wszystkich: 847
wybranych: 66
Wyniki wyszukiwania dla: CORROSION%20INHIBITION
-
Dynamic impedance data for various carboxylic acids corrosion inhibition of aluminium in alkaline media (pH=11)
Dane BadawczeThis dataset contains the results of Dynamic Electrochemical Impedance Spectroscopy (DEIS) carried out in galvanostatic mode under iDC=0, carried out in order to define the corrosion inhibition effect of various studied carboxylic acids: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, carballylic acid, and serine. The experiment...
-
SEM micrographs of aluminium corrosion in alkaline media with various bee products as corrosion inhibitors
Dane BadawczeThis dataset contains various scanning electron microscopy (SEM) micrographs of AA5754 aluminum alloy samples exposed to the corrosive alkaline environment without and with the addition of various bee products to act as green corrosion inhibitors. The products are bee pollen, honey, and putty. They were investigated in bicarbonate buffer (pH =10 or...
-
The corrosion studies of 3,4,5-trihydroxybenzoic acid as an effective corrosion inhibitor of low alloy steel
Dane BadawczeThe dataset contains the electrochemical studies evaluating if gallic acid is a corrosion inhibitor for low alloy steel. Three measurements were carried out each case; corrosion potential (label ecorr), electrochemical impedance spectroscopy (label eis) and cyclic polarization (label cp). The measurements were carried out in sodium chloride, acidified...
-
SEM micrographs of Ti tooth implant corrosion
Dane BadawczeThe dataset contains micrographs made with a scanning electron microscope (SEM) Hitachi S-3400N of the tooth implant removed after inflammation. The inflammation was induced by the increased corrosion rate of the titanium screw. The reason for the corrosion to occur was the appearance of the concentration cell of different aeration for various areas...
-
Imaging of the effects of pitting corrosion with the use of AFM
Dane BadawczePitting corrosion is a local attack on a metal surface, limited to a point or small area, which appears as a hole. Pitting corrosion is one of the most harmful forms of corrosion due to the fact that it is associated with small, difficult to detect damage, that can even lead to perforation of the structure. A single pit may range in size from micrometers...
-
L-Homoserine O-acetyltransferase (CaMet2p) activity and inhibition
Dane BadawczeThe dataset contains the description of methodology and data files with the results obtained spectrophotometrically at 412 nm to determine the rate of fungal enzyme activity. The goal of the study was to obtain conditions optimal for L-homoserine O-acetyltransferase (Met2p) activity as well as evaluation of inhibitory potential of commercially available...
-
Cyclic polarization studies of Mg corrosion in alkaline environment
Dane BadawczeThe dataset contains the cyclic polarization studies of Mg (99.99%) in NaOH electrolyte at different pH values: 10, 11 and 12 aiming at understanding of Mg(OH)2 passive layer formation mechanism and conditions. The electrochemical studies were carried out in a three electrode setup, with Pt mesh as the counter electrode and Ag|AgCl as the reference...
-
SEM micrographs of the austenitic stainless steel corrosion in asphalt fumes
Dane BadawczeThe dataset contains the scanning electron microscopy (SEM) studies of the austenitic stainless steels: AISI 304, AISI 316, AISI 321 and duplex stainless steel AISI 2205. The samples were polished and exposed to the installation carrying asphalt fumes at elevated temperatures (approx. ~210-240 Celsius). The exposition duration was three months. Some...
-
The influence of microstructure on the corrosion resistance for some titanium-based alloys
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs revealing the microstructure of some Ti-based alloys, namely: Ti-6Al-4V (file name: TiV), Ti-6Al-7Nb (file name: TiNb) and TC21 (file name: TiAlSnZrMoCrNbSi) alloys and their localized corrosion as a result of passive layer breakdown in a corrosive environment, ie. 0.9% NaCl solution...
