Seismic Response Analysis of Knee-Braced Steel Frames Using Ni-Ti Shape Memory Alloys (SMAs)
PublikacjaShape Memory Alloys (SMAs) are known as active materials that can be widely used for structural purposes due to their flag-shape behavior under loading and reloading. Their unique characteristics provided a potential solution for civil engi-neers especially to model buildings with the capability of dissipating seismic en-ergy. In this study, the main purpose is to explore the seismic behavior of Knee-Braced Frames (KBFs) and...
-
Study on Microstructure and Mechanical Properties of Laser Welded Dissimilar Joint of P91 Steel and INCOLOY 800HT Nickel Alloy
PublikacjaThis investigation attempts to explore the weld characteristics of a laser welded dissimilar joint of ferritic/martensitic 9Cr-1Mo-V-Nb (P91) steel and Incoloy 800HT austenitic nickel alloy. This dissimilar joint is essential in power generating nuclear and thermal plants operating at 600–650 °C. In such critical operating conditions, it is essential for a dissimilar joint to preserve its characteristics and be free from any kind...
-
Study of a Multicriterion Decision-Making Approach to the MQL Turning of AISI 304 Steel Using Hybrid Nanocutting Fluid
PublikacjaThe enormous use of cutting fluid in machining leads to an increase in machining costs, along with different health hazards. Cutting fluid can be used efficiently using the MQL (minimum quantity lubrication) method, which aids in improving the machining performance. This paper contains multiple responses, namely, force, surface roughness, and temperature, so there arises a need for a multicriteria optimization technique. Therefore,...
-
Fracture Surface Behavior of 34CrNiMo6 High-Strength Steel Bars with Blind Holes under Bending-Torsion Fatigue
PublikacjaThe present study evaluates the fracture surface response of fatigued 34CrNiMo6 steel bars with transverse blind holes subjected to bending with torsion loading. The analysis of the geometric product specification was performed by means of height parameters Sx, functional volume parameters Vx, and fractal dimension Df. Surface topography measurements were carried out using an optical profilometer with focus variation technology....
-
Efektywność skrępowania betonu w grubościennych słupach typu Concrete-Filled Steel Tube o przekroju kołowym
PublikacjaW słupach typu CFST w stanie granicznym dochodzi do zwiększenia wytrzymałości betonu rdzenia na skutek jego skrępowania. Zaistnienie tego zjawiska zależy od wielu czynników. Jednym z najważniejszych z nich jest sztywność obwodowa płaszcza stalowego. Jej wpływ na efektywność wzrostu wytrzymałości betonu rdzenia przebadano eksperymentalnie na grupie 48 grubościennych słupów CFST. Wykazano, że nadmierne zwiększanie grubości płaszcza...
-
On the Application of Magnetoacoustic Emission for a Nondestructive Assessment of the Post Welding Heat Treatment of High Chromium Steel Weld Seams
PublikacjaThe paper analyses the possibility of post weld heat treatment (PWHT) quality assessment with the help of magnetoacoustic emission (MAE) signal measurements. Two welded superheater tubes, made of high chromium VM12 steel, were analysed—as welded and heat treated one. The analysed sample in the as welded state exhibited significantly higher hardness, accompanied by a big difference in the MAE signal intensity (of order of about...
-
Mechanical and structural behavior of high-strength low-alloy steel pad welded by underwater wet welding conditions
PublikacjaThe aim of the paper was to determine the metallurgical and mechanical behaviors of a high-strength low-alloy (HSLA) steel pad-welded specimen used in the structures of industrial and naval parts. Then to predict the metallurgical consequences (nature of the phases present) and the mechanical properties (hardness and impact strength) of the pad-welded steel obtained by underwater wet welding with different heat input values. The...
-
The Impact Of The Selected Parameters Of Fdm Manufacturing Technology On Tribological Performance Of Abs–Steel Pair Under Dry Friction
PublikacjaThe paper presents the result of tribological test of ABS and steel samples sliding under dry friction. Polymeric samples were manufactured of ABS material using FDM technology. Testing was carried out in unidirectional sliding in a ring-on-flat contact in a PT-3 tribometer. The scope of tested parameters included volumetric and mass wear, the friction coefficient, and polymeric specimen temperature. Polymeric specimens used in...
