Filters
total: 2801
filtered: 526
Search results for: ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY
-
Electrochemical Impedance Spectroscopy data of PDA-modified TiO2 nanotubes
Open Research DataThis dataset contains Electrochemical Impedance Spectroscopy data of the samples from TiO2 nanotubes modified with polydopamine. The studies were presented as a part of the research on "Band Gap Engineering toward Semimetallic Character of Quinone-Rich Polydopamine" (DOI: 10.1021/acs.jpcc.2c08804).
-
The electrochemical impedance spectroscopy studies of cataphoretic-grown epoxy-based coatings
Open Research DataThe dataset contains electrochemical impedance spectroscopy spectra collected for epoxy-based cataphoretic coatings in order to determine the offered anti-corrosion protection. Particular spectra pertain to the coatings applied for the different magnitude of polarization potential imposed, namely 10V, 20V and 30V. The results were obtained within the...
-
Model dynamic electrochemical impedance spectroscopy (DEIS) results obtained with various DC polarization rates
Open Research DataThe dataset contains results of model dynamic electrochemical impedance spectroscopy studies carried out on a setup of 10 diodes in series, which were connected in parallel with a condenser. The impedance data were acquired every 1 s (the analytic window length for Fourier Transform was 1 s). The model system was polarized between 0 and +8 V with DEIS...
-
Electrochemical impedance spectroscopy measurements - conductivity vs. temperature and conductivity vs. oxygen partial pressure - BaCe0.6Zr0.2Y0.1Tb0.1O3-δ
Open Research DataThe dataset consists of two main catalogs consisting of measurement data: of the electrical conductivity of the BaCe0.6Zr0.2Y0.1Tb0.1O3-δ (BCZYTb) sample as a function of temperature and of the electrical conductivity as a function of oxygen partial pressure (pO2). Measurements as a function of temperature were carried out in dry and wet air (pH2O ~...
-
Influence of sintering temperature of porous SrTi0.30Fe0.70O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Influence of sintering temperature of porous SrTi0.50Fe0.50O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Influence of sintering temperature of porous SrTi0.65Fe0.35O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for SrxTi0.30Fe0.70O3-d cathode sintered at 900 °C measured at 700 °C
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with SrxTi0.30Fe0.70O3-d (x=0.90, 0.95, 1.00 and 1.05) cathodes sintered at 900 °C. EIS spectra were measured at 700 °C and 20% of oxygen partial pressure. Results converted to electrode surfaces area and dived by...
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for SrxTi0.30Fe0.70O3-d cathode sintered at 800 °C measured at 700 °C
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with SrxTi0.30Fe0.70O3-d (x=0.90, 0.95, 1.00 and 1.05) cathodes sintered at 800 °C. EIS spectra were measured at 700 °C and 20% of oxygen partial pressure. Results converted to electrode surfaces area and dived by...
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.50Fe0.50O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.65Fe0.35O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 800 °C, 750 °C and 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrode sintered at 800 °C
Open Research DataThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C; 750°C and 700 °C (synthetic air). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 800 °C and 15% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 800 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 100% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 100% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 15% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 20% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 20% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included....
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 700 °C and 5% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 700 °C and 5% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included. Results...
-
Electrochemical impedance spectroscopy and Distribution of Relaxation Times analysis results for porous SrTi0.30Fe0.70O3-d oxygen electrode measured at 600 °C and 15% oxygen partial pressure
Open Research DataThis dataset contains electrochemical impedance spectroscopy and Distribution of Relaxation Times results for symmetrical cell with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at 800 °C. EIS spectra were measured at 600 °C and 15% of oxygen partial pressure. Spectra of two RCPE elements from equivalent circuit , are also included. Results converted...
-
Electrochemical cell impedance spectra at Eoc
Open Research DataThe dataset presents impedance spectrum of electrochemical cell filled with 3% NaCl solution presented in the figure below. This cell was used measured using Atlas-Sollich 0531 impedance analyser with built-in potentiostat. When changing the DC polarisation of the cell the non-linear phenomena could be observed. The impedance spectrum frequency range...
-
Electrochemical cell impedance spectra at Eoc+100mV
Open Research DataThe dataset presents impedance spectrum of electrochemical cell filled with 3% NaCl solution presented in the figure below. This cell was used measured using Atlas-Sollich 0531 impedance analyser with built-in potentiostat. When changing the DC polarisation of the cell the non-linear phenomena could be observed. The impedance spectrum frequency range...
-
Electrochemical cell impedance spectra at Eoc+200mV
Open Research DataThe dataset presents impedance spectrum of electrochemical cell filled with 3% NaCl solution presented in the figure below. This cell was used measured using Atlas-Sollich 0531 impedance analyser with built-in potentiostat. When changing the DC polarisation of the cell the non-linear phenomena could be observed. The impedance spectrum frequency range...
-
Electrochemical cell impedance spectra at Eoc-100mV
Open Research DataThe dataset presents impedance spectrum of electrochemical cell filled with 3% NaCl solution presented in the figure below. This cell was used measured using Atlas-Sollich 0531 impedance analyser with built-in potentiostat. When changing the DC polarisation of the cell the non-linear phenomena could be observed. The impedance spectrum frequency range...
-
Electrochemical cell impedance spectra at Eoc-200mV
Open Research DataThe dataset presents impedance spectrum of electrochemical cell filled with 3% NaCl solution presented in the figure below. This cell was used measured using Atlas-Sollich 0531 impedance analyser with built-in potentiostat. When changing the DC polarisation of the cell the non-linear phenomena could be observed. The impedance spectrum frequency range...
-
Electrochemical impedance spectra and CV curves of V2O5 nanocrystals
Open Research DataThe DataSet contains the EIS spectra for coin-cells and CV curves with the V2O5 nanocrystals obtained by the sol-gel method. Cyclic voltammetry and electrochemical impedance spectroscopy (EIS) were measured using the AUTOLAB 302N potentiostat-galvanostat under Nova software. The EIS measurements were recorded in the frequency range 100 kHz to 10 mHz...
-
Electrochemical impedance spectra and CV curves of V2O5 nanorods
Open Research DataThe DataSet contains the EIS spectra for coin-cells and CV curves with the V2O5 nanorods obtained by the sol-gel method. Cyclic voltammetry and electrochemical impedance spectroscopy (EIS) were measured using the AUTOLAB 302N potentiostat-galvanostat under Nova software. The EIS measurements were recorded in the frequency range 100 kHz to 10 mHz for...
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Linear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
Impedance spectroscopy of the lithium titanate doped by copper thin films
Open Research DataLithium titanate doped by copper thin films were derived by sol-gel method. Prepared gel was deposited by spin-coating technique. Samples with various content of Cu were measured by impedance spectroscopy method in a wide range of temperature, from -120 up to 150 deg.
-
Linear impedance of 40Na2O-20CaO-40P2O5 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 40Na2O-20CaO-40P2O5 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched Bi2VO5.5 glass-ceramic was measured with impedance spectroscopy method at low temperature region
Open Research DataThe nonlinear electrical properties of as-quenched Bi2VO5.5 glass-ceramic was measured by impedance spectroscopy method.
-
Linear impedance of 10Na2O–60P2O5–30CaO glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 10Na2O–60P2O5–30CaO glass was measured by impedance spectroscopy method.
-
Linear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of as-quenched 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Open Research DataThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.