Filtry
wszystkich: 791
Wyniki wyszukiwania dla: bead-on plate welding
-
Nonlinear harmonic amplitudes in air coils above and below a metal plate as a function of tensile strength via finite element simulation.
PublikacjaOpisano wyniki obliczeń numerycznych (symulacja metodą MES) wpływu naprężeń na amplitudy nieliniowych harmonicznych napięcia indukowanego w cewkach powietrznych umieszczonych nad i pod płytą.
-
Effect of water salinity on properties of multipass underwater wet manual metal arc welded joints
PublikacjaThe weldability of steel under the water is limited due to the influence of the environment. Water causes limited visibility, presence of the residual stresses, increasing the cooling rate, and increasing the diffusible hydrogen content in deposited metal, leading to the formation of brittle microstructures in heat-affected zone (HAZ). The paper presents the results of mechanical properties testing of S420G2+M steel welded joints...
-
Simulation of hybridized nanofluids flowing and heat transfer enhancement via 3-D vertical heated plate using finite element technique
PublikacjaThe present study probed the creation of heat energy and concentrating into Newtonian liquids across vertical 3D-heated plates. The role of the Soret and Dufour theories in concentrating and energy formulas is discussed. The role of hybrid nanoparticles is introduced to illustrate particle efciency in terms of solute and thermal energy. It is removed a viscous dissipation process and a changing magnetic feld. The proposed approach...
-
Stalowe panele sandwicz - nowe możliwości wynikające z zastosowania spawania laserowego = All steel sandwich panels - new possibilities introduced by laser welding techniques
PublikacjaW artykule przedstawiono podstawowe dane na temat stalowych paneli typu sandwicz i technik ich wykonywania. Złącze takie charakteryzuje się specyficznymi własnościami, zdecydowanie odmiennymi od klasycznego połączenia spoiną pachwinową, którego cechy wytrzymałościowe i technologiczne są już dobrze opanowane. W podsumowaniu wykazano, że modelowanie jego geometrii musi być prowadzone na znacznie większym poziomie szczegółowości ze...
-
Evaluation by means of magneto-acoustic emission and Barkhausen effect of time and space distribution of magnetic flux density in ferromagnetic plate magnetized by a C-core
PublikacjaPokazano wyniki badań emisji magnetoakustycznej (EMA) i efektu Barkhausena (HEB) dla dwóch płyt stalowych o różnych wymiarach. Wyniki te są porównane z wynikami modelowania zjawiska EMA z wykorzystaniem metody elementów skończonych z uwzględniem efektu prądów wirowych. Uzyskano zadawalające dopasowanie modelu, który odtwarzał poszerzenie maksimum EMA oraz przesunięcie fazowe i zmianę amplitudy HEB.
-
Teoretyczna analiza procesu walcowania trójwarstwowego pasma AlMg-Al-Cu, Theoretical analysis of rolling process of composite plate AlMg-Al-Cu
PublikacjaPrzedstawiono symulacje komputerowe walcowania blach AlMg-Al-Cu łączonych wybuchowo. Symulacje przeprowadzono dla procesu walcowania w walcarce o średnicy walców D=150 mm z indywidualnym napędem walców roboczych. W ramach badań numerycznych określono wpływ nierówności odkształcenia warstw tworzących pasmo oraz nieliniowy rozkład predkości warstw blachy w kotlinie walcowniczej asymetrycznie walcowanej blachy trójwarstwowej AlMg-Al-Cu.
-
Annals of "Dunarea de Jos" University of Galati, Fascicle XII, Welding Equipment and Technology
Czasopisma -
Tytanowa międzywarstwa w łącznikach do spawania Al i stopów AlMg ze stalą=Titanium interlayer in transition joints to welding aluminium and aluminium alloys AlMg with steel
PublikacjaPrzedstawiono idee stosowania łączników i ich wytwarzanie oraz własności i niedostatki obecnie stosowanych łączników. Zaprezentowano wyniki prób technologicznych wytwarzania oraz wyniki badań mechanicznych i strukturalnych trójwarstwowego łącznika stal-tytan-aluminium.
-
Corrigendum to “Photocatalytical properties of maze-like MoO3 microstructures prepared by anodization of Mo plate” [Electrochim. Acta 228 (20 February) (2017) 139–145]
Publikacja -
Viscoplastic damage analysis of plate-shell structures subjected to impact loading = Lepkoplastyczna analiza zniszczenia konstrukcji płytowo-powłokowych pod wpływem obciążeń dynamicznych
PublikacjaW pracy przedstawiono rozważania nad analizą zachowania się konstrukcji płytowo-powłokowych pod wpływem obciążeń dynamicznych wzbudzanych przez eksplozje mieszanki gazowej. Zagadnienie to jest poddane badaniom ukierunkowanym na aspekty mechaniczne, głównie na przewidywanie ciągliwego zniszczenia. W pierwszej kolejności zaprezentowano przegląd literatury oraz opisano teorie, które w dzisiejszych czasach są najczęściej stosowane...
