The structure of lead-silicate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe structure of iron-doped glasses and glass-ceramics were studied. Samples has the composition of 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All samples were prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass plate preheated to 573...
-
The morphology of lead-silicate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass plate preheated to 573...
-
The morphology of lead-borate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped borate glasses and glass-ceramics were studied. Samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 < x < 37 in mol%) were prepared by the conventional meltquenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate...
-
Magnetic properties of of lead-silicate glasses and nanocomposites doped with iron oxide
Dane BadawczeMagnetic properties of iron-doped glasses and glass-ceramics were studied. Two different sets of glass samples were prepared. The first group of samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO– xFe2O3, where x = 15 and 20 (in mol%). Composition of the second group was 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All sampleswere...
-
Electrical properties of nanostructures in lead-silicate glasses and nanocomposites doped with iron oxide
Dane BadawczeElectrical properties of iron oxide nanostructures observed in silicate glasses and glass-ceramics were studied. Two different sets of glass samples were prepared. The first group of samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO– xFe2O3, where x = 15, 20 and 25 (in mol%). Composition of the second group was 50SiO2–(50−x)PbO–xFe2O3, where...
-
The structure of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with X-ray diffraction method
Dane BadawczeThe structure of strontium–borate glasses and glass-ceramics containing Bi2VO5.5 nanocrystallites was measured by XRD.
-
The topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with SEM method
Dane BadawczeThe topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. was measured by SEM.
-
The morphology of lead-silicate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
The structure of lead-silicate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe structure of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All samples were prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
The structure of lead-borate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe structure of iron-doped glasses and glass-ceramics were studied. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate and...