Filters
total: 6788
filtered: 366
-
Catalog
Chosen catalog filters
Search results for: SOLID OXIDE CELLS
-
TEM data of (Cr,Fe,Mn,Co,Ni)3O4 High-entropy spinel oxide thin films deposited on amorphous SiO2 substrate by spray pyrolysis techniqe
Open Research DataThis Dataset include presentation of summarized TEM investigation of (Mn,Co,Fe,Ni,Cr)3O4 high-entropy spinel oxide prepared in the form of a ~ 500 nm thin film utilising a facile spray pyrolysis technique. The structural and electrical properties of the layers were characterised after exposure to temperatures in the range of 400–900 ◦C. The as-deposited...
-
SEM/EDX data of (Cr,Fe,Mn,Co,Ni)3O4 High-entropy spinel oxide thin films deposited on amorphous SiO2 substrate by spray pyrolysis techniqe
Open Research DataThis Data set include SEM and EDX results of (Mn,Co,Fe,Ni,Cr)3O4 high-entropy spinel oxide prepared in the form of a ~ 500 nm thin film utilising a facile spray pyrolysis technique. The structural and electrical properties of the layers were characterised after exposure to temperatures in the range of 400–900 ◦C. The as-deposited layers were amorphous,...
-
The electrical properties mesurements of SOFC with Ce0.9Cu0.1O2-s functional layer
Open Research DataThe dataset includes the electrical properties mesurements of SOFC with Ce0.9Cu0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of SOFC with Ce0.9Co0.1O2-s functional layer
Open Research DataThe dataset includes the electrical properties mesurements of SOFC with Ce0.9Co0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of SOFC with Ce0.8Co0.1Cu0.1O2-s functional layer
Open Research DataThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Co0.1Cu0.1O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
The electrical properties mesurements of SOFC with Ce0.8Co0.15Cu0.05O2-s functional layer
Open Research DataThe dataset includes the electrical properties mesurements of SOFC with Ce0.8Co0.15Cu0.05O2-s layer. Samples were produced using aqueous soft chemistry methods (microemulsion method) and applied in form of a layer onto the anode of the commercial SOFC. The SOFC was working under biogas feeding at 750oC. The layers were sintered at 1100oC.
-
Total electrical conductivity data of (Cr,Fe,Mn,Co,Ni)3O4 High-entropy spinel oxide thin films deposited on amorphous SiO2 substrate by spray pyrolysis techniqe
Open Research DataThis dataset includes electrical conductivity measurements results measured by van der pauw technique up to 900oC.
-
The AFM micrographs of vanadium oxides thin films obtained at 800°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on a silicon substrate and vanadium thin films were obtained by annealing as-prepared films at...
-
The AFM micrographs of vanadium oxides thin films obtained at 1200°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 400°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 600°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of of vanadium oxides thin films obtained at 300°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 150°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
XRD patterns of V2O5 thin film morphology dependent on substrate types
Open Research DataThe DataSet contains the XRD patterns of the V2O5 thin film structure dependent on substrate types. The as-prepared thin films were deposited on alumina, zirconium, zirconium oxide and metallic vanadium substrate, then was annealing under an oxidizing atmosphere at 600C for 10h.
-
The AFM micrographs of vanadium oxides thin films obtained at 200°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films deposited on quartz glass - the influence of the thickness of the thin film on its morphology
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a quartz glass substrate and were...
-
The AFM micrographs of vanadium oxides thin films obtained at 450°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films deposited on silicon - the influence of the thickness of the film on morphology
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a silicon substrate and were annealing...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 200 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 100 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 300 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
XRD and electrochemical results for MoO3 films deposited using pulsed laser deposition system
Open Research DataThe attached data contains XRD and electrochemical results for MoO3 films deposited on fluorine-doped tin oxide glasses. Films were deposited using a pulsed laser deposition system at different conditions. Part of the samples was deposited at room temperature and then annealed at 575°C for given times (samples labeled PLD_RT_575C_xmin, where x stands...
-
The scanning spreading resistance microscopy (SSRM) of some CoCrMo alloys subjected to electrochemical litography
Open Research DataThe dataset contains the results of the experiment consisting of performing electrochemical lithography on the surface of the CoCrMo prosthetic alloy. First, by applying local anodic polarization, oxide structures were created on the surface of the material. Next, they were imaged in the SSRM (scanning spreading resistance microscopy) mode to visualize...
-
SEM micrographs of V2O5 thin film morphology dependent on substrate types
Open Research DataThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin film morphology dependent on substrate types. The as-prepared thin films were deposited on alumina, zirconium, zirconium oxide and metallic vanadium substrate, then was annealing under an oxidizing atmosphere at 600C for 10h. The results show that the morphology of...
-
Evaluation of antimicrobial properties of thermomelt adhesives modified with zinc compounds
Open Research DataThe dataset contains the results of microbiological tests of thermomelt adhesives modified with zinc compounds, whose activity was assessed for their ability to reduce the number of Escherichia coli and Staphylococcus aureus strain, representing the Gram (-) and Gram (+) bacteria, respectively. The evaluation of antimicrobial properties of samples were...
-
Luminescence properties of TeOx thin films annealing under an oxidizing atmosphere
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. The sol was obtained by vigorously stirring precursor solution at 50°C for 2h, then the temperature was raised...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 140 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 160 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 180 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 200 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-0optic sensor - 250 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 210 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 300 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 270 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 190 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 260 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 290 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 170 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 280 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 150 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 230 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 240 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Luminescence properties of TeOx-Eu thin films
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-Eu thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of europium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Tb thin films
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-Tb thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of terbium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Structural investigations of the LTO:Cu thin films
Open Research DataLithium titanate (Li1+xTi2-xO4) doped with Cu2+ ions was synthesized by sol-gel processing method. The structure was characterized by X-ray Diffraction (XRD). All samples revealed presence of LTO spinel phase. X-ray pattern of undoped LTO was free of any impurities and other crystal phases. Similarly, samples with low amount of copper dopant (x = 0.05...
-
Luminescence properties of TeOx-Dy thin films
Open Research DataThe DataSet contains the emission and excitation spectra of TeOx-Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of dysprosium ions were added, the nitrates were used as a source of rare-earth ions....
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.2
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.1
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...