Filtry
wszystkich: 2883
wybranych: 379
-
Katalog
- Publikacje 2432 wyników po odfiltrowaniu
- Czasopisma 16 wyników po odfiltrowaniu
- Konferencje 8 wyników po odfiltrowaniu
- Wydawnictwa 1 wyników po odfiltrowaniu
- Osoby 28 wyników po odfiltrowaniu
- Projekty 2 wyników po odfiltrowaniu
- Kursy Online 16 wyników po odfiltrowaniu
- Wydarzenia 1 wyników po odfiltrowaniu
- Dane Badawcze 379 wyników po odfiltrowaniu
Filtry wybranego katalogu
Wyniki wyszukiwania dla: SUM FREQUENCY GENERATION
-
Simulation of signal acquisition from a rotary flowmeter
Dane BadawczeThe dataset contains results of simulation measuring the flow of homogeneous substances by rotational flow meter: a moment of impulse at the output of flow meter, time between successive pulses, number of pulses counted from standard generator and relative error of measurement.
-
The short-term flicker severity level measured in the industrial power system supplying the rolling mill motors
Dane BadawczeThe dataset presents a short-term flicker severity level measured on the bus bars of the main switchgear of the industrial power network for the supply of rolling mills. The data were obtained during an experiment whose purpose was to determine a level of short-term and long-term flicker caused by voltage fluctuations. In the virtual application of...
-
Sound signals generated during lapping of technical ceramics using electroplated tools with diamond grains
Dane BadawczeData contains the recordings of sound generated during single-sided lapping with the use of electroplated diamond tools. This relationship was examined with the use of spectral analysis of the sound signal in the frequency domain with a focus on the Ra parameter of the surface roughness. The estimated sound coefficient increased as the surface roughness...
-
The luminescence study of SrAl11.88−xGaxO19:0.12Cr3+ coumpounds.
Dane BadawczePortable near-infrared (NIR) light sources are in high demand for applications in spectroscopy, night vision, bioimaging, and many others. Typical phosphor designs feature isolated Cr3+ ion centers, and it is challenging to design broadband NIR phosphors based on Cr3+–Cr3+ pairs. Here, we explore the solid-solution series SrAl11.88–xGaxO19:0.12Cr3+...
-
Electrical and noise responses of graphene/AlGaN/GaN field-effect transistor for nitrogen dioxide, teatrahydrofuran, and acetone sensing
Dane BadawczeThis data set consists of raw and modified data concerning current-voltage characteristics and low-frequency noise spectra measured for graphene/AlGaN/GaN field-effect transistor in the ambiance of selected gases (laboratory air, dry and wet synthetic air, nitrogen dioxide, tetrahydrofuran, and acetone). The data show that sensor responses are enhanced...
-
The conducted immunity test of a power supply unit in accordance with EMC standards
Dane BadawczeThe dataset presents a result of measurements that are a part of immunity tests to conducted disturbances, induced by radio-frequency fields. The immunity tests were carried out on the mains cable of the DF1723003TC NDN power supply. Tests of immunity of electronic systems to conducted disturbances in the frequency range from 150 kHz to 230 MHz are...
-
AeroSense Measurements: Wind Tunnel Ecole Centrale Lyon
Dane BadawczeData from wind tunnel tests of Aerosesne measurement system installed on NACA 63418 aerfoil in the anechoic wind tunnel at the Ecole Centrale Lyon.
-
Impedance spectra of ZnO varistor type 280 model O M ver. 89
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Ambient vibrations - footbridge over the Kolibkowski Stream in Gdynia, span P2
Dane BadawczeAmbient vibration tests carried out on the P2 span of the footbridge over the Kolibkowski Stream. The research was carried out using a set of 14 acceleration sensors - MEMS accelerometers TE 4332M3-002 and TE 4312M3-002, which allowed for simultaneous measurement and recording of 20 acceleration channels. These sensors are characterized by a natural...
-
Ambient vibrations - footbridge over the Kolibkowski Stream in Gdynia, span P3
Dane BadawczeAmbient vibration tests carried out on the P3 span of the footbridge over the Kolibkowski Stream. The research was carried out using a set of 14 acceleration sensors - MEMS accelerometers TE 4332M3-002 and TE 4312M3-002, which allowed for simultaneous measurement and recording of 20 acceleration channels. These sensors are characterized by a natural...
