Search results for: laser treatment nanoindentation
-
Nanoindentation tests titanium alloy Ti-6Al-4V after interference laser treatment
PublicationThe study aimed was to assess selected mechanical properties of surface layers obtained after interference laser treatment – DLIL of titanium alloy Ti-6Al-4V used for implants. The samples were melted in still air at room temperature, for this purpose Nd:YAG laser was used, the number of laser shots was variable. Next, nanoindentation tests were performed, based on which Young’s modulus and nanohardness in the obtained surface...
-
Mechanical Properties and Wear Susceptibility Determined by Nanoindentation Technique of Ti13Nb13Zr Titanium Alloy after “Direct Laser Writing”
PublicationLaser treatment has often been applied to rebuild the surface layer of titanium and its alloys destined for long-term implants. Such treatment has always been associated with forming melted and re-solidified thin surface layers. The process parameters of such laser treatment can be different, including the patterning of a surface by so-called direct writing. In this research, pulse laser treatment was performed on the Ti13Nb13Zr...
-
Cavitation behavior of the SUPERSTON alloy after laser treatment
PublicationResults of laser treatment at cryogenic conditions and its influence on microstructure, microhardness and cavitation resistance of the SUPERSTON alloy are presented in this paper. Obtained results point at possibility of the increase hardness and cavitation resistance of the parts worked in cavitation conditions.
-
New laser-enhanced surface treatment of Ti bioalloy
PublicationPrzedstawiono wyniki badan mikrostruktury i korozji w roztworze Ringera stopu Ti6Al4V, który był poddawany nadtapianiu laserem CO2 w powietrzu, wodzie i ciekłym azocie. Stwierdzono znaczący wpływ warunków obróbki na mikrostrukturę, mikrotwardość i głębokość zmodyfikowanej warstwy wierzchniej.
-
Laser surface treatment of aluminium alloys at cryogenic conditions.
PublicationPrzedstawiono nową metodę obróbki laserowej powierzchni stopów aluminium w warunkach kriogenicznych. W wyniku tej obróbki w warstwie wierzchniej stopów przeznaczonych na tłoki silników spalinowych uzyskano znaczące podwyższenie twardości, odporności na zużycie ścierne oraz wzrost właściwości korozyjnych.
-
Surface treatment of C80U steel by long CO2 laser pulses
PublicationThe paper presents the results of laser-melted C80U steel. The processed steel was placed between two permanent magnets and laser beam whose scanning velocity was 10 mm/s. CO2 laser beam was working in pulse mode. Pulses were generated at 100% of the average preset power of 700W, with 45 ms irradiation, zero interval between pulses and beginning of pulse repetition upon the achievement of the average laser power. During the operation,...
-
Laser surface treatment of aluminium-silicon alloy at cryogenic conditions
PublicationW artykule przedstawiono wpływ laserowego, powierzchniowego przetapiania w warunkach kriogenicznych na mikrostrukturę, mikrotwardość, zużycie na skutek tarcia oraz korozję stopu aluminium AlSi13Mg1CuNi. Stwierdzono zwiększenie mikrotwardości, odporności na ścieranie i korozję odlewniczego stopu AlSi13Mg1CuNi stosowanego w produkcji tłoków silników spalinowych.
-
Microstructural aspects of corrosion of the SUPERSTON alloy after laser treatment
PublicationW artykule przedstawiono rezultaty obróbki laserowej stopu SUPERSTON w warunkach kriogenicznych i jej wpływ na mikrostrukturę i odporność korozyjną. Badania korozyjne zostały zrealizowane metodą potencjostatyczną w 3% NaCl, odporność korozyjna stopu zmieniała się wraz ze zmianą parametrów nadtapiania laserowego.
-
Aluminium surface treatment with ceramic phases using diode laser
Publication -
Cavitation wearing of the SUPERSTON alloy after laser treatment at cryogenic conditions
PublicationThe purpose of this paper is to demonstrate the method of laser remelting at cryogenic conditions of the SUPERSTON alloy and its influence on microstructure and cavitation wearing. The cavitation test was performed using the rotating disc facility in IPM PAN Gdansk. During the cavitation test, the mass loss of the material with different parameters of laser remelting was determined. Surface and cross-section microstructure of the...
