Filtry
wszystkich: 4331
wybranych: 316
-
Katalog
- Publikacje 3167 wyników po odfiltrowaniu
- Czasopisma 91 wyników po odfiltrowaniu
- Konferencje 2 wyników po odfiltrowaniu
- Osoby 87 wyników po odfiltrowaniu
- Wynalazki 19 wyników po odfiltrowaniu
- Projekty 20 wyników po odfiltrowaniu
- Laboratoria 2 wyników po odfiltrowaniu
- Zespoły Badawcze 4 wyników po odfiltrowaniu
- Kursy Online 104 wyników po odfiltrowaniu
- Wydarzenia 58 wyników po odfiltrowaniu
- Dane Badawcze 777 wyników po odfiltrowaniu
Filtry wybranego katalogu
Wyniki wyszukiwania dla: ROZTWORY SOLI
-
Study of the influence of medium composition on motility and aggregation of recombinant Escherichia coli strain AAEC191A/pCC90 Dra D-mut-M9 + 0.5% cassaminic acids, M9 + 0.5% cassaminic acids + 0.2% glucose, M9 + 0.5% cassaminic acids + 0.5% glucose
Dane BadawczeMicrobial motility is a fundamental aspect of many microbial life cycles and is a key survival mechanism that enables microorganisms to navigate diverse and dynamic environmental conditions. This phenomenon becomes particularly important in response to changes in stimuli in time and space. The following experiment aimed to investigate how the composition...
-
Study of the influence of medium composition on motility and aggregation of recombinant Escherichia coli strain BL21(DE3)/pCC90 D54-STOP-M9 + 0.5% cassaminic acids, M9 + 0.5% cassaminic acids + 0.2% glucose, M9 + 0.5% cassaminic acids + 0.5% glucose
Dane BadawczeMicrobial motility is a fundamental aspect of many microbial life cycles and is a key survival mechanism that enables microorganisms to navigate diverse and dynamic environmental conditions. This phenomenon becomes particularly important in response to changes in stimuli in time and space. The following experiment aimed to investigate how the composition...
-
Study of the influence of medium composition on motility and aggregation of recombinant Escherichia coli strain BL21(DE3)/pCC90 Dra D-mut-M9 + 0.5% cassaminic acids, M9 + 0.5% cassaminic acids + 0.2% glucose, M9 + 0.5% cassaminic acids + 0.5% glucose
Dane BadawczeMicrobial motility is a fundamental aspect of many microbial life cycles and is a key survival mechanism that enables microorganisms to navigate diverse and dynamic environmental conditions. This phenomenon becomes particularly important in response to changes in stimuli in time and space. The following experiment aimed to investigate how the composition...
-
Genetic and Proteomic data
Dane BadawczeGenetic and Proteomic data (shotgun proteomics) for Uroseptic and UTI E. coli strains.
-
Metabolomics
Dane BadawczeWiff and Wiff2 files of untargeted metabolomics for E. coli strains (4 different experiments)
-
The AFM micrographs of vanadium oxides thin films obtained at 800°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on a silicon substrate and vanadium thin films were obtained by annealing as-prepared films at...
-
The AFM micrographs of vanadium oxides thin films obtained at 1200°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 400°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 600°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of of vanadium oxides thin films obtained at 300°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxide thin films obtained at 100°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 150°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 200°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
The AFM micrographs of vanadium oxides thin films obtained at 450°C
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on quartz glass and silicon substrate and vanadium thin films were obtained by annealing as-prepared...
-
Proteomics
Dane BadawczeWiff and Wiff2 files for shotgun proteomics analysis of E. coli strains (5 different strains in 10 different files).
-
Structure evolution of V2O5 thin films deposited on quartz glass substrate - High-Temperature X-ray Diffraction
Dane BadawczeThe DataSet contains the XRD patterns of V2O5 thin films deposited on guartz glass. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on the quartz glass substrate. The structure was measured in-situ during heating between 50-800°C under synthetic...
-
Structure evolution of V2O5 thin films deposited on silicon substrate - High-Temperature X-ray Diffraction
Dane BadawczeThe DataSet contains the XRD patterns of V2O5 thin films deposited on silicon substrates (111). The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The sol was deposited on the silicon substrate. The structure was measured in-situ during heating between 50-800°C under...
-
Powder x-ray diffraction pattern of polycrystalline synthetic leningradite, PbCu3V2O8Cl2
Dane BadawczePolycrystalline sample of Cu2+ (S=1/2) antiferromagnetic PbCu3V2O8Cl2 (synthetic analogue of the mineral leningradite) was prepared by solid state reaction of PbCl2, CuO, and V2O5.
-
XRD patterns of V2O5 thin films deposited on isotropic etching silicon substrates (111)
Dane BadawczeThe DataSet contains the XRD patterns of V2O5 thin films deposited on isotropic etching silicon substrates (111). The silicon wafers were etched in a mixture of nitric acid, hydrofluoric acid, and acetic acid in the ratio of 40:1:15. The soaking time for the substrates was from 30 to 90 seconds. The thin films were obtained by the sol-gel method. ...
