The scanning electron microscopy (SEM) studies of low voltage copper cables
Open Research DataThe dataset contains the scanning electron microscopy (SEM) images of the low voltage copper cables, which were studied in the article discussing the regulatory requirements for checking the electrical resistance of such cables. The cables were cut and studies in cross-section. The full results were published in:
-
SEM micrographs of the austenitic stainless steel corrosion in asphalt fumes
Open Research DataThe dataset contains the scanning electron microscopy (SEM) studies of the austenitic stainless steels: AISI 304, AISI 316, AISI 321 and duplex stainless steel AISI 2205. The samples were polished and exposed to the installation carrying asphalt fumes at elevated temperatures (approx. ~210-240 Celsius). The exposition duration was three months. Some...
-
Destruction of AFM probes during normal operation
Open Research DataThe quality of the images obtained with the use of an atomic force microscope is determined by the state of the blade interacting with the tested material. Image artifacts can be generated by various reasons, such as oxidation, contamination or an error in blade fabrication, but also appear as a result of the repeated scanning process and inevitable...
-
SEM micrographs of diamond-phase (sp3-C) rich boron-doped carbon nanowalls (sp2-C)
Open Research DataThis dataset contains the Scanning Electron Microscopy (SEM) micrographs taken for rich boron-doped carbon nanowalls structures, with different boron addition during the synthesis process and different CVD synthesis duration. The [B]/[C] ratios in the plasma were set to 0k, 1.2k, 2k and 5k ppm. The time of growth was ranging between 4 and 9 hours. This...
-
Experimental dataset on detection of SARS-CoV-2 specific IgG antibodies by the fiber optic microsphere-based sensor
Open Research DataThe presented dataset is related to experimental detection of the ARS-CoV-2 specific IgG antibodies by the fibre optic microsphere-based sensor. To perform measurement we used a dedicated microsphere-based probe whose surface was immobilized.
-
TiN coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #B48/#A45
Open Research DataWear tests in sliding friction of TiN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiN over TiN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 12 min....
-
TiC coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #B41/#A39
Open Research DataWear tests in sliding friction of TiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiC over TiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 9 min....
-
CrN coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #A23/#B22
Open Research DataWear tests in sliding friction of CrN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, CrN over CrN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 12 min. The...
-
TiC coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #B39/#A41
Open Research DataWear tests in sliding friction of TiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiC over TiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 3 min. The test...
-
SiC coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #B34/#A33
Open Research DataWear tests in sliding friction of SiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, SiC over SiC. Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 3 min. The test...
-
TiN coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #A45/#B48
Open Research DataWear tests in sliding friction of TiN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiN over TiN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 12 min....
-
TiC coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #A41/#B39
Open Research DataWear tests in sliding friction of TiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiC over TiC . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 3 min. The...
-
CrN coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #A25/#B21
Open Research DataWear tests in sliding friction of CrN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, CrN over CrN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 9 min....
-
CrN coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #B22/#A23
Open Research DataWear tests in sliding friction of CrN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, CrN over CrN. Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 6 min. The test...
-
SiC coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #A33/#B34
Open Research DataWear tests in sliding friction of SiC coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, SiC over SiC. Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 3 min. The test...
-
The influence of microstructure on the corrosion resistance for some titanium-based alloys
Open Research DataThis dataset contains scanning electron microscopy (SEM) micrographs revealing the microstructure of some Ti-based alloys, namely: Ti-6Al-4V (file name: TiV), Ti-6Al-7Nb (file name: TiNb) and TC21 (file name: TiAlSnZrMoCrNbSi) alloys and their localized corrosion as a result of passive layer breakdown in a corrosive environment, ie. 0.9% NaCl solution...
-
A synthetic result of the development of personnel risk factors in the A, B, C, D enterprise
Open Research DataThe data below presents the shape of all the researched personnel risk factors in the A, B, C, D enterprise (which were tested by the author). Further considerations should be started with the presentation of the synthesis of the obtained results, which is presented in this research data.
-
AFM images of the platinum (111) single crystal surface as delivered, without the polishing treatment
Open Research DataPlatinum (111) single crystal surface images as delivered, without polishing treatment. Topographic measurements in contact mode. NTEGRA Prima (NT-MDT) device. CSG probe 10.
-
Results of calibration of the piezoelectric scanner using the probe TGQ1
Open Research DataTeaching file. Results of calibration of the piezoelectric scanner using the probe TGQ1. Scanning in contact mode. NTEGRA Prima (NT-MDT) device. CSG probe 10.
-
CrN coating in ring-on-ring sliding with saline solution (0.9%) lubrication 5MPa, 0.1m/s specimn. #B21/#A21
Open Research DataWear tests in sliding friction of CrN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, CrN over CrN . Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: SALINE SOLUTION (0.9%). Tribometer: PT-3. Overall test time till coating penetration 25 min....
-
TiN coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #A45/#A47
Open Research DataWear tests in sliding friction of TiN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiN over TiN. Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 20 min. The test...
-
TiN coating in ring-on-ring sliding with distlled water lubrication 5MPa, 0.1m/s specimn. #A45/#B45
Open Research DataWear tests in sliding friction of TiN coating on 1.4021 (EN 10088-1) heat treated stainless steel. Ring - on - ring contact in unidirectional sliding, TiN over TiN. Mean contact stress: 5MPa. Sliding velocity: 0,1 m/s. Mean friction radius: 9.5mm. Lubricant: DISTILLED WATER. Tribometer: PT-3. Overall test time till coating penetration 90 min. The test...
-
Measurements of raising of 160EC pantograph type
Open Research DataIn this description the results of the experiment and also simulation performed on the total assembly of the 160 EC pantograph type is given. Multibody dynamics of pantograph rising due to external torque and forces are measured for parameter validation of the pantograph model.
-
Distance measurement by the low coherent interferometer
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1560 nm, an optical spectrum analyzer and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Dynamic impedance data for various carboxylic acids corrosion inhibition of aluminium in alkaline media (pH=11)
Open Research DataThis dataset contains the results of Dynamic Electrochemical Impedance Spectroscopy (DEIS) carried out in galvanostatic mode under iDC=0, carried out in order to define the corrosion inhibition effect of various studied carboxylic acids: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, carballylic acid, and serine. The experiment...
-
AFM and SSRM investiagtion of carbon nanowalls properties
Open Research DataStructures with limited dimensionality are of great interest in modern nanotechnology. The properties of these objects are used, among others, for the construction of modern displays or as a base for quantum computers. Carbon nanowalls, which are the subject of the imaging results contained in this collection, are also considered interesting building...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 0 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 40 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 30 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 200 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 20 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 80 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 170 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 20 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 140 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 130 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 50 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 120 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 110 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 130 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 90 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Investigation of plasmon resonance in a silver nanoparticles
Open Research DataSilver nanostructures were prepared on borosilicate glass (Corning 1737F) substrates. Thin Ag films (1–9 nm thickness) were deposited using a table-top dc magnetron sputtering coater (EM SCD 500, Leica) in pure Ar plasma (argon, Air Products 99.999%). The Ag target was of 99.99% purity, the rate of layer deposition was about 0.4 nm·s−1, and the incident...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 120 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 200 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 170 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 90 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 180 um (serie 1)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 140 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 60 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 190 um (serie 2)
Open Research DataThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...