Wyniki wyszukiwania dla: Titanium oxide film
-
Dewetting of silver films detected by XPS method
Dane BadawczeDewetting of silver thin films was detected by XPS method. Thin metallic films were deposited by magnetron sputtering method. Formation of nanostructures , as a result of thermal annealing, was confirmed by SEM microscope. For comparision three samples were measured. Bulg gold, as-deposited silver film with thickness of 3 nm and nanostructures.
-
Spectroscopy properties of 1,8-diazafluoren-9-one (DFO) in PVA polymer for different concentrations
Dane BadawczeSpectroscopy properties: absorption and fluorescence spectra of 1,8-diazafluoren-9-one (DFO) in PVA film for different concentrations of dye.
-
Application of optical microsphere in fiber optic sensors for measurement of electrochemical processes
Dane Badawczeinvestigation of the electrochemical processes using micro-sphere fiber-optic sensor with a zinc oxide (ZnO) coating applied by Atomic Layer Deposition method (ALD). The measurements were performed in 1M KNO3 during a decomposition of Bisphenol-A
-
X-ray diffraction spectra of modification of TiO2 nanotubes by graphene - strontium and cobalt molybdate perovskite
Dane BadawczeData show XRD results for strontium and cobalt molybdate-modified nanotubes that were also decorated with graphene oxide. The crystalline phases were characterized by X-ray diffractometer (Philips X”Pert with detector X’Celerator Scientific).
-
The reductivity of the transition metals - calculations
Dane BadawczeThe dataset includes the reduction enthalpy and Gibbs energy simulated for Co, Cu, Fe, La, Mo, Ni, Sr, Ti, and W from oxide form into metallic form in hydrogen. Simulations were performed using HSC Chemistry software.
-
BET adsorption-desorption isotherm of nano-CeO2 impregnated with Cu
Dane BadawczeThe dataset includes the isotherms of adortion and desorption of N2 at LN2 temperature. The sorption isotherms were obtained using Quatachrome NovaTouch LX1 equippment. The catalyts powder composed of nanoCeO2 impreganted with Cu oxide nanoparticles with the usage of BCD (Beta-cyclodextrins) and without addition.
-
BET adsorption-desorption isotherm of nano-CeO2 impregnated with Co
Dane BadawczeThe dataset includes the isotherms of adortion and desorption of N2 at LN2 temperature. The sorption isotherms were obtained using Quatachrome NovaTouch LX1 equippment. The catalyts powder composed of nanoCeO2 impreganted with Co oxide nanoparticles with the usage of BCD (Beta-cyclodextrins) and without addition.
-
BET adsorption-desorption isotherm of nano-CeO2 impregnated with Mn
Dane BadawczeThe dataset includes the isotherms of adortion and desorption of N2 at LN2 temperature. The sorption isotherms were obtained using Quatachrome NovaTouch LX1 equippment. The catalyts powder composed of nanoCeO2 impreganted with Mn oxide nanoparticles with the usage of BCD (Beta-cyclodextrins) and without addition.
-
BET adsorption-desorption isotherm of nano-CeO2 impregnated with Ni
Dane BadawczeThe dataset includes the isotherms of adortion and desorption of N2 at LN2 temperature. The sorption isotherms were obtained using Quatachrome NovaTouch LX1 equippment. The catalyts powder composed of nanoCeO2 impreganted with Ni oxide nanoparticles with the usage of BCD (Beta-cyclodextrins) and without addition.
-
BET adsorption-desorption isotherm of nano-CeO2 impregnated with Fe
Dane BadawczeThe dataset includes the isotherms of adortion and desorption of N2 at LN2 temperature. The sorption isotherms were obtained using Quatachrome NovaTouch LX1 equippment. The catalyts powder composed of nanoCeO2 impreganted with Fe oxide nanoparticles with the usage of BCD (Beta-cyclodextrins) and without addition.
-
A novel method for drop in drop edible oils encapsulation with chitosan using a coaxial technique
Dane BadawczeThe dataset present a novel one step method for oil encapsulation. In this coaxial system the oil constitutes the core of the capsule, while the chitosan solution is the polymer shell surrounding the core to provide separation of the core from the external environment. In comparison to other encapsulation methods, the presented technique is much simpler...
-
XRD patterns of VO2 and V6O13 nanostructures
Dane BadawczeThe DataSet contains the XRD patterns of VO2 and V6O13 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under a reducing atmosphere (94% Ar, 6% H2) at 500, 600 and 700C for 10h.
-
SEM micrographs of VO2 and V6O13 nanostructures
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V6O13 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under a reducing atmosphere (94% Ar, 6% H2) at 600 and 700C for 10h.
-
Impact of strontium non-stoichiometry of SrxTi0.3Fe0.7O3-δ
Dane BadawczeThis dataset contains results of the research on the basis of which the Figures presented in the manuscript entitled "Impact of strontium non-stoichiometry of SrxTi0.3Fe0.7O3-δ on structural, electrical, and electrochemical properties for potential oxygen electrode of intermediate temperature Solid Oxide Cells" were prepared. A detailed description...
