Filters
total: 1371
filtered: 329
Search results for: aluminum oxode
-
The AFM micrographs of vanadium oxides thin films obtained at 1200°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 400°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 600°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of of vanadium oxides thin films obtained at 300°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 150°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 200°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films deposited on quartz glass - the influence of the thickness of the thin film on its morphology
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a quartz glass substrate and were...
-
The AFM micrographs of vanadium oxides thin films obtained at 450°C
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films deposited on silicon - the influence of the thickness of the film on morphology
Open Research DataThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a silicon substrate and were annealing...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 200 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 100 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 300 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
The XRD diffraction patterns of as-prepared (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials synthesized via the solid state reaction method
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
XRD and electrochemical results for MoO3 films deposited using pulsed laser deposition system
Open Research DataThe attached data contains XRD and electrochemical results for MoO3 films deposited on fluorine-doped tin oxide glasses. Films were deposited using a pulsed laser deposition system at different conditions. Part of the samples was deposited at room temperature and then annealed at 575°C for given times (samples labeled PLD_RT_575C_xmin, where x stands...
-
The scanning spreading resistance microscopy (SSRM) of some CoCrMo alloys subjected to electrochemical litography
Open Research DataThe dataset contains the results of the experiment consisting of performing electrochemical lithography on the surface of the CoCrMo prosthetic alloy. First, by applying local anodic polarization, oxide structures were created on the surface of the material. Next, they were imaged in the SSRM (scanning spreading resistance microscopy) mode to visualize...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 900 deg.C in hydrogen
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 1000 deg.C in hydrogen
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 1100 deg.C in hydrogen
Open Research DataThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
Evaluation of antimicrobial properties of thermomelt adhesives modified with zinc compounds
Open Research DataThe dataset contains the results of microbiological tests of thermomelt adhesives modified with zinc compounds, whose activity was assessed for their ability to reduce the number of Escherichia coli and Staphylococcus aureus strain, representing the Gram (-) and Gram (+) bacteria, respectively. The evaluation of antimicrobial properties of samples were...
-
SEM images of Ni-Mo2CTx/Mo3AlC2 before and after catalytic dry reforming of methane
Open Research DataThe dataset includes SEM images of Ni-Mo2CTx/Mo2Ga2C catalysts before and after the dry reforming of methane.
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 4-8h.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 4-8h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Testing HIADAC high impedance analyzer in Trento University laboratory on protective foil using 2-wire probe 24h exposition
Open Research DataThe dataset presents impedance spectrum of anticorrosion foil (coating) protecting aluminium frame . This object was used to test high-impedance analyzer for diagnostic of anticorossion coatings (HIADAC) realized in the frame of Eureka project E!3174. The impedance spectrum frequency range (0.1 Hz – 100 kHz) was selected in order to test the whole...
-
Testing HIADAC high impedance analyzer in Trento University laboratory on protective foil using 2-wire probe 48h exposition
Open Research DataThe dataset presents impedance spectrum of anticorrosion foil (coating) protecting aluminium frame . This object was used to test high-impedance analyzer for diagnostic of anticorossion coatings (HIADAC) realized in the frame of Eureka project E!3174. The impedance spectrum frequency range (0.1 Hz – 100 kHz) was selected in order to test the whole...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 140 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 160 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 180 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 200 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-0optic sensor - 250 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 210 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 300 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 270 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 190 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 260 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 290 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 170 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 280 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 150 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 230 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 240 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Structural investigations of the LTO:Cu thin films
Open Research DataLithium titanate (Li1+xTi2-xO4) doped with Cu2+ ions was synthesized by sol-gel processing method. The structure was characterized by X-ray Diffraction (XRD). All samples revealed presence of LTO spinel phase. X-ray pattern of undoped LTO was free of any impurities and other crystal phases. Similarly, samples with low amount of copper dopant (x = 0.05...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.2
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.1
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM
Open Research DataThe morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h. High frequency burst recording.
Open Research DataWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. High frequency burst recording.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21,...
-
Structural investigations of the Al2O3 ultra thin films
Open Research DataUltra-thin layers of Al2O3 were deposited by atomic layer deposition (ALD) (Beneq TFS 200 ALD system). This method provides precise thickness control down to a single atomic layer. The precursors used were trimethylaluminum (Sigma-Aldrich) and purified water. The deposition of the atomic layer was carried out at 200 °C. Samples with a thickness of 2...
-
The luminescence study of Sr0.98Li2.5 + zAl1.5 – zO3 + 2zN1 – 2z:0.02Eu coumpounds.
Open Research DataEu2+-doped UCr4C4-type oxynitride phosphors are emerging innovative materials to replace oxide and nitride phosphors for high-end light-emitting devices. A series of Sr0.98Li2.5 + zAl1.5 – zO3 + 2zN1 – 2z:0.02Eu phosphors were synthesized by collaborators from the National Taiwan University by precursor engineering, and these products showed an unexpected...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.4
Open Research DataApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...