Filters
total: 42
Search results for: nanoindentation
-
Nanoindentation tests titanium alloy Ti-6Al-4V after interference laser treatment
PublicationThe study aimed was to assess selected mechanical properties of surface layers obtained after interference laser treatment – DLIL of titanium alloy Ti-6Al-4V used for implants. The samples were melted in still air at room temperature, for this purpose Nd:YAG laser was used, the number of laser shots was variable. Next, nanoindentation tests were performed, based on which Young’s modulus and nanohardness in the obtained surface...
-
Application of the nanoindentation method in assessing of properties of cement composites modified with silica-magnetite nanostructures
Publication -
Mechanical Properties and Wear Susceptibility Determined by Nanoindentation Technique of Ti13Nb13Zr Titanium Alloy after “Direct Laser Writing”
PublicationLaser treatment has often been applied to rebuild the surface layer of titanium and its alloys destined for long-term implants. Such treatment has always been associated with forming melted and re-solidified thin surface layers. The process parameters of such laser treatment can be different, including the patterning of a surface by so-called direct writing. In this research, pulse laser treatment was performed on the Ti13Nb13Zr...
-
Results of nanoindentation, XRD and microscopic studies of bacterial cellulose
Open Research DataThe archive contains the results of research on BNC bacterial biocellulose, which was modified in two ways. When BNC was synthesized, it was subjected to in situ modification involving the addition of hyuloronic acid to the bacterial medium. The second way of ex situ modification consisted of soaking the BNC in water and then convectionally drying it...
-
Nanoindentation tests of the hydroxyapatite composite coatings applicated on titanium alloys by the electrophoretic method
Open Research DataCurrently, there are no metal materials that meet all biomechanical and biochemical requirements needed for long life implantable biomaterials. The main purpose of the study was to functionalize the surface of the titanium alloys used in biomaterial implants.
-
Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-load
Open Research DataThe DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum load of Berkovich indenter force from 2 to 50 mN.
-
Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-depth
Open Research DataThe DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum depth of Berkovich indenter penetration: 60, 70, and 100 nm.
-
Results of nanoindentation test to calculate residual stress in an eyelet of undercarriage drag strut after laser treatment
Open Research DataIn order to determine the residual stress in the laser-processed an eyelet of undercarriage drag strut, a nanoindentation test was performed before and after stress relief annealing. For this purpose, after the hardness test, the sample was subjected to stress relief annealing at 270 °C for 2 hours. Annealing was performed in a vacuum furnace. Hardness...
-
Results after grinding C45 steel
Open Research DataThe database contains results from nanoindenter, scanning microscope and also X-ray diffractometer. To determine the residual stresses and the size of the crystallites in the ferrite grains in the grinded surface layer, the Williamson Hall analysis of the X-ray diffraction patterns was performed. XRD diffraction patterns were also used to perform a...
-
Microstructure and mechanical properties of laser surface-treated Ti13nb13zr alloy with MWCNTs coatings
PublicationLaser surface modification of titanium alloys is one of the main methods of improving the properties of titanium alloys used in implantology. This study investigates the microstructural morphology of a laser-modified surface layer on a Ti13Nb13Zr alloy with and without a carbon nanotube coating deposited by electrophoretic deposition. Laser modification was performed for samples with and without carbon nanotube coating for two...
-
The Influence of Nanometals, Dispersed in the Electrophoretic Nanohydroxyapatite Coatings on the Ti13Zr13Nb Alloy, on Their Morphology and Mechanical Properties
PublicationIn this work, nanohydroxyapatite coatings with nanosilver and nanocopper have been fabricated and studied. The presented results concern coatings with a chemical composition that has never been proposed before. The present research aims to characterize the effects of nanosilver and nanocopper, dispersed in nanohydroxyapatite coatings and deposited on a new, non-toxic Ti13Zr13Nb alloy, on the physical and mechanical properties of...
-
Influence of Surface Laser Treatment on Mechanical Properties and Residual Stresses of Titanium and its Alloys
PublicationSurface modification of the titanium and its alloys used in implantology with a long-pulse laser can change the surface topography, but it also leads to changes in the stress sign and magnitude in the resulting subsurface layer. The presented research was aimed at evaluating the state of stress after laser remelting with the Nd:YAG laser of pre-etched titanium alloys Ti6Al4V and Ti13Nb13Zr and pure titanium. The obtained surface...