-
Application of linear buckling sensitivity analysis to economic design of cylindrical steel silos composed of corrugated sheets and columns
PublikacjaThe paper deals with global stability of steel cylindrical silos composed of corrugated walls and vertical columns with loads imposed by a bulk solid following Eurocode 1. The optimum silo design with respect to the steel weight was based on a sensitivity analysis method. The changes of silo column profiles at each design step were performed by means of influence lines for the buckling load factor due to the unit column bending...
-
Experimental study and comparison with predictive methods for flow boiling heat transfer coefficient of HFE7000
PublikacjaThis article describes an experimental study of flow boiling of HFE7000 inside a smooth vertical channel. The investigation has been carried out in a circular stainless-steel tube with an inner diameter of 2.3 mm. The data have been collected for the applied heat fluxes q ranging from 61 to 205 kW/m2, the mass flux G ranging from 214 to 1006 kg/(m2 s), the saturation temperature Tsat ranging from 30 to 54 °C and the full range...
-
Study of the Layer-Type BST Thin Film with X-ray Diffraction and X-ray Photoelectron Spectroscopy
PublikacjaIn the present paper, results of X-ray photoelectron studies of electroceramic thin films of barium strontium titanate, Ba1xSrxTiO3 (BST), composition deposited on stainless-steel substrates are presented. The thin films were prepared by the sol-gel method. A spin-coating deposition of BST layers with different chemical compositions was utilized so the layer-type structure of (0-2) connectivity was formed. After the deposition,...
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in ambient temperature
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in 0°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – tensile test in -20°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
EH36 steel for shipbuilding (plate thicnkness 30 mm) - 3D fracture scan
Dane BadawczeThe basic method of ductility designation of structural steels is the Charpy impact test. The test consists of a single strike of the specimen using a Charpy pendulum. Its result is the value of work necessary to break a specimen at a test temperature. Despite its many advantages, such as its short implementation time and low costs, it has its disadvantages,...
-
RMS-based damage identification in adhesive joint between concrete beam and steel plate using ultrasonic guided waves
PublikacjaAdhesive joints have numerous applications in many branches of industry, such as civil engineering, automotive, aerospace and shipbuilding. As with most structural elements, adhesive joints can experience any damage mechanism, which induces the need for diagnostic testing. Ultrasonic waves are widely used for non-destructive inspection of many structures and their elements, including adhesive joints. Guided wave propagation method...
-
The stress and strain distribution in X10CrMoVNb9-1 power engineering steel after long time degradation studied by the ESPI system
Publikacja -
Fatigue damage development in 10CrMo9-10 steel for power plant pipes in as-received state and after 280,000 h of exploitation
Publikacja -
Monitoring of fatigue damage development in as-received and exploited 10CrMo9-10 power engineering steel supported by Digital Image Correlation
Publikacja -
The analysis of strain response for as-received and exploited 10H2M power engineering steel subjected to low cycle fatigue in plastic regime
Publikacja -
Experimental Evaluation of ND: YAG Laser Parameters and Sample Preparation Methods for Texturing Thin AISI 316L Steel Samples
Publikacja -
Effect of non-zero mean stress bending-torsion fatigue on fracture surface parameters of 34CrNiMo6 steel notched bars
Publikacja -
A fractographic study exploring the fracture surface topography of S355J2 steel after pseudo-random bending-torsion fatigue tests
Publikacja -
Wpływ starzenia stali budowlanej na jej właściwości mechaniczne. The effect of structural steel aging on its mechanical properties
PublikacjaPrzedstawiono wyniki badań właściwości mechanicznych i struktury trzech elementów stalowej konstrukcji budowlanej po długotrwałej eksploatacji.