-
Investigation of the C-1311 glucuronidation: an electrochemical approach
Dane BadawczeThis study was undertaken to investigate the glucuronidation of the compound C-1311 (5-diethylaminoethylamino-8-hydroxyimidazoacridinone – the model anticancer acridine derivative) using electrochemistry/mass spectrometry (EC/MS) as a complementary technique to in vitro (liver microsomes) and in silico approaches.
-
Data on bicycle traffic in Lodz (Poland) paired with weather and air quality data
Dane BadawczeThe file contains data on bicycle traffic registered by counting stations loacted in Lodz in the years 2016-2019. The data are paired with weather and air quality data from Lodz collected for the same period. The data is described below:
-
Data on bicycle traffic in Gdansk paired with weather and air quality data
Dane BadawczeThe file contains data on bicycle traffic registered by counting stations loacted in Gdańsk in the years 2013-2020. The data are paired with weather and air quality data from Gdansk collected for the same period. The data is described below:
-
The electrochemical studies of thin boron-doped diamond films deposited at conductive poly(lactic acid) 3D prints
Dane BadawczeThe dataset contains the electrochemical characteristics of the electrodes composed of thin boron-doped diamond films coated on commercially available graphene-doped polylactide acid. The boron doping level expressed as the [B]/[C] ratio in the gas phase for these studies was 500 and 10,000 ppm.
-
Signals of the 5G Standalone Radio Interface
Dane BadawczeThe research work conducted within the scope of NATO-STO (North Atlantic Treaty Organization – Science and Technology Organization) IST-187 group assumed investigation of the 5G gNodeB performance. The downlink (DL) signals of the FDD (Frequency Division Duplex) 5G-Standalone station were registered in isolated and controlled laboratory conditions....
-
Fuel cell noise data
Dane BadawczeMeasurement data of Hydrogen PEM fuel cels. The voltage fluctuations were measured over single cels of stack of 10 cels.
-
The conducted immunity test of an AC adaptor in accordance with EMC standards
Dane BadawczeThe dataset presents a result of measurements that are a part of immunity tests to conducted disturbances, induced by radio-frequency fields. The immunity tests were carried out on the mains cable of the ac adaptor PHILIPS DC power supply SBC 6654. Tests of immunity of electronic systems to conducted disturbances in the frequency range from 150 kHz...
-
Electrical and noise responses of graphene back-gated field-effect transistors enhanced by UV light for organic vapors sensing
Dane BadawczeBack-gated field-effect transistors with graphene channels (GFETs) were investigated toward organic vapors sensing. Two methods were used for sensing experiments including DC characteristics measurements and fluctuation-enhanced sensing by low-frequency noise studies. The data set consists of raw and modified data on GFET responses to acetonitrile,...
-
Destruction of AFM probes during normal operation
Dane BadawczeThe quality of the images obtained with the use of an atomic force microscope is determined by the state of the blade interacting with the tested material. Image artifacts can be generated by various reasons, such as oxidation, contamination or an error in blade fabrication, but also appear as a result of the repeated scanning process and inevitable...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 4-8h.
Dane BadawczeWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 4-8h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #24 - #25.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #24 (upper, rotating), #25 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #28 - #29.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #28 (upper, rotating), #29 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Wear in siding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specim. sets #20-#21, #22-#23, #24-#25, #26-#27, #28-#29,#30 - #31. Run time: 0-4h.
Dane BadawczeWear in sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer.Running time: 0 - 4h.Specimen sets:Specim. sets (# [upper, rotating] - #[lower, non-rotating]):#20-#21, #22-#23, #24-#25, #26-#27,...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #30 - #31.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #30 (upper, rotating), #31 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #20 - #21.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #20 (upper, rotating), #21 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #22 - #23.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #22 (upper, rotating), #23 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #28 - #29.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #28 (upper, rotating), #29 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Specimen running-in. Prep. to sliding friction tests. Ring-on-ring contact. Sintered alumina ceramics (98%). Paraffin oil lubrication. Specimen set #26 - #27.
