The morphology of vanadate glass-ceramics containing BaTiO3 measured with the use of AFM
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by AFM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
The structure of vanadate glass-ceramics containing BaTiO3 measured with X-ray diffraction method
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by XRD. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
The morphology of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Linear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glass-ceramics containing BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
The morphology of lead-borate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped borate glasses and glass-ceramics were studied. Samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 < x < 37 in mol%) were prepared by the conventional meltquenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate...
-
The structure of lead-borate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe structure of iron-doped glasses and glass-ceramics were studied. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate and...
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...
-
Electrical properties of lead-borate glasses and glass-ceramics containing iron ions
Dane BadawczeElectrical properties were studied for borate-lead glasses and glass-ceramics doped with iron ions. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated...
-
Linear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
The structure of vanadate glass-ceramics containing BaTiO3.
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
The topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope
Dane BadawczeThe topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope.
-
Depth chemical profile in a CeIr3 sample
Dane BadawczeThe polycrystalline sample of CeIr3 used in the present studies was synthesized by arc-melting cerium (4N) and iridium (3N5) in an arc furnace on a water-cooled copper hearth using a tungsten electrode under a high purity argon atmosphere. A piece of zirconium was used as an oxygen getter. First, a button of Ir was prepared by arc-melting the iridium...
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
The morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with AFM
Dane BadawczeThe morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses was measured with the use of atomic force microscope.
-
The morphology of vanadate glasses containing BaTiO3
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...
-
The topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with confocal microscope
Dane BadawczeThe topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with confocal microscope.
-
The topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with AFM
Dane BadawczeThe topography of as-quenched and heat treated 50(2Bi2O3-V2O5)-50SrB4O7 and 50Bi2VO5.5-50SrB4O7 glasses measured with AFM.
-
The structure of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with X-ray diffraction method
Dane BadawczeThe structure of strontium–borate glasses and glass-ceramics containing Bi2VO5.5 nanocrystallites was measured by XRD.
-
Thermal properties of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with DSC method
Dane BadawczeThermal properties of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. was measured by DSC.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 613 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Thermal properties of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides measured with DSC method
Dane BadawczeThermal properties of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides was measured by DSC.
-
Thermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with DSC
Dane BadawczeThermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by DSC.
-
Linear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
The structure of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides measured with X-ray diffraction method
Dane BadawczeThe structure of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides was measured by XRD.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear and nonlinear impedance of iron containing silicate glasses
Dane BadawczeThe linear and nonlinear impedance ofglasses doped with iron oxide were measured. Glass samples (50 SiO2-50-xPbO-xFe2O3 in mol%) were prepared by the conventional melt quenching technique. The substrates were powdered in a mortar and melted in Al2O3 crucibles. The melting was conducted in air at 1623K. The melts were poured out on plate heated up to...
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 annealed glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of as-quenched 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched Bi2VO5.5 glass-ceramic was measured with impedance spectroscopy method at low temperature region