Filters
total: 7822
filtered: 1572
-
Catalog
- Publications 5543 available results
- Journals 76 available results
- Conferences 3 available results
- Publishing Houses 1 available results
- People 133 available results
- Inventions 5 available results
- Projects 12 available results
- Laboratories 1 available results
- Research Teams 2 available results
- Research Equipment 1 available results
- e-Learning Courses 183 available results
- Events 9 available results
- Open Research Data 1853 available results
Chosen catalog filters
displaying 1000 best results Help
Search results for: PERFORATED PLATES
-
The voltage on bus bars of the main switchboard of the ferry electrical power system during a sea voyage
Open Research DataThe dataset is part of the research results on the quality of supply voltage on bus bars of the main switchboard of the ship's electrical power system in different states of ship exploitation. The attached dataset contains the measurement results carried out onboard the ferry during a sea voyage.
-
The voltage on bus bars of the main switchboard of the ro-ro ship electrical power system during a sea voyage
Open Research DataThe dataset is part of the research results on the quality of supply voltage on bus bars of the main switchboard of the ship's electrical power system in different states of ship exploitation. The attached dataset contains the measurement results carried out onboard a ro-ro ship during a sea voyage.
-
The voltage on bus bars of the main switchboard of the ro-ro ship electrical power system during maneuvering
Open Research DataThe dataset is part of the research results on the quality of supply voltage on bus bars of the main switchboard of the ship's electrical power system in different states of ship exploitation. The attached dataset contains the measurement results carried out onboard a ro-ro ship during maneuvering.
-
The voltage on bus bars of the main switchboard of the ferry electrical power system during maneuvering
Open Research DataThe dataset is part of the research results on the quality of supply voltage on bus bars of the main switchboard of the ship's electrical power system in different states of ship exploitation. The attached dataset contains the measurement results carried out onboard the ferry during maneuvering.
-
D.C. electrical measurements of Bi2VO5.5 ceramic measured at high temperature region
Open Research DataD.C. electrical properties of Bi2VO5.5 ceramic was measured.
-
Reduction of the strontium titanate doped by Ytrium ceramics observed by X-ray photoemission spectroscopy method
Open Research DataYtrium-doped strontium titanate (YSTF) ceramics materials were manufactured by three various methods: 1) standard solid-state reaction method from Y2O3 (Sigma Aldrich, 99,9%), TiO2 (Sigma Aldrich, 99%) and SrCO3 (Sigma Aldrich,98%), 2) Pechini method, 3) wet method.
-
Plaque of Dorothy and John Brandes in St. Mary's Church in Gdańsk
Open Research DataThe data set concerns epigraphy. It refers to the plaque placed in St. Mary’s Church in Gdańsk, that is dedicated to John Brandes, highly influential citizen of Gdańsk, whose official career was crowned with the function of mayor, and his wife Dorothy née Zimmermann. The plaque was placed in the church in 1586. Data set contains two photos of the plaque,...
-
Nonlinear impedance as a function of A.C. voltage for glass 40Bi2VO5.5-60SrB4O7 annealed at 473 K for 3h and next fully crystallized measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for annealed at 473 K for 3h and next fully crystallized 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for fully crystallized 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for fully crystallized 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched glass 40Bi2VO5.5-60SrB4O7 after full crystallization was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of as-quenched glass 40Bi2VO5.5-60SrB4O7 afetr full crystallization was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 473 K for 3 h measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 473 K for 3h was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for annealed at 593 K and next fully crystallized 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of glass 40Bi2VO5.5-60SrB4O7 annealed at 473 K for 3h and next fully crystallized was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 fully crystallized glass at 813 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 593 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 partially crystallized glass at 613 K measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 partially crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for fully crystallized 45Bi2VO5.5-55SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties as a function of A.C. voltage for fully crystallized 45Bi2VO5.5-55SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured with impedance spectroscopy method at high temperature region
Open Research DataThe nonlinear electrcial properties of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured by impedance spectroscopy method.
-
Voltage fluctuations on the main switchgear of the industrial power system supplying the rolling mill motors_part_2
Open Research DataThe dataset presents the voltage waveforms on the bus bars of the main switchgear of the industrial power network for the supply of rolling mills. The data was recorded during an experiment whose purpose was to determine a level of short-term and long-term flicker caused by voltage fluctuations. In the virtual application of flickermeter, a hardware...
-
TG analyses - content of SiO2 and TiO2 in polystyrene
Open Research DataTG analyses were performed for polystyrene spheres coating by SiO2 and then coating by SiO2-TiO2. Thermal analyses of polystyrene spheres only were also performed. The content of inorganic remaining was used for calculation the quantity of coating SiO2 and TiO2 in the polystyrene spheres.
-
Ethylene photocatalytic decomposition in high temperature reaction chamber
Open Research DataData contain data logs of measurements performed on High Temperature Chamber "The Praying Mantis" coupled with SRI 8010 gas chromatograph. Measurement was performed for TiO2 irradiated by UV and under flowing of ethylene gas diluted in air and with the use of elevated temperature.
-
EU state aid - compatible with the internal market for social reasons
Open Research DataThe dataset encompasses a choice of Polish and foreign bibliography, together with a list of important individual EC decisions issued in the period 2007-2013 on state aid delivered to final consumers for social reasons ( in Poland and in selected UE member states), in form of different financial instruments. Thanks to this compilation the reader is...
