Acoustic emission studies of the 7075 aluminium alloy pitting corrosion process
Dane BadawczeThe dataset contains the cyclic polarization studies and corresponding acoustic emission measurements, revealing the pitting corrosion process of the passive layer at the surface of the 7075 aluminum alloy in the borate buffer with different chloride ions concentrations, in the range between 0.05 and 25 mM.
-
Tensile test of 1.4307 / X2CrNi18-9 / AISI 304L grade austenitic steel
Dane BadawczeShip structures and their components are build mainly of steel. Hull steel is used to build the hull structure. Some structural elements, such as RSW (Refrigerated See Water) tanks, or LNG (Liquid Natural Gas) tanks - gas transported at temperatures below -162° C, are build from austenitic steels. Austenitic steels have a different microstructure and...
-
Tensile test of 1.4541 / X6CrNi18-10 / AISI 321 grade austenitic steel
Dane BadawczeShip structures and their components are build mainly of steel. Hull steel is used to build the hull structure. Some structural elements, such as RSW (Refrigerated See Water) tanks, or LNG (Liquid Natural Gas) tanks - gas transported at temperatures below -162° C, are build from austenitic steels. Austenitic steels have a different microstructure and...
-
Tensile test of 1.4571 / X6CrNiMoTi17-12-2 / AISI 316Ti grade austenitic steel
Dane BadawczeShip structures and their components are build mainly of steel. Hull steel is used to build the hull structure. Some structural elements, such as RSW (Refrigerated See Water) tanks, or LNG (Liquid Natural Gas) tanks - gas transported at temperatures below -162° C, are build from austenitic steels. Austenitic steels have a different microstructure and...
-
Imaging of the effects of pitting corrosion with the use of AFM
Dane BadawczePitting corrosion is a local attack on a metal surface, limited to a point or small area, which appears as a hole. Pitting corrosion is one of the most harmful forms of corrosion due to the fact that it is associated with small, difficult to detect damage, that can even lead to perforation of the structure. A single pit may range in size from micrometers...
-
The corrosion studies of 3,4,5-trihydroxybenzoic acid as an effective corrosion inhibitor of low alloy steel
Dane BadawczeThe dataset contains the electrochemical studies evaluating if gallic acid is a corrosion inhibitor for low alloy steel. Three measurements were carried out each case; corrosion potential (label ecorr), electrochemical impedance spectroscopy (label eis) and cyclic polarization (label cp). The measurements were carried out in sodium chloride, acidified...
-
SEM micrographs of aluminium corrosion in alkaline media with various bee products as corrosion inhibitors
Dane BadawczeThis dataset contains various scanning electron microscopy (SEM) micrographs of AA5754 aluminum alloy samples exposed to the corrosive alkaline environment without and with the addition of various bee products to act as green corrosion inhibitors. The products are bee pollen, honey, and putty. They were investigated in bicarbonate buffer (pH =10 or...
-
SEM micrographs of the austenitic stainless steel corrosion in asphalt fumes
Dane BadawczeThe dataset contains the scanning electron microscopy (SEM) studies of the austenitic stainless steels: AISI 304, AISI 316, AISI 321 and duplex stainless steel AISI 2205. The samples were polished and exposed to the installation carrying asphalt fumes at elevated temperatures (approx. ~210-240 Celsius). The exposition duration was three months. Some...
-
SEM micrographs of Ti tooth implant corrosion
Dane BadawczeThe dataset contains micrographs made with a scanning electron microscope (SEM) Hitachi S-3400N of the tooth implant removed after inflammation. The inflammation was induced by the increased corrosion rate of the titanium screw. The reason for the corrosion to occur was the appearance of the concentration cell of different aeration for various areas...
-
The AFM micrographs of pitting corrosion evolution on high-alloy steel 1.4301
Dane BadawczeThe dataset contains the results of topographic imaging of high-alloy stainless steel 1.4301 on which the pitting corrosion process was induced by electrochemical methods. The study of the effects of a local attack allows for conclusions about the intensity and mechanism of this type of corrosion. The file contains atomic force microscopy (AFM) data...