-
Deformation of the Titanium Plate Stabilizing the Lateral Ankle Fracture Due to Its Overloading in Case of the Young, Obese Patient: Case Report Including the Biomechanical Analysis
Publikacja -
EH36 steel for shipbuilding (plate thicnkness 30 mm) - 3D fracture scan
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
Michał Wasilczuk prof. dr hab. inż.
OsobyMichał Wasilczuk, absolwent Wydziału Budowy Maszyn Politechniki Gdańskiej (1986), a obecnie profesor zwyczajny na Wydziale Mechanicznym PG i kierownik Katedry Konstrukcji Maszyn i Pojazdów od początku swojej działalności naukowej zajmuje się hydrodynamicznymi łożyskami wzdłużnymi oraz, szerzej inżynierią łożyskowania, w ramach zespołu naukowego stworzonego przez doc. Olgierda Olszewskiego. Od kilkunastu lat zespół specjalizuje...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 60mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 40mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 40mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 60 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 50mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 50mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
Expression of metalloproteinase 2 (MMP-2) and metalloproteinase 9 (MMP-9) in THP-1 macrophages cultured with three-dimensional titanium mini-plate systems used for surgical treatment of condylar fractures
Publikacja -
In vitro effect of three-dimensional (3D) titanium mini-plate systems used for surgical treatment of condylar fractures on interleukin 1 (IL-1) and interleukin 6 (IL-6) concentration in THP-1 macrophages
Publikacja -
Wpływ współczynnika promienia walca i stosunku grubości warstw na odkształ- cenie warstwy twardej. The influence of radius of rolls coefficient and re-lations of thickness layers at the deformation of hard layers of bimetalic plate
PublikacjaW pracy przedstawiono analizę numeryczną walcowania blachy platerowanej 18 G2A i 0H18N10T. Wytwarzanie blach dwuwarstwowych jest procesem trudnym do rozwiązania na drodze teoretycznej. Do analizy procesu wykorzystano program Forge 2 oparty na teorii elementów skończonych. Artykuł przedstawia wpływ wartości współczynnika promienia walcaH/R i stosunku grubości warstw HT/HM na charakter rozkładu odkształceń blachy dwuwarstwowej.
-
Numeryczna analiza wpływu kierunku rozchodzenia się fali wybuchu na krzywiznę asymetrycznie walcowanego pasma Al-Cu. Numerical analysis the influence of the direction of explosion wave at the curvature of asymmetrical rolling of bimetallic plate.
PublikacjaW artykule przedstawiono numeryczną analizę wpływu kierunku rozchodzenia się fali wybuchu na krzywiznę asymetrycznie walcowanego pasma Al-Cu. Przeprowadzono symulacje dla procesu walcowania w temperaturze 20 C. Proces walcowania prowadzono w walcarce duo D 150 mm, o prędkości obwodowej 18,5 obr/min. Badania przeprowadzono dla dwóch stosunków grubości warstw 2/10 i 4/8. Symulację procesu przeprowadzono dla trzech gniotów 10%, 20%,...
-
Prediction of Weld Deformations by Numerical Methods - Review
PublikacjaThe welding process is the basic technique of joining in the shipbuilding industry. This method generates welding distortions that cause a lot of problems during the manufacturing process due to both the time and cost of straightening as well as their influence on later stages of production. Proper preparation of welding processes plays a growing role in the shipbuilding industry and the development of calculating tools is being...
-
Selection of material for X-ray tomography analysis and DEM simulations: comparison between granular materials of biological and non-biological origins
PublikacjaPhysical properties and X-ray tomography images of five different granular materials: glass bead, glass grit, short grain white rice, sorghum and clay granules (Seramis) are investigated to select the most promising materials for numerical simulations and time-lapse X-ray tomography imaging. The examined materials represent granular materials of non-biological origin (glass bead, glass grit and Seramis) and granular plant materials...
-
Effects of Storing Flux-Cored Wires under Various Conditions
PublikacjaWelding processes involving the use of flux-cored wires are becoming increasingly popular, particularly in shipbuilding as well as in off-shore and civil engineering. The article presents characteristics of the welding process, its areas of application as well as advantages and disadvantages (e.g. necessity of ensuring appropriate conditions for the storage of filler metal wires). The satisfaction of quality-related requirements...
-
Cold Cracking Of Underwater Wet Welded S355G10+N High Strength Steel
PublikacjaWater as the welding environment determines some essential problems influencing steel weldability. Underwater welding of high strength steel joints causes increase susceptibility to cold cracking, which is an effect of much faster heat transfer from the weld area and presence of diffusible hydrogen causing increased metal fragility. The paper evaluates the susceptibility to cold cracking of the high strength S355G10+N steel used,...
