Filtry
wszystkich: 708
wybranych: 135
-
Katalog
Filtry wybranego katalogu
Wyniki wyszukiwania dla: COATING SOFC ELECTROPHORETIC DEPOSITION SPINEL ELECTRON MICROSCOPY
-
Microstructure of cross-sections of samples after laser treatment for the article entitled "Mechanical and corrosive properties of Ti13Nb13Zr alloy subjected to laser treatment with MWCNTs coatings"
Dane Badawcze -
Influence of bio-polyols with different molecular weight on properites of PUR-PIR foams
Dane BadawczeThis work attempts to validate the possibility of replacing petrochemical polyols with previously synthesized bio-polyols and their impact on the structure and properties of rigid polyurethane-polyisocyanurate (PUR-PIR). The influence of bio-polyols addition on foam properties was investigated by mechanical testing, Fourier transform infrared spectroscopy...
-
SEM micrographs of NH4VO3 crystals
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of NH4VO3 crystals obtained by the LPE-IonEx method. The SEM images clearly show that the morphology of the end product can be nicely tuned by changing the type of ammonium salt and the solvent. It can be concluded that the used solvent affected crystal shapes and their size was...
-
TEM and EDX study of the Al2O3 ultra thin films
Dane BadawczeThe ultra-thin layers of Al2O3 were deposited on a silicon substrates. The method of atomic layer deposition (Beneq TFS 200 ALD system) was chosen as the proper method of dielectric layer deposition. This method provides precise thickness control down to a single atomic layer. The precursors used were trimethylaluminum (Sigma-Aldrich) and purified water....
-
SEM micrographs of the austenitic stainless steel corrosion in asphalt fumes
Dane BadawczeThe dataset contains the scanning electron microscopy (SEM) studies of the austenitic stainless steels: AISI 304, AISI 316, AISI 321 and duplex stainless steel AISI 2205. The samples were polished and exposed to the installation carrying asphalt fumes at elevated temperatures (approx. ~210-240 Celsius). The exposition duration was three months. Some...
-
Validation of polyurethane-wood composites properties
Dane BadawczeThis study focuses on the development of the PU-WC manufacturing method, the determination of properties of this type of composite, and the indication of its potential application. The mechanical properties of PU-WC were characterized by flexural tests. To determine the thermal properties, dynamic mechanical analysis (DMA) and thermogravimetric analysis...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 200 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 100 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 300 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
SEM micrographs of diamond-phase (sp3-C) rich boron-doped carbon nanowalls (sp2-C)
Dane BadawczeThis dataset contains the Scanning Electron Microscopy (SEM) micrographs taken for rich boron-doped carbon nanowalls structures, with different boron addition during the synthesis process and different CVD synthesis duration. The [B]/[C] ratios in the plasma were set to 0k, 1.2k, 2k and 5k ppm. The time of growth was ranging between 4 and 9 hours. This...
-
TEM micrographs of ammonium vanadate nanocrystals
Dane BadawczeThe DataSet contains the TEM images of ammonium vanadate nanobelts obtained by the hydrothermal method with different conditions. The results show that the microstructure of an ammonium vanadate single nanobelt dependent on reaction condition.
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.4
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.5
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.3
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
SEM micrographs of morphology evolution of V2O5 nanostructures
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of morphology evolution of vanadium pentaoxide nanostructures obtained by the sol-gel, depending on annealing temperature under synthetic air. The results show that the morphology dependent on the annealing temperature.
-
The influence of microstructure on the corrosion resistance for some titanium-based alloys
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs revealing the microstructure of some Ti-based alloys, namely: Ti-6Al-4V (file name: TiV), Ti-6Al-7Nb (file name: TiNb) and TC21 (file name: TiAlSnZrMoCrNbSi) alloys and their localized corrosion as a result of passive layer breakdown in a corrosive environment, ie. 0.9% NaCl solution...
-
SEM micrographs of V2O5 thin films deposited on isotropic etching silicon substrates (111)
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on isotropic etching silicon substrates (111). The silicon wafers were etched in a mixture of nitric acid, hydrofluoric acid, and acetic acid in the ratio of 40:1:15. The soaking time for the substrates was from 30 to 90 seconds. The thin films were...