-
Damage imaging algorithm for non-destructive inspection of CFRP/steel adhesive joints based on ultrasonic guided wave propagation
PublikacjaThe paper concerns assessing the quality of the adhesive connection between a steel plate and the reinforcing CFRP laminate. A three-stage algorithm for non-destructive damage imaging was developed. As the first step, an initial study involving dispersion curves of joint components was executed to determine the material parameters and the appropriate excitation frequency. During the second step, damage identification in three-layer...
-
Strain energy density and entire fracture surface parameters relationship for LCF life prediction of additively manufactured 18Ni300 steel
PublikacjaIn this study, the connection between total strain energy density and fracture surface topography is investigated in additively manufactured maraging steel exposed to low-cycle fatigue loading. The specimens were fabricated using laser beam powder bed fusion (LB-PBF) and examined under fully-reversed strain-controlled setup at strain amplitudes scale from 0.3% to 1.0%. The post-mortem fracture surfaces were explored using a non-contact...
-
Fracture surface topography measurements analysis of low-alloyed corrosion resistant steel after bending-torsion fatigue tests
PublikacjaIn this paper, an assessment of a topography measurement method for fracture surfaces of 10HNAP steel after bending-torsion fatigue tests was performed. Surface roughness was measured by using a non-contact Focus Variation Microscopy (FVM) technique in which the non-measured points (NMPs) and outliers (spikes) were removed by the application of general methods. The results revealed, that the optical measurement method introduced...
-
Low temperature deposition of dense MnCo 2 O 4 protective coatings for steel interconnects of solid oxide cells
PublikacjaIn this work manganese cobalt spinel (MnCo2O4) coatings were deposited on steel substrates by spray pyrolysis at 390 °C. This is at much lower temperatures than previously reported (typically in excess of 900 °C). It was possible to produce coatings with well controlled thickness (2-5-10 μm). The as-deposited coatings were evaluated for their microstructural changes and electrical conductivity up to 800 °C. Results confirm the...
-
Study of microstress state of P91 steel using complementary mechanical Barkhausen, magnetoacoustic emission, and X-ray diffraction techniques
PublikacjaThe paper deals with assessment of microstress state of martensite P91 steel using three complementary techniques: mechanical Barkhausen emission, magnetoacoustic emission (MAE), and X-ray diffraction (XRD) profile analysis. Magnetic coercivity Hc and microstructure were investigated with inductive magnetometry and magnetic force microscopy (MFM), respectively. Internal stress level of P91 steel was modified by heat treatment....
-
EVALUATING THE INFLUENCE OF BENDING STRESS ON A 1H18N9 STEEL SHAFT WEAR PROCESS IN A WATER LUBRICATED SLIDING BEARING WITH A RUBBER BUSHING
PublikacjaThe issue of excessive wear of shaft journals co-working with a rubber bearing has been unexplained so far. Premature and sometimes very intensive wear of ship sliding bearings in water conditions is the reason for carry out very expensive and more frequent than expected repairs. The authors (E. Piątkowska, W. Litwin) made an attempt to find a case that influences the value of this wear described in the paper “Attempt at Evaluating...
-
The abrasive wear resistance of coatings manufactured on high-strength low-alloy (HSLA) offshore steel in wet welding conditions
PublikacjaSome marine and offshore structure elements exploited in the water cannot be brought to the surface of the water as this will generate high costs, and for this reason, they require in-situ repairs. One of the repair techniques used in underwater pad welding conditions is a wet welding method. This paper presents an investigation of the abrasive wear resistance of coatings made in wet welding conditions with the use of two grades...
-
Experimental Evaluation of ND: YAG Laser Parameters and Sample Preparation Methods for Texturing Thin AISI 316L Steel Samples
PublikacjaIn mechanical and material engineering, the effect of laser texturing depends on many factors besides device specification, primarily the properties of the materials being processed, and, secondly, the preparation of the sample. Laser texturing of thin (<5 mm) samples is mostly performed utilizing short-pulse lasers, but depending on the power of the laser beam, the process can also be performed by using continuous operation lasers....
