, contact angle measurements and SEM micrographs of the electrode surfaces were included.
-
Change of exhaust gases concentration for reference SOFC and SOFC with LSCNT layer fueled by biogas mixture at 750 C
Dane BadawczeThe dataset changes of exhaust gases concentrations (CH4,CO,CO2,H2) over working time for SOFC with La0.27Sr0.54Ce0.09Ni0.1Ti0.9O3-s layer as well as reference SOFEC (unmodified). Concentrations were calculated based on the FTIR measurements and calibration curves presented in different dataset. Longterm measurements of SOFC were performed using in-house...
-
Complex modulus of Cement Bitumen Treated Material Mixture (28 days of curing at 20C)
Dane BadawczeDataset presents data of complex modulus determined for cold recycled mixture – cement bitumen treated material mixture with 3 combinations of binding agents: 2% cement, 6% emulsion (C2E6), 6% cement, 6% emulsion (C6E6), 6% cement, 2% emulsion (C6E2). Mixture was designed according to Polish requirements for the base course of pavement. Mixture contains...