-
The SEM micrographs of the synergistic action between cavitation erosion and pitting corrosion on stainless steel 304
Dane BadawczeThe dataset contains Scanning Electron Micrographs of stainless steel AISI304 samples made after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The micrographs compare the topography of samples subjected to either cavitation erosion (in deionized water), pitting corrosion (in 8% FeCl3 solution, without...
-
The SEM micrographs of the cavitation erosion-corrosion process of selected copper alloys degradation
Dane BadawczeThe dataset contains Scanning Electron Micrographs of CuZn40Mn3Fe brass compared with Superston and Novoston bronze after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The micrographs compare the topography of samples subjected cavitation erosion in 3% NaCl at room temperature, leading to the surface...
-
Dynamic impedance data for various carboxylic acids corrosion inhibition of aluminium in alkaline media (pH=11)
Dane BadawczeThis dataset contains the results of Dynamic Electrochemical Impedance Spectroscopy (DEIS) carried out in galvanostatic mode under iDC=0, carried out in order to define the corrosion inhibition effect of various studied carboxylic acids: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, carballylic acid, and serine. The experiment...
-
The influence of microstructure on the corrosion resistance for some titanium-based alloys
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs revealing the microstructure of some Ti-based alloys, namely: Ti-6Al-4V (file name: TiV), Ti-6Al-7Nb (file name: TiNb) and TC21 (file name: TiAlSnZrMoCrNbSi) alloys and their localized corrosion as a result of passive layer breakdown in a corrosive environment, ie. 0.9% NaCl solution...
-
The AFM micrographs of austenitic stainless steel subjected to sensitization for intergranular corrosion
Dane BadawczeThe dataset contains atomic force microscopy (AFM) maps of topographic images of austenitic steel samples subjected to sensitization to the process of intergranular corrosion. Precipitations of carbides as well as other intermetallic phases can be observed and detected before the fragments of structures sensitized by improper thermal treatment are exposed...
-
The microstructure of AA5754 alloy under corrosion in alkaline media (pH=11) with 20 mM of various carboxylic acids
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs taken for polished aluminum AA5754 alloy samples, exposed for 100 min in bicarbonate buffer (pH=11) with the addition of 20 mM of carboxylic acids, namely: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, tricarballylic acid and serine. The goal of this study was...
-
The microstructure of AA5754 alloy under corrosion in alkaline media (pH=11) with 4.5 mM of various carboxylic acids
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs taken for polished aluminum AA5754 alloy samples, exposed for 100 min in bicarbonate buffer (pH=11) with the addition of 4.5 mM of carboxylic acids, namely: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, tricarballylic acid and serine. The goal of this study was...
-
SEM micrographs of cavitation erosion-corrosion of aluminium alloy 2024 with anodic polarization
Dane BadawczeThe dataset contains Scanning Electron Micrographs of aluminium alloy 2024 samples made after cavitation erosion-corrosion exposure using a vibratory transducer (in accordance with ASTM G32). The experiment duration was 240 min, with cyclic cavitation exposure in on/off cycles 30s:30s. The electrolyte was 0.1 M KNO3 solution. Some samples were anodically...
-
Acoustic emission signals in concrete beams under 3-point bending (beams #1, #2, #3)
Dane BadawczeThe DataSet contains the results of the mechanical behaviour of concrete beams with dimensions 40 x 40 x 160 cm3under the 3-point bending. The beams were made of concrete with the following ingredients: cement CEM I 42.5R (330 kg/m3), aggregate 0/2 mm (710 kg/m3), aggregate 2/8 mm (664 kg/m3), aggregate 8/16 mm (500 kg/m3), water (165 kg/m3) and super-plasticizer...
-
Acoustic emission signals in concrete beams under 3-point bending (polyolefin and steel fibre concrete)
Dane BadawczeThe DataSet contains the results of the mechanical behaviour of concrete beams with dimensions 40 x 40 x 160 cm3 under the 3-point bending. All specimens were manufactured based on the same concrete mixture composed of cement CEM I 42.5R (380 kg/m3), water (165 kg/m3), aggregate 0/2 mm (648 kg/m3), aggregate 2/8 mm (426 kg/m3), aggregate 8/16 mm (754...