-
The AFM micrographs of pitting corrosion evolution on high-alloy steel 1.4301
Dane BadawczeThe dataset contains the results of topographic imaging of high-alloy stainless steel 1.4301 on which the pitting corrosion process was induced by electrochemical methods. The study of the effects of a local attack allows for conclusions about the intensity and mechanism of this type of corrosion. The file contains atomic force microscopy (AFM) data...
-
The AFM micrographs of austenitic stainless steel subjected to sensitization for intergranular corrosion
Dane BadawczeThe dataset contains atomic force microscopy (AFM) maps of topographic images of austenitic steel samples subjected to sensitization to the process of intergranular corrosion. Precipitations of carbides as well as other intermetallic phases can be observed and detected before the fragments of structures sensitized by improper thermal treatment are exposed...
-
Acoustic emission studies of the 7075 aluminium alloy pitting corrosion process
Dane BadawczeThe dataset contains the cyclic polarization studies and corresponding acoustic emission measurements, revealing the pitting corrosion process of the passive layer at the surface of the 7075 aluminum alloy in the borate buffer with different chloride ions concentrations, in the range between 0.05 and 25 mM.
-
Ellipsometric monitoring during the polarization studies of Mg corrosion in alkaline environment
Dane BadawczeThe dataset contains the ellipsometric results from the Mg polarization studies aiming at understanding the Mg(OH)2 passive layer formation mechanism and conditions. The single-wavelength ellipsometer ELX-02C from Dr Riss GmbH was utilized, operating He-Ne laser at 632.8 nm. The polarization conditions for the experiment are depicted in the related...
-
X-ray Photoelectron Spectroscopy studies of various carboxylic acids adsorption on aluminium alloys in alkaline media
Dane BadawczeThis dataset contains the results of high-resolution XPS studies obtained during evaluation of high corrosion inhibition efficiency of various carboxylic acids towards aluminium alloy 5754 in bicarbonate buffer pH=11.
-
The SEM micrographs of the cavitation erosion-corrosion process of selected copper alloys degradation
Dane BadawczeThe dataset contains Scanning Electron Micrographs of CuZn40Mn3Fe brass compared with Superston and Novoston bronze after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The micrographs compare the topography of samples subjected cavitation erosion in 3% NaCl at room temperature, leading to the surface...
-
SEM micrographs of cavitation erosion-corrosion of aluminium alloy 2024 with anodic polarization
Dane BadawczeThe dataset contains Scanning Electron Micrographs of aluminium alloy 2024 samples made after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The experiment duration was 240 min, with cyclic cavitation exposure in on/off cycles 30s:30s. The electrolyte was 0.1 M KNO3 solution. Some samples were anodically...
-
AFM visualization of Mg alloy surface modification
Dane BadawczeMagnesium alloys with additives improving their mechanical properties are valued as materials with low density and elasticity coefficient. Additionally, their biocompatibility and biodegradability make them interesting in prosthetic applications. However, the last of these features, valuable in medicine, contradicts the industrial needs for the described...
-
X-ray Photoelectron Spectroscopy studies of citric acid adsorption on aluminium alloy 5754 in alkaline media
Dane BadawczeThis dataset contains the results of high-resolution XPS obtained during evaluation of high corrosion inhibition efficiency of citric acid towards aluminium alloy 5754 in bicarbonate buffer pH=11. The exposition duration of samples to electrolytic environment was 100 min. Each sample was exposed at different citric acid concentration ranging from 0...
-
The SEM micrographs of the synergistic action between cavitation erosion and pitting corrosion on stainless steel 304
Dane BadawczeThe dataset contains Scanning Electron Micrographs of stainless steel AISI304 samples made after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The micrographs compare the topography of samples subjected to either cavitation erosion (in deionized water), pitting corrosion (in 8% FeCl3 solution, without...
-
Austenitic stainless steel sensitization
Dane BadawczeHigh-alloy steels, thanks to their composition and content of appropriate alloying additives, are characterized by increased resistance to many corrosive environments. However, this is due to the increased sensitivity of the described construction materials to specific environmental conditions during their use. An example may be the increased susceptibility...