-
Effects of CO2 and utilization of spent trickling liquid towards plant growth
Open Research DataDataset presents the results of biomass yield for Phaseolus vulgaris pot cultures watered with diluted trickling liquid from biotrickling filtration experiments with or without additional CO2 in air by means of introducting post-biofilter air to the plant culture.
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
The rovibrational energy levels of the diatomic silver anion and neutral silver dimer
Open Research DataThe process of a two-channel decay of the diatomic silver anion (Ag2-), namely the spontaneous electron ejection giving Ag2 + e- and the dissociation leading to Ag- + Ag is theoretically studied. The ground state potential energy curves (PECs) of the neutral silver dimer and anionic silver diatomic molecule are calculated using the single reference...
-
IRAP tax differentiation in Italian Regions
Open Research DataThe following table presents the widespread differentiation in the standard IRAP rates applied in the particular regions of Italy. The tax rates in the table have been updated to 2019 (Only Regions marked with "*" updated their tax rates to the 2020 tax period as of March 16, 2020).
-
Proceeds from value added tax to the state budget as a percentage of the revenues (2010-2014)
Open Research DataFrom 1 January 2011, there was a general increase in the rates of tax on goods and services. According to the assumptions, it was temporary, and the amended regulations were to apply until the end of 2013. However, due to government policy, the rate hike was maintained. The changes introduced in 2010 concerned the basic and reduced rates - they were...
-
Electrical properties of lead-borate glasses and glass-ceramics containing iron ions
Open Research DataElectrical properties were studied for borate-lead glasses and glass-ceramics doped with iron ions. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated...
-
The topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope
Open Research DataThe topography of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with confocal microscope.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Open Research DataThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Elgold intermediate: annotated raw
Open Research DataThe dataset contains a subset of texts from Elgold intermediate: raw texts with named entities marked and linked to corresponding Wikipedia articles. The texts were annotated by 31 participants during the 1.5-hour session.
-
Results of nanoindentation test to calculate residual stress in an eyelet of undercarriage drag strut after laser treatment
Open Research DataIn order to determine the residual stress in the laser-processed an eyelet of undercarriage drag strut, a nanoindentation test was performed before and after stress relief annealing. For this purpose, after the hardness test, the sample was subjected to stress relief annealing at 270 °C for 2 hours. Annealing was performed in a vacuum furnace. Hardness...
-
Destruction of AFM probes during normal operation
Open Research DataThe quality of the images obtained with the use of an atomic force microscope is determined by the state of the blade interacting with the tested material. Image artifacts can be generated by various reasons, such as oxidation, contamination or an error in blade fabrication, but also appear as a result of the repeated scanning process and inevitable...
-
Electrical conductivity of the Sr0.86Ti0.65Fe0.35O3-d pellet at different oxygen partial pressures
Open Research DataThis dataset contains results electrical conductivity measurements of dense Sr0.86Ti0.65Fe0.35O3-d (STF35) pellet. DC electrical conductivity measurements of STF35 were performed by the Van der Pauw method. Studies were performed at different oxygen partial pressures (20%, 1% and 0.1%) under humidified (~4 vol%) gas flow rate of 50 ml min -1.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Open Research DataThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
The morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses measured with AFM
Open Research DataThe morphology of as-quenched and heat treated 58(2Bi2O3-V2O5)-42SrB4O7 glasses was measured with the use of atomic force microscope.
-
Electrical conductivity of the SrTi1-xFexO3-d pellets at 20% pO2
Open Research DataThis dataset contains results electrical conductivity measurements of dense SrTi1-xFexO3-d (x=0.35, 0.50, 0.70) pellets. DC electrical conductivity measurements were performed by the Van der Pauw method between 900 °C and 200 °C. Studies were performed at 20% of oxygen partial pressure under humidified (~4 vol%) gas flow rate of 50 ml min -1.
-
Low temperature electrical conductivity of the SrFeO3-d pellet
Open Research DataThis dataset contains results of low temperature electrical conductivity measurements of dense SrFeO3-d (SFO) pellet. DC electrical conductivity measurements of SFO were performed by the Van der Pauw method between 400 °C and room temperature with 20 °C step. Studies were performed at Synthetic Air flow under humidified (~4 vol%) gas flow rate of 40...
-
Low temperature electrical conductivity of the SrTi0.65Fe0.35O3-d pellet
Open Research DataThis dataset contains results of low temperature electrical conductivity measurements of dense SrTi0.65Fe0.35O3-d (STF35) pellet. DC electrical conductivity measurements of STF35 were performed by the Van der Pauw method between 400 °C and room temperature with 20 °C step. Studies were performed at Synthetic Air flow under humidified (~4 vol%) gas...
-
Low temperature electrical conductivity of the SrTi0.30Fe0.70O3-d pellet
Open Research DataThis dataset contains results of low temperature electrical conductivity measurements of dense SrTi0.30Fe0.70O3-d (STF70) pellet. DC electrical conductivity measurements of STF70 were performed by the Van der Pauw method between 400 °C and room temperature with 20 °C step. Studies were performed at Synthetic Air flow under humidified (~4 vol%) gas...