Topography of iron-phosphate glasses doped with niobium and titanium tested by confocal microscope
Dane BadawczeThe topography of phosphate-iron glasses containing niobium and titanium were investigated with the use of confocal miscroscope. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5, 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 and 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents...
-
Linear impedance of 35P2O5-30Fe2O3-20Nb2O5-15TiO2
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and...
-
Linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2 (≥99.9%, anatase...
-
High temperature linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
High temperature linear impedance of 35P2O5-30Fe2O3-25Nb2O5-15TiO2
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%,...
-
High temperature linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear and nonlinear impedance of iron containing silicate glasses
Dane BadawczeThe linear and nonlinear impedance ofglasses doped with iron oxide were measured. Glass samples (50 SiO2-50-xPbO-xFe2O3 in mol%) were prepared by the conventional melt quenching technique. The substrates were powdered in a mortar and melted in Al2O3 crucibles. The melting was conducted in air at 1623K. The melts were poured out on plate heated up to...
-
The structure of 70(2Bi2O3-V2O5) - 30SrBO7 measured with X-ray diffraction and SEM methods
Dane BadawczeThe structure changes of 70(2Bi2O3-V2O5)-30SrB4O7 glass occurred during increase in temperature was measured by XRD and SEM.
-
Topography and microstructure of phosphate-iron glasses containing niobium and titanium
Dane BadawczeThe topography and microstructure of phosphate-iron glasses containing niobium and titanium were investigated by the means of X-ray diffraction (XRD), scanning electron microscopy (SEM). Glass samples of the composition of 35P2O5-30Fe2O3-(35-x)Nb2O5-xTiO2 where x= 0; 7.5 and 15 (in %mol) were prepared by the conventional melt quenching technique. Appropriate...
-
Linear and nonlinear impedance of alkali and iron doped silicate-lead glasses
Dane BadawczeLinear and nonlinear impedance was studied for lead-silicate glass samples doped with iron ions and alkaline oxides. The compositions of glasses were as follows: (in %mol) 50% SiO2, 25% PbO, 15% Fe2O3 and 15% one of alkaline oxides: Na2O, K2O, Li2O. All samples were prepared by the conventional melt quenching technique. The substrates were powdered...
-
The topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with SEM method
Dane BadawczeThe topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. was measured by SEM.
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-35Nb2O5 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH) and Nb2O5 (≥99.9%, PLUKA AG) were...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
The structure of strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with X-ray diffraction and SEM methods
Dane BadawczeThe structure of strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by XRD and SEM.
-
The topography of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides measured with SEM method
Dane BadawczeThe topography of strontium–borate glasses and glass-ceramics containing bismuth and vanadium oxides was measured by SEM.
-
Stability of steel plate girder with alternative web geometry
Dane BadawczeThe main aim of this study is to determine the influence of an alternative geometry of plate girder cross-section on web stability. The proposed modification of geometry consists in application of a variable web thicknesses along its height in order to reduce the number of transverse and longitudinal stiffeners along the length of the plate girder....
-
Sepulchral plate of James von Werden in St. Mary's Church in Gdańsk
Dane BadawczeThe data set concerns epigraphy. It refers to the It refers to the sepulchral plate placed in St. Mary’s Church in Gdańsk which is dedicated to James von Werden, a rich merchant, a provisor of St. Mary Church in Gdańsk, father of Mayor John von Werden, a founder of this sepulchral plate. The data set contains one general photo of the sepulchral plate,...
-
Mode shapes of a beam and plate with defects, obtained by experimental modal analysis
Dane BadawczeThe DataSet contains the experimental results of the first mode shape for a beam and a plate.
-
Sepulchral plate of Dorothy and Matthias Zimmermann in St. Mary's Church in Gdańsk
Dane BadawczeThe data set concerns epigraphy. It refers to the sepulchral plate placed in St. Mary’s Church in Gdańsk which is dedicated to Dorothy and Matthias Zimmermann, a wealthy merchant and Gdańsk mayor, trusted courtier of King Alexander Jagiellon. The data set contains one general photo of the sepulchral plate, transcription of its text in Latin, its Polish...
-
Sepulchral plate of Thomas Tympfius in St. Mary's Church in Gdańsk
Dane BadawczeThe data set concerns epigraphy. It refers to the sepulchral plate placed in St. Mary’s Church in Gdańsk which is dedicated to Thomas Tympfius, a minter who, together with his brother Andrew, rented several mints in the Kingdom of Poland, and gave his name to the timpf - the silver zloty released by the Tympfius mint. Unfortunately, as a result of...
-
Bending test results of first metatarsophalangeal joint after arthrodesis with medially or dorsally positioned locking plate and lag screw.
Dane BadawczeThe Dataset contains the results of the bending test of first metatarsophalangeal (MTP1) joint specimens after arthrodesis.
-
Displacements of bones during bending test of first metatarsophalangeal joint after arthrodesis with medially or dorsally positioned locking plate and lag screw.
Dane BadawczeThe Dataset contains the values of displacements of bone control points during the bending test of first metatarsophalangeal (MTP1) joint specimens after arthrodesis.
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - 3D fracture scan
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture SEM investigation (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 60mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 40 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 40mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 30mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 30mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 40mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 60 mm) - CMOD - force record, a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 50 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - CMOD - force record, a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 50mm), a0/W = 0.6
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
EH36 steel for shipbuilding - fracture documentation for CTOD test (plate thicnkness 50mm), a0/W = 0.5
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
LDRAW based positional renders of LEGO bricks
Dane Badawcze243 different LEGO bricks renders of size 250x250 in 5 colors in 120 viewing angles stored as JPEG images. The renders are used to train neural networks for bricks recognition. All images were generated using L3P (http://www.hassings.dk/l3/l3p.html) and POV-Ray (http://www.povray.org/) tools and were based on the 3D models from LDraw (https://www.ldraw.org/)...
-
The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...
-
The morphology of vanadate glass-ceramics containing BaTiO3 measured with the use of AFM
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by AFM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Effect of C-1748 derivatives on the biofilm formation of C. albicans ATCC 10231 cells
Dane BadawczeThe datasets contain the results of the impact of five C-1748 derivatives (IKE28 - IKE32) on the biofilm formation of Candida albicans strain ATCC 10231 cells. Photographic documentation prepared with the TECAN Spark 10M titration plate reader.
-
Effect of C-1748 derivatives on the morphological transformation of C. albicans ATCC 10231 cells
Dane BadawczeThe datasets contain the results of the impact of five C-1748 derivatives (IKE28 - IKE32) on morphological transformation of Candida albicans strain ATCC 10231 cells. Photographic documentation prepared with the TECAN Spark 10M titration plate reader.
-
The morphology of vanadate glasses containing BaTiO3
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...
-
The morphology of lead-borate glasses and nanocomposites doped with iron oxide
Dane BadawczeThe topography of iron-doped borate glasses and glass-ceramics were studied. Samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 < x < 37 in mol%) were prepared by the conventional meltquenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate...
-
The topography of Bi2VO5.5 ceramics prepared by melt-quenching technique was measured with confocal microscope
Dane BadawczeThe topography of Bi2VO5.5 ceramics prepared by melt-quenching technique was measured by confocal microscope.
-
The structure of lead-borate glasses containing nanocrystallites of iron oxides
Dane BadawczeThe structure of iron-doped glasses and glass-ceramics were studied. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated (573 K) brass plate and...