-
Effects of the preheating laser treatment on microstructure and corrosion resistance of Ti6Al4V bioalloy
PublicationThe laser remelting of the Ti6Al4V alloy was made on specimens pre-heated at elevated temperatures. The laser treatment effected in change of microstructures of surface layers and an appearance of blisters and numerous cracks. The corrosion tests demonstrated the decrease in corrosion resistance for each preheating temperature. The observed effects were attributed to negative influence of excessive compressive stresses with no...
-
Effect of laser treatment on the wear and corrosion resistance of aluminiumalloy used for pistons
PublicationPrzedstawiono wpływ powierzchniowego laserowego przetapiania w warunkach kriogenicznych na skład chemiczny, mikrostrukturę, mikrotwardość oraz zużycie ścierne i odporność korozyjną stopu AlSi13Mg1CuNi stosowanego na tłoki silników spalinowych. Uzyskano zwiększenie odporności na ścieranie i korozję stopu AlSi13Mg1CuNi.
-
Laser Surface Treatment of Sintered Stainless Steels for Wear Resistance Enhancement
Publication -
Influence of Surface Laser Treatment on Mechanical Properties and Residual Stresses of Titanium and its Alloys
PublicationSurface modification of the titanium and its alloys used in implantology with a long-pulse laser can change the surface topography, but it also leads to changes in the stress sign and magnitude in the resulting subsurface layer. The presented research was aimed at evaluating the state of stress after laser remelting with the Nd:YAG laser of pre-etched titanium alloys Ti6Al4V and Ti13Nb13Zr and pure titanium. The obtained surface...
-
Effect of Laser Treatment on Intrinsic Mechanical Stresses in Titanium and Some of Its Alloys
PublicationLaser surface treatment conducted at different power levels is an option to modify titanium bone implants to produce nano- and microtopography. However, such processing can lead to excess mechanical stress within the surface layer. This research aims to calculate the level of such residual stresses after the surface processing of Ti grade IV, Ti15Mo, and Ti6Al7Nb alloys with an Nd:YAG laser. Light and scanning electron microscopies...
-
Corrosion characteristics of the AL-Si alloy after laser treatment at cryogenic conditions
PublicationOmówiono wpływ laserowego powierzchniowego przetapiania stopu Al-Si w warunkach kriogenicznych na jego mikrostrukturę i właściwości użytkowe. W wyniku badań korozyjnych stwierdzono zwiększenie odporności na korozję stopu Al-Siw 0,01 M roztworze H2SO4.
-
Influence of Laser Treatment on Microstructure of Surface Layer of the Ti-6Al-4V Alloy
PublicationPrzedstawiono mikrostrukturę powierzchni, przekroju i przełomu warstwy wierzchniej stopu Ti-6Al-4V uzyskanej po nadtapianiu laserem w różnym środowisku. Stwierdzono wzrost mikrotwardości stopu w warstwie nadtopionej, rozdrobnienie ziarna, a także tworzenie azotków tytanu i mikropęknięć skutkiem obecności znacznych naprężeń własnych. Grubość wytworzonych warstw osiągała wartość 1,5 mm.
-
The possibility of an use of laser treatment to improve the behaviour of the Ti-6Al-4V alloy
PublicationPrezentowana praca miała na celu stworzenie warunków ultraszybkiego chłodzenia przetopionej warstwy w obecności azotu tak, aby otrzymać twardą i gruba warstwę wierzchnią na stopie Ti-6Al-4V , najczęściej używanm stopie Ti, zawierającą struktury martenzytu i azotku tytanu.
-
The impact of laser surface treatment on the microstructure, wear resistance and hardness of the AlMg5 aluminum alloy
Publication -
Effect of selective laser treatment on initiation of fatigue crack in the main part of an undercarriage drag strut
PublicationThis paper presents the results of material characterization and a fatigue test conducted for a laser-re-melted drag strut used in an aircraft landing gear. The drag strut was re-melted with a CO2 laser beam. Eight re-melted paths were made in the form of spiral lines along the axis of the drag strut. Next, the drag strut was subjected to variable loads on a testing machine simulating loads occurring when an aircraft lands. The...
-
Organic pollutants photodegradation increment with use of TiO2 nanotubes decorated with transition metals after pulsed laser treatment
PublicationAmong various titanium(IV) oxide (TiO2, titania) structures, 1D nanotubes (TiO2 NTs) produced during the two-electrode anodization process, are extensively utilized in sensors or supercapacitors as well as in photo(electro)catalytic water splitting. However, due to wide bandgap and fast electron-hole recombination additional modifications, mostly concerned on materials surface, are required. According to the recent research, TiO2...
