Wyniki wyszukiwania dla: CONDUCTIVITY
-
Methane emissions from mangrove soils in hydrologically disturbed and reference mangrove tidal creeks in southwest Florida
PublikacjaStudies have suggested that some mangrove soils might contribute to wetland methane (CH4) production and emissions, especially when the mangroves are disturbed. CH4 emissions were measured seasonally from nine locations on two mangrove creeks on Naples Bay in southwest Florida, USA. One of the tidal creeks has been impacted in the past few decades with alteration of upstream watersheds and freshwater inflows; the other creek was...
-
CTD Gdańsk Deep_2001_2005
Dane BadawczeDataset includes measurements of conductivity (mS cm-1), temperature (°C), sound speed (m s-1) and salinity (PSU) made with the probe Falmouth Scientific Inc. The research was carried out in 2001 (at the turn of May and June), 2003 (beginning of May), 2005 (end of April) and in 2002 and 2004 (at the turn of September and October). In 2002, only temperature...
-
Nutrients, oxygen and suspended matter - Gdansk Deep (2001-2005)
Dane BadawczeThe results show short-term changes in the concentration of nutrients (nitrates, nitrites, ammonium ions, phosphates and total forms of nitrogen and phosphorus), dissolved oxygen and suspended particulate matter - SPM and its main components (organic carbon - POC, nitrogen - PON, phosphorus - TPP) in the water column of the Gdańsk Deep (Gdańsk Bay).
-
Residence time distribution in rapid multiphase reactors
PublikacjaResidence time distribution (RTD) provides information about average hydraulic residence time and the distribution of material in the reactor. A method for determining RTD for reactors with very short hydraulic residence times is deconvolution based on extraction of real RTD by the analysis of a non-ideal input signal. The mean residence time and dispersion were determined for the spinning fluids reactor (SFR). For the first time...
-
Silver(I) complexes with nitrile ligands: New materials with versatile applications
PublikacjaIn the present study, the structure, thermal stability, conductive properties, and antimicrobial activity of silver(I) complexes with nitrile ligands were investigated. For the construction of the materials, 2-cyanopyridine (2-cpy), 4-cyanopyridine (4-cpy), 1,2-dicyanobenzene (1,2-dcb), and 1,3-dicyanobenzene (1,3-dcb) were used in addition to the silver nitrite and nitrate. Four new compounds were isolated and structurally characterized:...
-
Fabrication of wormhole-like YSZ and Ni-YSZ by the novel soft-hard template CTAB/NaCl-assisted route. Suppressing Ni coalescence in SOFC
PublikacjaA novel one-pot synthesis route leading to the formation of a wormhole-like structure was developed for the successful fabrication of porous YSZ and Ni-YSZ systems. This method involved co-precipitation in the presence of the micelle-forming agents CTAB/Pluronic P123 and crystallising NaCl. The obtained skeletons were mechanically stable and presented almost 50% uniform, open porosity without using any additional pore-formers....
-
Sounding rocket temperature and heat transfer data
Dane BadawczeThis dataset contains temperature and heat transfer data measured during REXUS 25 sounding rocket HEDGEHOG Experiment launched from Esrange Space Centre, Kiruna, Sweden. For experiment details, please see:
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Linear impedance of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 10Na2O–60P2O5–30CaO glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 10Na2O–60P2O5–30CaO glass was measured by impedance spectroscopy method.
-
Linear impedance of 40Na2O-20CaO-40P2O5 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 40Na2O-20CaO-40P2O5 glass was measured by impedance spectroscopy method.
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 1SiO2–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 1SiO2–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 glass-ceramic measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
AlP compound and P-doping for promotion of electrocatalytic activity of N-doped carbon derived from metal-organic framework
PublikacjaWater splitting plays a key role in future fuels, where two processes occur - the hydrogen evolution reaction (HER) and the oxygen evolution reaction (OER). Nitrogen-doped carbon derived from...
-
Aiswarya Manohar
OsobyI joined as a PhD student in Gdansk tech university of Technology in 2022. In my scientific work, I am primarily focusing on studies related to 3D printing, laser induced graphene, electrochemical sensors and biosensors as well as micro arc oxidation, corrosion, and degradation with emphasis on impedance spectroscopy studies of electrode processes. I am specializing in Materials and surface modifications and characterization. ...