-
Study of nanomechanical properties of (1-y)BST-yMgO thin films
PublicationIn the present study thin films of MgO – modified Ba0.6Sr0.4TiO3 (BST60/40) solid solution were prepared by the sol-gel-type chemical solution deposition method on stainless steel substrates. A multilayer spin-coating approach was utilized for the Ba0.6Sr0.4TiO3-MgO thin film deposition with subsequent thermal annealing at T=650-750C. Dried BST60/40-MgO gel powders were studied with thermogravimetric and differential thermal analysis...
-
Effects of electrophoretic deposition times and nanotubular oxide surfaces on properties of the nanohydroxyapatite/nanocopper coating on the Ti13Zr13Nb alloy
PublicationLoad-bearing implants are developed with a particular emphasis placed on an application of ceramic hydroxyapatite coatings in order, to enhance the bioactivity of titanium implants and to shorten the healing time. Therefore, thin, fully crystalline coatings that are, highly adhesive, hydrophilic and demonstrating antibacterial properties are ly looked for. The aim of this research was to develop and characterize the properties...
-
Hydrogen Embrittlement and Oxide Layer E ect in the Cathodically Charged Zircaloy-2
PublicationThe present paper is aimed at determining the less investigated effects of hydrogen uptake on the microstructure and the mechanical behavior of the oxidized Zircaloy-2 alloy. The specimens were oxidized and charged with hydrogen. The different oxidation temperatures and cathodic current densities were applied. The scanning electron microscopy, X-ray electron diffraction spectroscopy, hydrogen absorption assessment, tensile, and...
-
The Influence of the Depth of Cut in Single-Pass Grinding on the Microstructure and Properties of the C45 Steel Surface Layer
PublicationThe paper contains the results of a metallographic examination and nanoindentation test conducted for the medium carbon structural steel with low content of Mn, Si, Cu, Cr, and Ni after its grinding to a depth ranging from 2 μm to 20 μm, at constant cutting speed (peripheral speed) of vs = 25 ms−1 and constant feed rate of vft = 1 m/min. Applied grinding parameters did not cause the surface layer hardening, which could generate...
-
Physicochemical and Mechanical Performance of Freestanding Boron-Doped Diamond Nanosheets Coated with C:H:N:O Plasma Polymer
PublicationThe physicochemical and mechanical properties of thin and freestanding heavy boron-doped diamond (BDD) nanosheets coated with a thin C:H:N:O plasma polymer were studied. First, diamond nanosheets were grown and doped with boron on a Ta substrate using the microwave plasma-enhanced chemical vapor deposition technique (MPECVD). Next, the BDD/Ta samples were covered with nylon 6.6 to improve their stability in harsh environments and...
-
Effects of solution composition and electrophoretic deposition voltage on various properties of nanohydroxyapatite coatings on the Ti13Zr13Nb alloy
PublicationThe purpose of the research was to establish the influence of the solution composition and the electrophoretic deposition voltage on the coating homogeneity and thickness, nanohardness, adhesion, corrosion resistance and wettability. The Ti13Zr13Nb alloy was coated by the electrophoretic technique with hydroxyapatite in a solution containing 0.1, 0.2 or 0.5 g nanoHAp in 100 mL of suspension and at voltage 15, 30 or 50 V. The scanning...
-
The Influence of Laser Alloying of Ti13Nb13Zr on Surface Topography and Properties
PublicationThe laser alloying is a continually developing surface treatment because of its significant and specific structuration of a surface. In particular, it is applied for Ti alloys, being now the most essential biomaterials` group for load-bearing implants. The present research was performed on the Ti13Nb13Zr alloy subject to laser modification in order to determine the treatment effects on surface topography and its some mechanical...
-
Biological and mechanical research of titanium implants covered with bactericidal coating
PublicationThe paper concerns the biological and mechanical properties of titanium implants with an antibacterial coating. The Ti13Zr13Nb alloy samples were coated with hydroxyapatite (HAp) coatings using the electrophoretic deposition technique (EPD). Subsequently, the surface of the samples was modified with silver, copper, and nickel nanoparticles by the immersion method. Different titanium sample types (i.e. HAp-only and nanometals-enriched...