-
Effect of pulse laser treatment at different process variables on mechanical behavior of carbon nanotubes electrophoretically deposited on titanium alloy
PublicationPurpose: Titanium and its alloys are widely used as biomaterials for long-term implants, but they are usually surface-modified due to their weak bioactivity and wear resistance. Laser processing was used to modify the surface layer, and elemental carbon was a component of the deposited coatings. This research aims to use a combination of both methods based on preliminary electrophoretic deposition of multi-wall carbon nanotubes...
-
Mechanical Properties and Residual Stress Measurements of Grade IV Titanium and Ti-6Al-4V and Ti-13Nb-13Zr Titanium Alloys after Laser Treatment
PublicationNowadays, surface engineering focuses on research into materials for medical applications. Titanium and its alloys are prominent, especially Ti-6Al-4V and Ti-13Nb-13Zr. Samples made of pure grade IV titanium and the titanium alloys Ti-6Al-4V and Ti-13Nb-13Zr were modified via laser treatment with laser beam frequency f = 25 Hz and laser beam power P = 1000 W during a laser pulse with duration t = 1 ms. Subsequently, to analyze...
-
The Influence of Laser Alloying of Ti13Nb13Zr on Surface Topography and Properties
PublicationThe laser alloying is a continually developing surface treatment because of its significant and specific structuration of a surface. In particular, it is applied for Ti alloys, being now the most essential biomaterials` group for load-bearing implants. The present research was performed on the Ti13Nb13Zr alloy subject to laser modification in order to determine the treatment effects on surface topography and its some mechanical...
-
Effect of plasma sprayed and laser re-melted Al2O3 coatings on hardness and wear properties of stainless steel
PublicationCommercially available austenic stainless steel substrate was coated with commercially available, raw Al2O3 powder applied by means of plasma spraying method and then re-melted with CO2 laser beam of various parameters. Tribological and mechanical properties of the 120 J/mm and 160 J/mm laser re-melted coatings were compared with the tribological and mechanical properties of the “as-sprayed” coating. The influence of the laser...
-
Microstructure and mechanical properties of laser surface-treated Ti13nb13zr alloy with MWCNTs coatings
PublicationLaser surface modification of titanium alloys is one of the main methods of improving the properties of titanium alloys used in implantology. This study investigates the microstructural morphology of a laser-modified surface layer on a Ti13Nb13Zr alloy with and without a carbon nanotube coating deposited by electrophoretic deposition. Laser modification was performed for samples with and without carbon nanotube coating for two...
-
Laser Beam as a Precision Tool to Increase Fatigue Resistance in an Eyelet of Undercarriage Drag Strut
PublicationThe article contains the results of tests on a laser-processed eyelet of undercarriage drag strut to increase its fatigue strength. Laser processing concentrated on both sides around the hole of eye for connecting the undercarriage drag strut caused that the material in this area withstood more than twice the number of load cycles established for this material. In order to determine the reasons for the increase in fatigue strength,...
-
Influence of Nitriding and Laser Remelting on Properties of Austenitic Stainless Steel Type X10CrNi18-8 and Cavitation Erosion Resistance
PublicationThe paper presents properties of surface layers. Surface layers were obtained by using low temperature glow–discharge nitriding process and laser remelting carried out on austenitic stainless steel type X10CrNi18-8. Investigations were done by using an Ultra Nanoindentation Tester (UNHT) in the Warsaw Institute of Fundamental Technological Research. The influence of the above mentioned...
-
Wytwarzanie i modyfikacja powierzchni porowatych struktur tytanowych przeznaczonych na implanty
PublicationCelem pracy było wytworzenie stopu Ti-13Nb-13Zr z wykorzystaniem technologii selektywnego topienia laserowego (SLM) oraz jego biofunkcjonalizacja za pomocą utleniania mikrołukowego (MAO), a następnie określenie wpływu parametrów procesowych na właściwości otrzymanych materiałów pod kątem ich zastosowania na implanty. Oceniono wpływ napięcia, natężenia i czasu procesu MAO przeprowadzanego w elektrolicie zawierającym wapń i fosfor...
-
Wpływ azotowania jarzeniowego i laserowego nadtapiania na odporność kawitacyjną stali X5CrNi18-10
PublicationNierdzewne stale austenityczne charakteryzują się doskonałą odpornością korozyjną, aczkolwiek niskimi właściwościami mechanicznymi. W wielu przypadkach ogranicza to ich eksploatację w warunkach przemysłowych. Ponadto, nierdzewne stale austenityczne są wrażliwe na korozję lokalną w obecności jonów halogenkowych. Technologie materiałowe, które dają potencjalne możliwości otrzymywania korzystnego wpływu na właściwości mechaniczne...