-
X-ray diffractometry results of the Sr0.86Ti0.65Fe0.35O3 powder
Dane BadawczeThis dataset contains results of X-ray diffractometry mesurement (XRD) of the Sr0.86Ti0.65Fe0.35O3-d (STF35) powder. The phase composition of the investigated STF35 powder was analyzed by XRD at room temperature. It confirms the formation of the cubic perovskite oxide phase. Calculated average lattice constant is a 3.90882(1) Å, with Goodness of Fit...
-
Temperature of formation of Au nanostructures
Dane BadawczeNanostructures were obtained via annealing of thin Au films. In order to determine possible nanoislands formation mechanisms, dependence on initial film thickness was examined. For the surface morphology studies, nanograin structure and chemical composition analysis, SEM, HR TEM and EDS measurements were performed, respectively. Morphology studies shown...
-
The morphology of V2O5 nanostructures deposited on quartz glass
Dane BadawczeThe DataSet contains the confocal microscope images of morphology evolution of vanadium pentaoxide nanostructures on quartz glass obtained by annealing as-prepared films at 500C and 600C under synthetic air.
-
The AFM micrographs of vanadium oxides thin films obtained at 800°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on a silicon substrate and vanadium thin films were obtained by annealing as-prepared films at...
-
The AFM micrographs of vanadium oxides thin films obtained at 1200°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 400°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 600°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of of vanadium oxides thin films obtained at 300°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 150°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 200°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 450°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 200 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 100 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 300 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Optical properties of tellurium dioxide thin films
Dane BadawczeTeO2 and TeO2 doped by Eu thin films manufactured by magnetron sputtering method were measured by optical spectroscopy. Metallic Te target and Te-Eu mosaic target with diameter of 50.8 mm were sputtered for about 45 min in argon-oxygen atmosphere what resulted in 300 nm film thickness deposition. The pressure in the chamber was below 0.2 Pa and substrate...
-
The scanning spreading resistance microscopy (SSRM) of some CoCrMo alloys subjected to electrochemical litography
Dane BadawczeThe dataset contains the results of the experiment consisting of performing electrochemical lithography on the surface of the CoCrMo prosthetic alloy. First, by applying local anodic polarization, oxide structures were created on the surface of the material. Next, they were imaged in the SSRM (scanning spreading resistance microscopy) mode to visualize...
-
The XRD diffraction patterns of as-prepared (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials synthesized via the solid state reaction method
Dane BadawczeThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
XRD and electrochemical results for MoO3 films deposited using pulsed laser deposition system
Dane BadawczeThe attached data contains XRD and electrochemical results for MoO3 films deposited on fluorine-doped tin oxide glasses. Films were deposited using a pulsed laser deposition system at different conditions. Part of the samples was deposited at room temperature and then annealed at 575°C for given times (samples labeled PLD_RT_575C_xmin, where x stands...
-
Evaluation of antimicrobial properties of thermomelt adhesives modified with zinc compounds
Dane BadawczeThe dataset contains the results of microbiological tests of thermomelt adhesives modified with zinc compounds, whose activity was assessed for their ability to reduce the number of Escherichia coli and Staphylococcus aureus strain, representing the Gram (-) and Gram (+) bacteria, respectively. The evaluation of antimicrobial properties of samples were...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 900 deg.C in hydrogen
Dane BadawczeThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 1000 deg.C in hydrogen
Dane BadawczeThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
The XRD diffraction patterns of (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials after reduction at 1100 deg.C in hydrogen
Dane BadawczeThe (La0.3Sr0.6Ce0.1)0.9Me0.1Ti0.9O3-δ (Me= Co, Cu, Fe, Mn, Ni) materials were synthesized via the solid state reaction method and examined as a potential anode material. First, the mixed oxide reagents were pressed into pellets and calcined at 1200 °C for 12 hours to decompose most of the organic compounds. The resulting calcined pellet was ground...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 0 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 40 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 30 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 200 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 20 um (serie 1)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 80 um (serie 1)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 170 um (serie 1)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 20 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 140 um (serie 1)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 130 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 50 um (serie 1)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 120 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Distance measurement with the low coherent interferometer with silver mirror (the source wavelegth 1310 nm) - 110 um (serie 2)
Dane BadawczeThe obtained data was acquired by the interferometric fiber-optic sensor of distance. The setup was constructed of a broadband light source working at the central wavelength of 1310 nm, an optical spectrum analyzer, and a fiber-optic 2x1 coupler (with the power split 50:50). All elements were connected by standard single-mode optical fibers. The measurement...
-
Plasmon resonance in gold-silver nanoalloys
Dane BadawczeSurface plasmon resonance (SPR) can lead to improve or formation a new linear or nonlinear optical phenomena. Especially it can enhance a light emission from luminescence materials. The presence of metal nanostructures or nanoparticles is necessary to excitation of the SPR. It is well known that gold and silver nanostructures exhibit plasmon resonance...