-
A brief note on entire fracture surface topography parameters for 18Ni300 maraging steel produced by LB-PBF after LCF
PublikacjaThe concept of entire fracture surface investigation is helpful in explaining fatigue phenomena. In this paper, this method has been applied for 18Ni300 maraging steel using a 3D measurement system. Before post-mortem analysis, the specimens produced by laser beam powder bed fusion (LB-PBF) were tested under low-cycle fatigue (LCF) for eight strain amplitudes in the interval 0.3% to 1.0%. The attention was placed on the relationship...
-
Stability of cylindrical steel silos composed of corrugated sheets and columns based on FE analyses versus Eurocode 3 approach
PublikacjaComprehensive static and dynamic 3D stability finite element analyses of a cylindrical steel silo composed of corrugated sheets and open thin-walled vertical stiffener profiles were carried out by taking the geometric and material non-linearity into account. The silowas subjected to axisymmetric and non-axisymmetric loads imposed by a bulk solid following Eurocode 1. Theoretical and measured initial geometric imperfections were...
-
Ireneusz Kreja dr hab. inż.
OsobyAbsolwent klasy matematycznej I Liceum Ogólnokształcącego w Gdańsku im. Mikołaja Kopernika (1974). Absolwent Wydziału Budownictwa Lądowego Politechniki Gdańskiej (1979). Od 1979 pracuje na PG. W 1989 uzyskał doktorat (z wyróżnieniem), na Wydziale Budownictwa Lądowego, a w 2008 habilitował się (również z wyróżnieniem) na Wydziale Inżynierii Lądowej i Środowiska PG. Od 2011 jest profesorem PG. Na Politechnice Gdańskiej pełnił funkcje:...
-
Degradacja stali 9CR-1Mo pod wpływem podwyższonej temperatury. Degradation of 9Cr-1Mo steel under the influence of elevated temperature
PublikacjaBadano charakterystyczne cechy degradacji mikrostruktury i właściwości mechanicznych stali 9Cr-1Mo gat. P9 ASTM SA-335 po eksploatacji w piecu rafineryjnym w temperaturze 390-500 stopni C. Wykazano, że po 30 000 godzin wydłużenie obniżyło się o około 30%. Przyczyną spadku wydłużenia były zmiany mikrostruktury związane z umocnieniem osnowy metalicznej przez chrom oraz wynikające z kruchości odpuszczania stali. Większy spadek wydłużenia...
-
High-Performance Face Milling of 42CrMo4 Steel: Influence of Entering Angle on the Measured Surface Roughness, Cutting Force and Vibration Amplitude
Publikacja -
Abrasive Wear, Scuffing and Rolling Contact Fatigue of DLC-Coated 18CrNiMo7-6 Steel Lubricated by a Pure and Contaminated Gear Oil
Publikacja -
Effects of extreme pressure and anti-wear additives on surface topography and tool wear during MQCL turning of AISI 1045 steel
Publikacja -
Machine learning-based prediction of seismic limit-state capacity of steel moment-resisting frames considering soil-structure interaction
PublikacjaRegarding the unpredictable and complex nature of seismic excitations, there is a need for vulnerability assessment of newly constructed or existing structures. Predicting the seismic limit-state capacity of steel Moment-Resisting Frames (MRFs) can help designers to have a preliminary estimation and improve their views about the seismic performance of the designed structure. This study improved data-driven decision techniques in...
-
Monitoring Steel Bolted Joints during a Monotonic Tensile Test Using Linear and Nonlinear Lamb Wave Methods: A Feasibility Study
PublikacjaThe structural integrity of steel bolted joints may be compromised due to excessive loading. Therefore, condition assessment and the detection of potential defects before they cause a failure have become a major issue. The paper is focused on the condition monitoring of a bolted lap joint subjected to progressive degradation in a tensile test. The inspection used Lamb waves propagated through the overlap area. Wave propagation...