Dane BadawczeSpecimen running-in procedure. Preparation to sliding friction tests in ring-on-ring contact. Sintered alumina ceramics (98%) in self-mated contact. Lubrication: paraffin oil. Sliding velocity: 0.2 m/s. Mean contact stress: 10 MPa. Test rig: PT-3 Tribometer. Specimen set #26 (upper, rotating), #27 (lower, non-rotating)CZ_PRZYS.MAT - accelerometerMOM_TAR.MAT...
-
Nonlinear impedance of as-quenched Bi2VO5.5 glass-ceramic was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of as-quenched Bi2VO5.5 glass-ceramic was measured by impedance spectroscopy method.
-
Wave propagation signals in concrete beams under 3-point bending
Dane BadawczeThe DataSet contains the results of the mechanical behaviour of a concrete beams with dimensions 40 x 40 x 160 cm3under the 3-point bending. The beams were made of concrete with the following ingredients: CEM I 42.5R (450 kg/m3), water (177 kg/m3), sand 0-2 (675 kg/m3) and gravel 2-8 (675 kg/m3). The bending test was performed using a Zwick/Roell Z10...
-
Electrical and noise responses of Graphene-Silicon Schottky diodes decorated with Au nanoparticles for light-enhanced sensing of organic gases
Dane BadawczeGraphene-Silicon Schottky junctions decorated with Au nanoparticles were used for light-enhanced detection of organic tetrahydrofuran and chloroform. Au nanoparticles exhibited localized surface plasmon resonance (LSPR) in the range of yellow light; thus yellow LED (wavelength of 592 nm) was utilized to induce the plasmonic effect, that increased the...
-
Nonlinear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic heat-treated at 913 K was measured by impedance spectroscopy method.
-
Impedance spectra of ZnO varistor type 440 model A ver. M
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 680 model A M ver. 93
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 680 model O M ver. 65 13
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 680 model A M ver. xx
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 280 model A ver. M
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 280 model 0 ver. 89
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 280 model O ver. 68
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 100 kHz down to 100 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 440 model O ver. 68
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 10 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
Impedance spectra of ZnO varistor type 680 model O M ver. 65 60
Dane BadawczeThe impedance spectrum of high-voltage ZnO varistor obtained using FRA EIS impedance spectrosocpy measurement method. The 1V sinusoidal excitation was used. The frequency range was chosen from 10 kHz down to 10 uHz. The object under test and the measuring instrument were placed in a Faraday cage due to high impedance of the object. The data was acquired...
-
The α-µ model of the multipath fading channel
Dane BadawczeThe dataset contains the results of simulations that are part of the research on modelling the multipath fading in the communication channel. The envelope of the α-µ fading process is generated using the Monte-Carlo simulation (MCS) in the LabVIEW programming environment.
-
Electrochemical impedance spectra and CV curves of V2O5 nanocrystals
Dane BadawczeThe DataSet contains the EIS spectra for coin-cells and CV curves with the V2O5 nanocrystals obtained by the sol-gel method. Cyclic voltammetry and electrochemical impedance spectroscopy (EIS) were measured using the AUTOLAB 302N potentiostat-galvanostat under Nova software. The EIS measurements were recorded in the frequency range 100 kHz to 10 mHz...
-
Electrochemical impedance spectra and CV curves of V2O5 nanorods
Dane BadawczeThe DataSet contains the EIS spectra for coin-cells and CV curves with the V2O5 nanorods obtained by the sol-gel method. Cyclic voltammetry and electrochemical impedance spectroscopy (EIS) were measured using the AUTOLAB 302N potentiostat-galvanostat under Nova software. The EIS measurements were recorded in the frequency range 100 kHz to 10 mHz for...
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Measurements of radiation emission of a portable power bank with a capacity of 10400 mAh
Dane BadawczeThe dataset contains the emission measurement results that are part of comprehensive tests carried out for portable power banks with different capacities. The measurements were performed in the frequency range from 30 MHz to 3 GHz using a Gigahertz Transverse Electromagnetic (GTEM) cell (Fig. 1). The test setup was configured to measure a portable power...
-
The voltage on bus bars of the main switchboard of the car carrier electrical power system during sea trials
Dane BadawczeThe dataset is part of the research results on the quality of supply voltage on bus bars of the main switchboard of the ship's electrical power system in different states of ship exploitation. The attached dataset contains the measurement results conducted onboard the car carrier during sea trials.