Filtry
wszystkich: 619
wybranych: 75
Wyniki wyszukiwania dla: MORPHOLOGY
-
Morphology of the gold nanoislands
Dane BadawczeDewetting of the thin metallic films leads to formation of an isolated islands. morphology of nanostructures was measured by SEM microscope. Thin gold films with a thickness of 1.2 nm, 1.5 nm and 3.4 nm were anealed at 550, 600 and 650 Celcius degress.
-
The morphology of vanadate glasses containing BaTiO3
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...
-
Morphology of the sol-gel derived LTO:Cu films
Dane BadawczeMorphology of the lithium titanate doped by Cu thin films were investigated by SEM microscope. Films were deposited by spin-coater from sol-gel derived sol. SEM images showed a high porous structure, tipaciall for sol-gel based films. For measurements samples with a various content of Cu were selected.
-
SEM micrographs of morphology evolution of V2O5 nanostructures
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of morphology evolution of vanadium pentaoxide nanostructures obtained by the sol-gel, depending on annealing temperature under synthetic air. The results show that the morphology dependent on the annealing temperature.
-
The morphology of V2O5 nanostructures deposited on quartz glass
Dane BadawczeThe DataSet contains the confocal microscope images of morphology evolution of vanadium pentaoxide nanostructures on quartz glass obtained by annealing as-prepared films at 500C and 600C under synthetic air.
-
The morphology of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
SEM micrographs of morphology evolution of V2O3 nanostructures
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O3 nanostructures obtained by the sol-gel with different reaction conditions. The xerogel powder was annealing under a reducing atmosphere (94% Ar, 6% H2) in the temperature range 350-700C. The results show that the morphology dependent on the annealing temperature.
-
The influence of chitosan hydrogels on the morphology of L929 cells
Dane BadawczeRepresentative image at 20x magnification of L929 cells following 24 h of treatment with chitosan derivatives: chitosan dissolved in carbonic acid, chitosan dissolved in carbonic acid endotoxin free, chitosan dissolved in hydroacetic acid at 1:3 diluent factor. The scale bar is 100 µm; Microscope Olympus IX83, Tokyo, Japan).
-
SEM micrographs of morphology evolution of VO2 and V2O3 nanostructures
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 nanostructures obtained by the sol-gel with different reaction conditions. The information about xerogel powder synthesis is described in the Journal of Nanomaterials. The xerogel powder was annealing under argon atmosphere in the temperature range 400-800C. The...
-
Morphology and structure of ammonium vanadates synthesis by hydrothermal method
Dane BadawczeThe DataSet contains the XRD patterns, FTIR spectra, and scanning electron microscopy (SEM) micrographs of ammonium vanadates synthesis by hydrothermal method from different NH4VO3 precursors. The results reveal that a mixture of (NH4)V4O10xH2O and(NH4)0.76V4O10 was obtained for both precursors, however the contribution of each phase was different for...
-
The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...
-
The morphology of lead-borate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped borate glasses and glass-ceramics were studied. Samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 < x < 37 in mol%) were prepared by the conventional meltquenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate...
-
The morphology of lead-silicate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass...
-
The morphology of lead-silicate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped glasses and glass-ceramics were studied. Samples has the composition of 50SiO2–(50−x)PbO–xFe2O3, where x=15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in air at 1623 K in alumina crucibles. The melts were poured on a brass plate preheated to 573...
-
Morphology and structure of V2O5 nanorods deposited on the silicon substrate after reduction
Dane BadawczeThe DataSet contains the XRD patterns and SEM micrographs of V2O5 nanorods on the silicon substrate after thermal treatment under a reducing atmosphere. Thin films were annealed at 500C for 40 under a reducing atmosphere (94% Ar, 6% H2).
-
SEM micrographs of V2O5 thin film morphology dependent on substrate types
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin film morphology dependent on substrate types. The as-prepared thin films were deposited on alumina, zirconium, zirconium oxide and metallic vanadium substrate, then was annealing under an oxidizing atmosphere at 600C for 10h. The results show that the morphology of...
-
SEM micrographs of morphology evolution of V2O5 thin films on quartz glass
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a quartz glass substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 200-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
SEM micrographs of morphology evolution of V2O5 thin films on silicon substrate
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on a silicon substrate. The as-prepared thin films were annealing under an oxidizing atmosphere in the temperature range 250-600C. The results show that the morphology of the films dependent on the annealing temperature.
-
The morphology of vanadate glass-ceramics containing BaTiO3 measured with the use of AFM
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by AFM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
XRD patterns of V2O5 thin film morphology dependent on substrate types
Dane BadawczeThe DataSet contains the XRD patterns of the V2O5 thin film structure dependent on substrate types. The as-prepared thin films were deposited on alumina, zirconium, zirconium oxide and metallic vanadium substrate, then was annealing under an oxidizing atmosphere at 600C for 10h.