-
SEM micrographs of the topography of Cu-Sn-TiO2 nanocomposite coatings
Dane BadawczeThe dataset contains the scanning electron microscopy (SEM) micrographs of nanocomposite Cu-Sn-TiO2 coatings electrodeposited from oxalic acid bath containing Cu and Sn salts as well as TiO2 nanoparticles under various treatments: mechanical stirring, ultrasonic or none. The details of the electrodeposition process are presented in the readme file attached...
-
Luminescence properties of TeOx thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. The sol was obtained by vigorously stirring precursor solution at 50°C for 2h, then the temperature was raised...
-
The microstructure of AA5754 alloy under corrosion in alkaline media (pH=11) with 20 mM of various carboxylic acids
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs taken for polished aluminum AA5754 alloy samples, exposed for 100 min in bicarbonate buffer (pH=11) with the addition of 20 mM of carboxylic acids, namely: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, tricarballylic acid and serine. The goal of this study was...
-
The microstructure of AA5754 alloy under corrosion in alkaline media (pH=11) with 4.5 mM of various carboxylic acids
Dane BadawczeThis dataset contains scanning electron microscopy (SEM) micrographs taken for polished aluminum AA5754 alloy samples, exposed for 100 min in bicarbonate buffer (pH=11) with the addition of 4.5 mM of carboxylic acids, namely: citric acid, malic acid, maleic acid, succinic acid, tartaric acid, tricarballylic acid and serine. The goal of this study was...
-
The effect of cobalt addition on the corrosion behavior of near equiatomic NiTi shape memory alloy in normal saline solution, impedance and microscopic studies
Dane BadawczeThe electrochemical and corrosion (uniform and localized) behavior of a binary Ni52Ti48 shape memory alloy (SMA) and two ternary Ni52Ti48-xCox (x = 1.5 and 4.0 wt.%) SMAs were studied. Measurements were conducted in 0.9% NaCl solution at 37 oC. This dataset contains the results of electrochemical impedance spectroscopy (EIS) studies done on daily basis...
-
Morphology and conductivity investigations of nickel-molybdenium alloy by means of Scanning Spreading Resistance Microscopy
Dane BadawczeElectrolytically deposited nickel-molybdenum alloys are interesting materials because of their high corrosion resistance and low over-potential for hydrogen evolution. Despite many studies devoted to the deposition of these alloys, the mechanism of co-deposition is not fully understood [1]. The aim of the research was to preserve the electrochemically...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 140 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 160 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 180 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 200 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-0optic sensor - 250 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 210 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 300 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 270 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 190 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 260 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 290 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 170 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 280 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 150 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 230 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 240 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Luminescence properties of TeOx-Eu thin films
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Eu thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of europium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Tb thin films
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Tb thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of terbium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Dy thin films
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of dysprosium ions were added, the nitrates were used as a source of rare-earth ions....
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.2
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.1
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
SEM images of dewetted gold films
Dane BadawczeGold nanostructures were prepared on silicon - Si(111) as a substrate. as a result of dewetting process. Thin golds films were deposited using a table-top dc magnetron sputtering coater under pure Ar plasma conditions . The Au target had 99.99% purity, the rate of Au layer deposition was about 0.4 nm·s−1 and the incident power was 32 W. The thickness...
-
Images revealing the effect of local femtosecond laser ablation of conductive poly(lactic acid) 3D printed electrodes
Dane BadawczeThe dataset reveals the images of the femtosecond laser (FSL) ablation at the surface of commercially available carbon black-filled poly(lactic acid) 3D printed electrode. The process is used for the increase of the charge transfer of this electrode in electrochemical studies.
-
SEM micrographs of aluminium corrosion in alkaline media with various bee products as corrosion inhibitors
Dane BadawczeThis dataset contains various scanning electron microscopy (SEM) micrographs of AA5754 aluminum alloy samples exposed to the corrosive alkaline environment without and with the addition of various bee products to act as green corrosion inhibitors. The products are bee pollen, honey, and putty. They were investigated in bicarbonate buffer (pH =10 or...
-
Luminescence properties of TeOx-Dy thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of dysprosium ions were added, the nitrates were used as a source of rare-earth ions....