Filtry
wszystkich: 1109
wybranych: 96
-
Katalog
Filtry wybranego katalogu
Wyniki wyszukiwania dla: TIO2/SRTIO3 COMPOSITES
-
SEM analysis of the TiO2 layers deposited on a FTO substrates
Dane BadawczeTitanium dioxide layers were deposited on a FTO conducting glass by sol-gel method. For sol gel synthesis butoxy titanium and ethanol were used as a reagents. Samples were sintered in a furnace at temperature of 600 deg. SEM measurements were performed by FEI Quanta FEG250 microscope. SEM images of a cross-section of samples exhibit a porous structures...
-
Electrochemical studies of poly(lactic acid)-carbon black-nanodiamond composites
Dane BadawczeThis dataset contains electrochemical investigation on electrodes 3D printed using a new composite composed of poly-lactic acid (PLA), carbon black (CB) and nanodiamond fillers. Two types of nanodiamonds were studied: detonation nanodiamonds (DND) and boron-doped carbon nanowalls (BCNW). The presented results contain:1. electrochemical characterisation...
-
The influence of the type of composition of PVA-chitosan blends on stability at elevated temperature
Dane BadawczeThe dataset shows the results of a visual evaluation of chitosan and polyvinyl alcohol composites. The composites were prepared by combining chitosan water solutions, dissolved in selected acids, and polyvinyl alcohol solution, freeze drying, and heating at 150°C dry composites. The results confirm that the chitosan / PVA composites, in which the first...
-
Rheology studies of multiple times processed poly(lactic acid)-carbon black composites
Dane BadawczeThis dataset contains MFR/MVR (melt flow rate) rheology studies of commercially available ProtoPasta 3D printable filament, composed of poly-lactic acid (PLA) and conductive carbon black (CB) filler. The study aims to observe structural differences and applied properties changes under multiple reprocessing of the composite material at different temperatures...
-
Topography studies of multiple times processed poly(lactic acid)-carbon black composites
Dane BadawczeThis dataset contains topography studies with scanning electron microscope of commercially available ProtoPasta 3D printable filament, composed of poly-lactic acid (PLA) and conductive carbon black (CB) filler. The aim of the study is to observe structural differences and applied properties changes under multiple reprocessing of the composite material...
-
Electrochemical analyses of multiple times processed poly(lactic acid)-carbon black composites
Dane BadawczeThis dataset contains cyclic voltammetry studies of commercially available ProtoPasta 3D printable filament, composed of poly-lactic acid (PLA) and conductive carbon black (CB) filler. The aim of the study is to observe structural differences and applied properties changes under multiple reprocessing of the composite material at different temperatures...
-
Thermal analyses of multiple times processed poly(lactic acid)-carbon black composites
Dane BadawczeThis dataset contains thermal analyses (TGA, DTG, DSC) studies of commercially available ProtoPasta 3D printable filament, composed of poly-lactic acid (PLA) and conductive carbon black (CB) filler. The aim of the study is to observe structural differences and applied properties changes under multiple reprocessing of the composite material at different...
-
Physicochemical studies (Raman) of multiple times processed poly(lactic acid)-carbon black composites
Dane BadawczeThis dataset contains Raman spectroscopy studies of commercially available ProtoPasta 3D printable filament, composed of poly-lactic acid (PLA) and conductive carbon black (CB) filler. The aim of the study is to observe structural differences and applied properties changes under multiple reprocessing of the composite material at different temperatures...
-
Broadband dielectric spectroscopy studies of multiple times processed poly(lactic acid)-carbon black composites
Dane BadawczeThis dataset contains broadband dielectric spectroscopy studies of commercially available ProtoPasta 3D printable filament, composed of poly-lactic acid (PLA) and conductive carbon black (CB) filler. The aim of the study is to observe structural differences and applied properties changes under multiple reprocessing of the composite material at different...
-
X-ray diffraction spectra of modification of TiO2 nanotubes by graphene - strontium and cobalt molybdate perovskite
Dane BadawczeData show XRD results for strontium and cobalt molybdate-modified nanotubes that were also decorated with graphene oxide. The crystalline phases were characterized by X-ray diffractometer (Philips X”Pert with detector X’Celerator Scientific).