-
Mechanical and Corrosion Properties of Laser Surface-Treated Ti13Nb13Zr Alloy with MWCNTs Coatings
Publication: Titanium and its alloys is the main group of materials used in prosthetics and implantology. Despite their popularity and many advantages associated with their biocompatibility, these materials have a few significant disadvantages. These include low biologic activity—which reduces the growth of fibrous tissue and allows loosening of the prosthesis—the possibility of metallosis and related inflammation or other allergic reactions,...
-
Hydroxyapatite deposition on the laser modified Ti13Nb13Zr alloy
PublicationThe Ti13Nb13Zr alloy was subjected to laser modification with the Nd:YAG laser provided that such treatment would increase the surface roughness followed improved adhesion of hydroxyapatite (HAp) coatings The hydroxyapatite was deposited by electrophoretic method in suspension of 0.5 g HA powder and 100 ml ethyl alcohol. The deposition was carried out for 10 min at 10 V voltage followed by drying at room temperature for 24 h and...
-
THE POSSIBILITY OF USE OF LASER-MODIFIED Ti6Al4V ALLOY IN FRICTION PAIRS IN ENDOPROSTHESES
PublicationThe purpose of this paper is to show results of laser treatment at cryogenic conditions of the Ti6Al4V alloy used for orthopedic applications. That modification process ought to bring beneficial changes of microstructure and residual stresses in the surface layer. The paper presents the abrasive wear of the base and laser remelted material in association with ceramics Al2O3. Despite the surface cracking after laser treatment the...
-
Effects of CO2 and Nd:YAG Laser Remelting of the Ti6Al4V Alloy on the Surface Quality and Residual Stresses
PublicationThe titanium alloys are materials susceptible to tribological wear and the laser treatment can be applied in surface treatment processes to obtain for example higher hardness level. From the other side, it is important to take into consideration, that hardness increase that can be connected with cracks . The aim of this research was to investigate the effects of different lasers and the process parameters on the form and level...
-
Effects of Laser Remelting at Cryogenic Conditions on Microstructure and Wear Resistance of the Ti6Al4V Alloy Applied in Medicine
PublicationThe titanium and its alloys can be subjected to surface treatment, including laser treatment. In this work a new laser treatment at cryogenic conditions of Ti6Al4V alloy has been described. The work has been aimed at establishing whether such surface treatment could be suitable for implants working under wear in biological corrosive environment. The remelting has been made with the use of CO2 continuous work laser at laser power...
-
Selective Laser Melting of Ti Alloy for Manufacturing The Prosthetic Elements
PublicationThe selective laser melting (SLM) is the additive manufacturing method of custom-designed parts. The used materials and the applications are various, including medicine. The titanium and its alloys are materials for which the dimensional quality, surface smoothness and no or extremely low porosity are difficult to reach. In this paper, the successful attempt to obtain by SLM the individually designed prosthetic bridges is described....
-
Formation of the hollow nanopillar arrays through the laser-induced transformation of TiO2 nanotubes
PublicationIn the following article, we present a simple, two-step method of creating spaced, hollow nanopillars, from the titania nanotube arrays via pulsed laser-treatment. Due to the high ordering of the structure, the prepared material exhibits photonic properties, which has been shown to increase the overall photoefficiency. The optical and morphological changes in the titania nanotubes after pulsed laser-treatment with 532, 355, and...
-
A prototype femtosecond laser system for MEMS fabrication
Publicationn this article, the concept of a prototype femtosecond laser micromachining system and a femtosecond solid-state Yb:KYW laser is presented. Ultrashort laser pulses have many advantages over the long pulses in laser micromachining, due to their unique ability to interact with different materials without transferring heat to them. This allows very precise and pure laser-processing, clean cuts and sharp edges. A femtosecond laser...
-
Application of the nanoindentation method in assessing of properties of cement composites modified with silica-magnetite nanostructures
Publication -
Use of optical skin phantoms for preclinical evaluation of laser efficiency for skin lesion therapy
PublicationSkin lesions are commonly treated using laser heating. However, the introduction of new devices into clinical practice requires evaluation of their performance. This study presents the application of optical phantoms for assessment of a newly developed 975-nm pulsed diode laser system for dermatological purposes. Such phantoms closely mimic the absorption and scattering of real human skin (although not precisely in relation to...
