Impedance spectroscopy of the lithium titanate doped by copper thin films
Dane BadawczeLithium titanate doped by copper thin films were derived by sol-gel method. Prepared gel was deposited by spin-coating technique. Samples with various content of Cu were measured by impedance spectroscopy method in a wide range of temperature, from -120 up to 150 deg.
-
Electrochemical Impedance Spectroscopy data of PDA-modified TiO2 nanotubes
Dane BadawczeThis dataset contains Electrochemical Impedance Spectroscopy data of the samples from TiO2 nanotubes modified with polydopamine. The studies were presented as a part of the research on "Band Gap Engineering toward Semimetallic Character of Quinone-Rich Polydopamine" (DOI: 10.1021/acs.jpcc.2c08804).
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Linear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
The electrochemical impedance spectroscopy studies of cataphoretic-grown epoxy-based coatings
Dane BadawczeThe dataset contains electrochemical impedance spectroscopy spectra collected for epoxy-based cataphoretic coatings in order to determine the offered anti-corrosion protection. Particular spectra pertain to the coatings applied for the different magnitude of polarization potential imposed, namely 10V, 20V and 30V. The results were obtained within the...
-
Linear impedance of 40Na2O-20CaO-40P2O5 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 40Na2O-20CaO-40P2O5 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched Bi2VO5.5 glass-ceramic was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of as-quenched Bi2VO5.5 glass-ceramic was measured by impedance spectroscopy method.
-
Linear impedance of 10Na2O–60P2O5–30CaO glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 10Na2O–60P2O5–30CaO glass was measured by impedance spectroscopy method.
-
Linear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of as-quenched 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Linear impedance of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 1SiO2–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 1SiO2–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 annealed glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 593 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 2.88 mm was measured at 693 K with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of frequency for Bi2VO5.5 ceramic of thickness 2.88 mm was measured at high temperature range with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched glass 40Bi2VO5.5-60SrB4O7 after full crystallization was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of as-quenched glass 40Bi2VO5.5-60SrB4O7 afetr full crystallization was measured by impedance spectroscopy method.
-
Nonlinear impedance of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 fully crystallized glass at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 partially crystallized glass at 613 K measured with impedance spectroscopy method at high temperature region