-
Results of acoustic emission tests of corrosion protection degree of ship steel tanks covered by means of protective coatings (Phase I)
PublikacjaThis paper presents methods and results of the 1st series of tests of acoustic emission (AE) signals, aimed at assessing degree of corrosion protection of a tank made of hull structural steel, protected by means of a protective coating combined from polyurethane layer and concrete filler. The tests were carried outin compliance with a method specially elaborated for application to the work in question. In the method were used requirements...
-
Effect of Some Sulphur Additives on The Degradation of 9Cr-1Mo Steel After Its 10 Years Service in The CCR Platforming Unit
PublikacjaThe work shows the results of the tests of 9Cr-1Mo steel, which was for 10 years operated in the CCR platforming unit in Group Lotos SA in Gdańsk, and then in the laboratory was sulphidised during 166 h at a temperature of 600 °C. Sulphidation was performed in a mixture of H2-H2S gases at the vapour pressure of sulphur 4.1·10-14 atm, so the order of magnitude of vapour pressure was less than that of the dissociation pressure of...
-
Badania eksperymentalne modelu zbiornika stalowego na stole sejsmicznym = Experimental study on steel tank model using shaking table
PublikacjaCylindrical steel tanks are very popular structures used for storage of products of chemical and petroleum industries. Their safety and reliability is really crucial because any failure may have serious consequences. Earthquakes are the most dangerous and also the most unpredictable dynamic loads acting on such structures. On the other hand, rockburst-induced ground motions are usually considered to be less severe due to lower...
-
Experimental Study on Steel Tank Model Using Shaking Table/ Badania Eksperymentalne Modelu Zbiornika Stalowego Na Stole Sejsmicznym
PublikacjaStalowe zbiorniki walcowe są bardzo popularnymi konstrukcjami używanymi do magazynowania produktów przemysłu chemicznego i naftowego. Ich bezpieczeństwo i niezawodność są kluczowe, ponieważ każde uszkodzenie może nieść za sobą bardzo poważne konsekwencje. Trzęsienia ziemi są najbardziej niebezpiecznymi, a zarazem najbardziej nieprzewidywalnymi obciążeniami dynamicznymi, które mogą oddziaływać na tego typu konstrukcje. Z drugiej...
-
CTOD designation for WM and HAZ in butt joint made from S460 ML steel, Expertise No. WOiO/II/82/2015
PublikacjaTypical (normative) testing of materials and/or welded joints do not answer on all questions about material or welded joint properties. In ship building and off-shore sectors, many strucures requires materials and joint with higher than typical fatigue resistance. Imact tests, which are carried out during welding technology qualification, gives answer about ductility, CTOD tests results about material or welded joint ability to...
-
Effect of Pin Shape on Thermal History of Aluminum-Steel Friction Stir Welded Joint: Computational Fluid Dynamic Modeling and Validation
PublikacjaThis article studied the effects of pin angle on heat generation and temperature distribution during friction stir welding (FSW) of AA1100 aluminum alloy and St-14 low carbon steel. A validated computational fluid dynamics (CFD) model was implemented to simulate the FSW process. Scanning electron microscopy (SEM) was employed in order to investigate internal materials’ flow. Simulation results revealed that the mechanical work...
-
Enhancing seismic performance of steel buildings having semi-rigid connection with infill masonry walls considering soil type effects
PublikacjaUnpreventable constructional defects are the main issues in the case of steel Moment-Resisting Frames (MRFs) that mostly occur in the rigidities of beam-to-column connections. The present article aims to investigate the effects of different rigidities of structures and to propose Infill Masonry Walls (IMWs) as retrofitting strategy for the steel damaged buildings. A fault or failure to meet a certain consideration of the soil type...
-
Mechanical properties of VL E27 steel for shipbuilding – fracture toughness test in 0°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....
-
Mechanical properties of VL E27 steel for shipbuilding – fracture toughness test in 20°C
Dane BadawczeOne of the basic divisions of steels used for ship hulls and ocean engineering structures is the division into: normal strength steels, high strength steels and extra high strength steels. The belonging to the group is determined by the mechanical properties of the steel, such as: yield point, ultimate strength and plastic elongation after fracture....