-
Photocatalytic degradation of acetaldehyde in high temperature reaction chamber
Dane BadawczeThis dataset contains chromatograms recorded during the decomposition of acetaldehyde in a high-temperature reaction chamber under UV irradiation using TiO2 (titanium dioxide) as photocatalysts. It includes data on the influence of flow rate, TiO2 (titanium dioxide) filling the entire reactor, a thin layer of TiO2 (titanium dioxide) supported on KBr...
-
Hydrogenation process ofTiO2/BiVO4/PEDOT:PSS observed by XPS method
Dane BadawczeTitania nanotubes synthesis was based on a two-stage anodization process at water/ethylene glycol (5%/95%) electrolyte containing 0.27 M NH4F and 1 M H3PO4 described previously. Anodization process was performed in two-electrode cell compartment using platinum mesh as a cathode. The distance between electrodes was about 2 cm. The anodization voltage...
-
X-ray diffraction of ZnIn2S4 layers on TiO2NT and FTO annealed at different temperatures
Dane BadawczeData show XRD results for ZnIn2S4 layers deposited using hydrothermal method on FTO glass and TiO2 nanotubes. The layers were annealed in air atmosphere at 300, 400 and 500 oC.
-
Thermal stability analysis of poly(lactic acid)-carbon black-nanodiamond composite
Dane BadawczeThis dataset contains thermal stability tests carried out on new 3D printing-dedicated composites with poly-lactic acid (PLA), carbon black (CB) and nanodiamond fillers. Two types of nanodiamonds were studied: detonation nanodiamonds (DND) and boron-doped carbon nanowalls (BCNW). The investigated techniques include: thermogravimetric analysis (TGA)...
-
Ethylene photocatalytic decomposition in high temperature reaction chamber
Dane BadawczeData contain data logs of measurements performed on High Temperature Chamber "The Praying Mantis" coupled with SRI 8010 gas chromatograph. Measurement was performed for TiO2 irradiated by UV and under flowing of ethylene gas diluted in air and with the use of elevated temperature.
-
XRD for molybdenum sulfide modified with nickel or platinum nanoparticles
Dane BadawczeThe presented data showcases the results of XRD analysis conducted on molybdenum sulfide modified with nickel or platinum nanoparticles . The MoS2 was prepared on the TiO2 nanotube substrates via a facile hydrothermal method, followed by the deposition by magnetron sputtering of Ni or Pt nanoparticles on the MoS2 surface. Structural characterization...
-
New 3D printable filaments with nanodiamonds, physicochemical additives characteristics and electrochemical activity
Dane BadawczeThis dataset contains the physicochemical analyses (XRD, Raman spectroscopy, BET analyses) and electrochemical analyses (CV, EIS) for a new 3D-printable composite has been developed dedicated to electroanalytical applications. Two types of diamondised nanocarbons - detonation nanodiamonds (DNDs) and boron-doped carbon nanowalls (BCNWs) - were added...
-
Photocatalytic ethylene decomposition with the use of fluidized bed photoreactor
Dane BadawczeData contain exported raw data recorded during decomposition of ethylene during utilization of fluidized bed photoreactor equipped with either UV-LEDs or fluorescent UV lamps as well as in either humid or dry conditions. In separate folder, the photographs of the photocatalytic system were included. As photocatalytic material, polystyrene spheres coated...
-
The morphology of vanadate glasses containing BaTiO3 measured with the use of AFM
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured with the use of AFM method. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured...
-
The morphology of vanadate glass-ceramics containing BaTiO3 measured with the use of AFM
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by AFM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
The morphology of vanadate glasses containing BaTiO3
Dane BadawczeThe morphology of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573 K) brass...
-
The structure of vanadate glass-ceramics containing BaTiO3 measured with X-ray diffraction method
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by XRD. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Linear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
The morphology of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe morphology of vanadate glass-ceramic doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Ni-based compounds in multiwalled graphitic shell for electrocatalytic oxygen evolution reactions
Dane BadawczeThis study investigates Ni-based compounds (Ni, NiO, Ni3C) coated with a graphitic shell as electrocatalysts for the oxygen evolution reaction (OER). Electron paramagnetic resonance (EPR) and X-ray diffraction (XRD) are employed to identify the presence and contribution of Nickel ions (Ni0, Ni2+, Ni3+) and determine the phase composition. Electrochemical...