-
Influence of laser melting on surface layer properties of titanium alloy Ti6Al4V
PublicationIn time of rapid technology and medicine progress, implants are becoming more widely used in the human body, ranging from dental implants, stabilizing plates, screws, orthopaedic prostheses. For example, there are many types of hip prostheses used for hip replacement as well as various types of materials used for these orthopaedic prostheses. Properties of titanium alloys used in hip prostheses combined with good strength properties,...
-
Influence of the laser remelting parameters on the thickness of surface layers created on the stainless steel X5CrNi18-10
PublicationIn this work the surface of austenitic stainless steel type X5CrNi18-10 was treated by using laser. Laser remelting was done by means of laser MLT 2500 CO2 with different parameters of treatment: P - power beam (800 [W], 1000 [W], 1100 [W], 1200 [W]); v - scanning velocity (6 [mm/s], 7 [mm/s], 8 [mm/s]); diameter of laser beam (1.4 [mm], 1.6 [mm]). The influence of these parameters on the thickness and shape of layers in manufacturing...
-
Nanostructure of the laser-modified transition metal nanocomposites for water splitting
PublicationAlthough hydrogen is considered by many to be the green fuel of the future, nowadays it is primarily produced through steam reforming, which is a process far from ecological. Therefore, emphasis is being put on the development of electrodes capable of the efficient production of hydrogen and oxygen from water. To make the green alternative possible, the solution should be cost-efficient and well processable, generating less waste...
-
The In-Depth Studies of Pulsed UV Laser-Modified TiO2 Nanotubes: The Influence of Geometry, Crystallinity, and Processing Parameters
PublicationThe laser processing of the titania nanotubes has been investigated in terms of morphology, structure, and optical properties of the obtained material. The length of the nanotubes and crystallinity, as well as the atmosphere of the laser treatment, were taken into account. The degree of changes of the initial geometry of nanotubes were checked by means of scanning electron microscopy, which visualizes both the surface and the cross-section....
-
Use laser to measure girder deflection
PublicationThe paper presents a new, simple way to measure deflection of selected intens using the device dkkz-2010, which user a laser light source.
-
Airborne Laser Scanning Point Cloud Update by Used of the Terrestrial Laser Scanning and the Low-Level Aerial Photogrammetry
PublicationLaser scanning technology is a spatial information gathering technique which is commonly used all over the world. Systems where the red-light beam are used, are divided into: terrestrial, mobile and airborne scanning systems. The main differences between those are the accuracy, the data acquisition solution (f. e. in ALS and MLS besides of the laser scanner, the inertial navigation system is required) and the covered area in one...
-
Triangular 3D Laser Scanning in Underwater Photogrammetry
PublicationThe use of triangular 3D laser scanning may significantly enhance the visual inspection of underwater objects. In these days of high demand for accurate information, exclusively photographic documentation is not enough, as it is geometrically flawed. The authors of this article are trying to present the rudiments of laser scanning, a modern means of measuring, which is reliable, relatively easy to use and works in accordance with...
-
The interaction of the pulsed laser irradiation with titania nanotubes - Theoretical studies on the thermal effect
PublicationThis paper reports temperature dispersion simulations of titania nanotubes irradiated by the 355 nm, pulsed, nanosecond laser. The modelling with the use of Finite Elements Method concerns titania nanotubes of the length and the wall thickness in the range of 0.5–2 μm and 5–20 nm, respectively. The uniqueness of the morphology was preserved by ensuring the wall thickness variation along the height of the tube, which was determined...
-
Influence of laser processing of the low alloy medium carbon structural steel on the development of the fatigue crack
PublicationThe paper contains the results of the structural analysis, hardness tests and fatigue tests conducted for the medium carbon structural steel with low content of Cr and Ni after its processing with CO2 laser beam. Pre-cracks were made in the round compact tension (RCT) specimen used for fatigue test. Next, four paths, parallel to each other, were melted on both sides of the samples using a laser beam. The paths were perpendicular...
-
Laser reflectance interferometry system with a 405 nm laser diode for in-situ measurement of CVD diamond thickness
PublicationIn situ monitoring of the thickness of thin diamond films during technological processes is important because it allows better control of deposition time and deeper understanding of deposition kinetics. One of the widely used techniques is laser reflectance interferometry (LRI) which enables non-contact measurement during CVD deposition. The authors have built a novel LRI system with a 405 nm laser diode which achieves better...