-
The effect of cobalt addition on the corrosion behavior of near equiatomic NiTi shape memory alloy in normal saline solution, impedance and microscopic studies
Dane BadawczeThe electrochemical and corrosion (uniform and localized) behavior of a binary Ni52Ti48 shape memory alloy (SMA) and two ternary Ni52Ti48-xCox (x = 1.5 and 4.0 wt.%) SMAs were studied. Measurements were conducted in 0.9% NaCl solution at 37 oC. This dataset contains the results of electrochemical impedance spectroscopy (EIS) studies done on daily basis...
-
Acoustic emission signals in concrete beams under 3-point bending (plain concrete, steel fibre reinforced concrete, steel bar reinforced concrete)
Dane BadawczeThe DataSet contains the results of the mechanical behaviour of concrete beams with dimensions 40 x 40 x 160 cm3under the 3-point bending. Two concrete mixes, both based on the same design, were produced in the test programme. Mixture #1 was the plain concrete (PC), consisting of cement CEM I 42.5R (380 kg/m3), water (165 kg/m3), aggregate 0/2 mm (648...
-
Cyclic polarization studies of Mg corrosion in alkaline environment
Dane BadawczeThe dataset contains the cyclic polarization studies of Mg (99.99%) in NaOH electrolyte at different pH values: 10, 11 and 12 aiming at understanding of Mg(OH)2 passive layer formation mechanism and conditions. The electrochemical studies were carried out in a three electrode setup, with Pt mesh as the counter electrode and Ag|AgCl as the reference...
-
Ellipsometric monitoring during the polarization studies of Mg corrosion in alkaline environment
Dane BadawczeThe dataset contains the ellipsometric results from the Mg polarization studies aiming at understanding the Mg(OH)2 passive layer formation mechanism and conditions. The single-wavelength ellipsometer ELX-02C from Dr Riss GmbH was utilized, operating He-Ne laser at 632.8 nm. The polarization conditions for the experiment are depicted in the related...
-
Austenitic stainless steel sensitization
Dane BadawczeHigh-alloy steels, thanks to their composition and content of appropriate alloying additives, are characterized by increased resistance to many corrosive environments. However, this is due to the increased sensitivity of the described construction materials to specific environmental conditions during their use. An example may be the increased susceptibility...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of water cooled materia
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of reference material materia (transverse direction)
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of reference material materia (longitudinal direction)
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - microstructure of naturally colled material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - microstructure of water cooled material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - microstructure of reference material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
Straightening of ship hull structure made of 316L stainless steel - tensile test of naturally cooled material
Dane BadawczeThe AISI 316L type steel belongs to the group of chromium-nickel stainless steels. They are determined according to European standards as X2CrNiMo17-12-2 and belong to the group of austenitic stainless steels. Steels of this group are used for elements working in seawater environments, for installations in the chemical, paper, and food, industries,...
-
AFM analysis of duplex steel structure and composition
Dane BadawczeDue to the high content of alloying elements, duplex stainless steels are characterized by a complex structure of phase transitions. Among all types of intermetallic compounds, the sigma phase is of major interest due to its detrimental effect on both mechanical properties and corrosion behavior. It is an intermetallic phase enriched in Cr and Mo and...
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in ambient temperature
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in 0°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in -20°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture documentation (test in +20°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture documentation (test in 0°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture documentation (test in -20°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding –SEM fracture investigation (Charpy test in -60°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding –SEM fracture investigation (Charpy test in +20°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding –SEM fracture investigation (Charpy test in -40°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding –SEM fracture investigation (Charpy test in -50°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in +20°C, specimens diameter 10 mm
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in +20°C, specimens diameter 14 mm
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in +20°C, specimens diameter 20 mm
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding –SEM fracture investigation (Charpy test in 0°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding –SEM fracture investigation (Charpy test in -20°C)
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in +20°C, elastic modulus
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture toughness test in 0°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....