-
The structure of vanadate glasses containing BaTiO3.
Dane BadawczeThe structure of vanadate glasses doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Linear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glass-ceramics containing BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
XPS study of the YST ceramics
Dane BadawczeYttrium-doped strontium titanate was prepared via conventional solid-state reaction method from Y2O3 (Sigma Aldrich, 99,9%), TiO2 (Sigma Aldrich, 99%) and SrCO3 (Sigma Aldrich,98%). For comparision, two other techniques were used for synthesis: Pechini and wet methods. Both kind of samples were measured, after and before reduction process (in a hydrogen)....
-
The structure of vanadate glass-ceramics containing BaTiO3.
Dane BadawczeThe structure of vanadate glass-ceramics doped with BaTiO3 was measured by SEM technique. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on...
-
Topography of iron-phosphate glasses doped with niobium and titanium tested by confocal microscope
Dane BadawczeThe topography of phosphate-iron glasses containing niobium and titanium were investigated with the use of confocal miscroscope. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5, 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 and 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents...
-
The structure of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with X-ray diffraction method
Dane BadawczeThe structure of strontium–borate glasses and glass-ceramics containing Bi2VO5.5 nanocrystallites was measured by XRD.
-
Thermal properties of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with DSC method
Dane BadawczeThermal properties of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. was measured by DSC.
-
Linear impedance of 35P2O5-30Fe2O3-20Nb2O5-15TiO2
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
Linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and...
-
Linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Dane BadawczeThe electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2 (≥99.9%, anatase...
-
Reduction of the strontium titanate doped by Ytrium ceramics observed by X-ray photoemission spectroscopy method
Dane BadawczeYtrium-doped strontium titanate (YSTF) ceramics materials were manufactured by three various methods: 1) standard solid-state reaction method from Y2O3 (Sigma Aldrich, 99,9%), TiO2 (Sigma Aldrich, 99%) and SrCO3 (Sigma Aldrich,98%), 2) Pechini method, 3) wet method.
-
Thermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with DSC
Dane BadawczeThermal properties of ceramic Bi2VO5.5 and strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by DSC.
-
High temperature linear impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...
-
High temperature linear impedance of 35P2O5-30Fe2O3-25Nb2O5-15TiO2
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium and titanium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-20Nb2O5-15TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%,...
-
High temperature linear impedance of 35P2O5-30Fe2O3-35Nb2O5
Dane BadawczeThe high temperature electrical properties of phosphate-iron glasses containing niobium were investigated. Glass samples of the composition of 35P2O5-30Fe2O3-35Nb2O5 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG) and TiO2...
-
The topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. measured with SEM method
Dane BadawczeThe topography of strontium–borate glasses and glass-ceramics containing nanocrystallites of Bi2VO5.5. was measured by SEM.
-
The structure of strontium–borate glass-ceramics containing crystalites of Bi2VO5.5. measured with X-ray diffraction and SEM methods
Dane BadawczeThe structure of strontium–borate glass-ceramics containing Bi2VO5.5 crystallites was measured by XRD and SEM.
-
Nonlinear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Topography and microstructure of phosphate-iron glasses containing niobium and titanium
Dane BadawczeThe topography and microstructure of phosphate-iron glasses containing niobium and titanium were investigated by the means of X-ray diffraction (XRD), scanning electron microscopy (SEM). Glass samples of the composition of 35P2O5-30Fe2O3-(35-x)Nb2O5-xTiO2 where x= 0; 7.5 and 15 (in %mol) were prepared by the conventional melt quenching technique. Appropriate...
-
Nonlinear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Nonlinear high temperature impedance of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 glass
Dane BadawczeThe nonlinear high temperature impedance of iron- phosphate glasses doped with niobium oxide was measured. Glass samples of the composition of 35P2O5-30Fe2O3-27.5Nb2O5-7.5TiO2 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents ((NH4)2HPO4 (≥99.9%, POCH), Fe2O3 (≥99.9%, POCH), Nb2O5 (≥99.9%, PLUKA AG)...