-
Assessment of Corrosive Behaviour and Microstructure Characterization of Hybrid Friction Stir Welded Martensitic Stainless Steel
PublikacjaThis study examined the effect of induction heating on the microstructure and corrosion characteristics of hybrid friction stir welded AISI 410 stainless steel. Five joints have been produced with different friction stir welding parameters like welding speed, spindle speed, plunge depth, and induction power. Their microstructures were evaluated using a scanning electron microscope, and chemical composition was examined using...
-
THE INFLUENCE OF MANUFACTURING OVERSIZING ON POSTWELDING DISTORTIONS OF THE FILLET WELDED JOINT
PublikacjaWelding proces is basic joining technique in shipbuilding. Such method generated welding distortions which cause a lot of problems during the manufacturing process. In the literature it is proposed wide spectrum of suggestions for a correct estimation of welding deformation in particular angular deformation in the fillet welded T joint. In the work influence of oversizing of weld on angular distortions of joint is presented basing...
-
Weldability of S460ML High Strength Low Alloy Steel in Underwater Conditions
PublikacjaThe paper presents experimental evaluation of susceptibility of the high strength S460ML steel to cold cracking in the conditions of wet welding with the use of covered electrodes. From the results of Tekken tests it was found out that the investigated steel was characterised, in the conditions of the carried out experiments (underwater wet welding and air welding with rutile electrodes), of high susceptibility to cold cracking....
-
The Influence of Tool Shape and Process Parameters on the Mechanical Properties of AW-3004 Aluminium Alloy Friction Stir Welded Joints
PublikacjaThe purpose of the following study was to compare the effect of the shape of a tool onthe joint and to obtain the values of Friction Stir Welding (FSW) parameters that provide the bestpossible joint quality. The material used was an aluminium alloy, EN AW-3004 (AlMn1Mg1). To theauthors’ best knowledge, no investigations of this alloy during FSW have been presented earlier. Fivebutt joints were made with a self-developed, cylindrical,...
-
The Influence of Selected Parameters of Numerical Modelling on Strains and Stresses at Weld Toe Notch
PublikacjaLatest development in the field of welding technology and prefabrication enabled massive production of thin-walled sandwich structures. Multi-layered sandwich structures are fabricated with the use of high-power CO2 lasers, friction welding, arc welding, hybrid welding, or other technique designed for the special purpose. Steel or aluminium alloy plates with thickness between 1 and 5 mm are connected by internal stiffeners. Strength...
-
Weldability of S500MC Steel in Underwater Conditions
PublikacjaWet welding with the use of covered electrodes is one of the methods of underwater welding. This method is the oldest, the most economic and the most versatile. The main difficulties during underwater wet welding are: high cooling rates of the joint, the presence of hydrogen in the arc area and formation of hard martensitic structure in the weld. These phenomena are often accompanied by porosity of welds and large number of spatters,...
-
Effect of Arc Strikes on High Strength Low Alloy Steels Welded by SMAW
PublikacjaWet welding with covered electrodes (Shielded Metal Arc Welding – SMAW) is the most commonly used method of carrying out welding repair works in a water environment. Limited visibility and the inability to move freely under water result in an increased risk of formation of welding imperfections such as lack of fusion, lack of penetration and arc strikes. The work focused on changes in the properties and structure of steel subjected...
-
Regeneration of marine engine valves using laser surfacing
PublikacjaThis article presents an analysis of the applicability of laser surfacing of the exhaust valve face of a marine diesel engine using cobalt-based powder. After preparation by machining, the selected valves were subjected to laser surfacing using a high-power ROFIN DL020 laser. The EuTroLoy 16012 powder was used in the surfacing process. One of the valves was cut and subjected to metallographic examination and hardness measurements,...
-
Investigations into tendency to stress corrosion of joints welded in austenitic and duplex steels
PublikacjaPrzedstawiono wyniki badań spawanych złączy różnoimiennych wykonanych ze stali austenitycznej oraz typu duplex 2205. Badania podatności do korozji naprężeniowej złączy wykonano metodą odkształcania z małą prędkością. Próby przeprowadzono w środowisku obojętnym oraz agresywnym (MgCl2).
-
Heat tint colours on stainless steel and welded joints
PublikacjaSurface layer condition of stainless steels and welded joints influences strongly their corrosion resistance. This problem seems to be underestimated. This current study explains the phenomenon of heat tint forming on welds, the methods of its removal, inspection procedures after heat tint removing and post weld finishing
-
Research into GTA automatic soft soldering technology for solar energy collector components
Publikacja -
A study of modern materials for arc spraying
Publikacja -
Effect of Porosity on the Thermo-Mechanical Behavior of Friction-Stir-Welded Spark-Plasma-Sintered Aluminum Matrix Composites with Bimodal Micro- and Nano-Sized Reinforcing Al2O3 Particles
PublikacjaThe thermo-mechanical behavior of nanosized Al2O3 particles reinforcing aluminum was analyzed in the present paper. The material was prepared by spark plasma sintering and friction stir welding. The thermal stresses affecting the composite behavior during welding were modeled through COMSOL MultiPhysics, and the results were validated by the analyses of the composites’ mechanical properties. The spark-plasma-sintered materials...