-
Luminescence properties of TeOx thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. The sol was obtained by vigorously stirring precursor solution at 50°C for 2h, then the temperature was raised...
-
Luminescence properties of TeOx-Eu thin films
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Eu thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of europium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Tb thin films
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Tb thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of terbium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Dy thin films
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of dysprosium ions were added, the nitrates were used as a source of rare-earth ions....
-
SEM micrographs of V2O5 thin films deposited on isotropic etching silicon substrates (111)
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of V2O5 thin films deposited on isotropic etching silicon substrates (111). The silicon wafers were etched in a mixture of nitric acid, hydrofluoric acid, and acetic acid in the ratio of 40:1:15. The soaking time for the substrates was from 30 to 90 seconds. The thin films were...
-
Luminescence properties of TeOx gels
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx gels. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. The sol was obtained by vigorously stirring precursor solution at 50°C for 2h, then the temperature was raised...
-
The AFM micrographs of V2O5 single crystals
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of V2O5 single crystals. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The As-prepared films were deposited on a quartz glass substrate and were annealing at 600°C under synthetic air.
-
SEM analysis of the TiO2 layers deposited on a FTO substrates
Dane BadawczeTitanium dioxide layers were deposited on a FTO conducting glass by sol-gel method. For sol gel synthesis butoxy titanium and ethanol were used as a reagents. Samples were sintered in a furnace at temperature of 600 deg. SEM measurements were performed by FEI Quanta FEG250 microscope. SEM images of a cross-section of samples exhibit a porous structures...
-
Luminescence properties of TeOx-Dy thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of dysprosium ions were added, the nitrates were used as a source of rare-earth ions....
-
Luminescence properties of TeOx-Tb thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Tb thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of terbium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
Luminescence properties of TeOx-Eu thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-Eu thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of europium ions were added, the nitrates were used as a source of rare-earth ions. The...
-
XPS study of the NH4-VOx powders
Dane BadawczeVanadium pentoxide samples were prepared by sol-gel method. The starting solution was prepared by mixing vanadium (V) oxytripropoxide (Aldrich) in an anhydrous ethanol as solvent and acetylacetone. By drying the sol at 323 K for 48 h, it transforms via gel into a xerogel powder. Next, the precursor powder was pressed into the disk-shaped pellets. Samples...
-
The AFM micrographs of vanadium oxides thin films deposited on quartz glass - the influence of the thickness of the thin film on its morphology
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a quartz glass substrate and were...
-
The AFM micrographs of vanadium oxides thin films deposited on silicon - the influence of the thickness of the film on morphology
Dane BadawczeThe DataSet contains the atomic force microscope images of the surface of vanadium oxide thin films. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (1, 2 or 3 AsP layers) were deposited on a silicon substrate and were annealing...
-
XRD patterns of vanadium oxide nanostructures on silicon substrate obtained by V2O5 recrystallization
Dane BadawczeThe DataSet contains the XRD patterns of vanadium oxide nanostructures on silicon substrates obtained by recrystallization of V2O5 thin films between 800-1200°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
XRD patterns of VO2 and V2O3 thin films obtained at 500°C
Dane BadawczeThe DataSet contains the XRD patterns of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (3-9 AsP layers) were deposited on a silicon substrate and were annealing at 500°C under an argon atmosphere.
-
XRD patterns of vanadium oxide nanostructures on quartz glass substrate obtained by V2O5 recrystallization
Dane BadawczeThe DataSet contains the XRD patterns of vanadium oxide nanostructures on quartz glass substrates obtained by recrystallization of V2O5 thin films between 800-1200°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
Chemical composition of V2O5 nanorods
Dane BadawczeThe DataSet contains the chemical compositions of the V2O5 nanorods on a silicon substrate. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The As-prepared thin films were annealed at 600C under a synthetic air atmosphere.
-
XRD patterns of VO2 and V2O3 thin films obtained at 700°C
Dane BadawczeThe DataSet contains the XRD patterns of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films with different thicknesses (5-9 AsP layers) were deposited on a silicon substrate and were annealing at 700°C under an argon atmosphere.
-
Overproduction of CaMet15p native and His-tag versions.
Dane BadawczeEnzyme of fungal L-methionine biosynthetic pathway: O-acetylhomoserine sulfhydrylase (Met15p) could be exploited as molecular target for antifungal chemotherapy. The goal of the study was to obtain conditions optimal for protein production with the use of prokaryotic cells. The constructed expression plasmids, designed in three different versions: encoding...
-
Overproduction of CaStr2p native and His-tag versions.
Dane BadawczeEnzyme of fungal L-methionine biosynthetic pathway: cystathionine-γ-synthase (CaStr2p) could be exploited as molecular target for antifungal chemotherapy. The goal of the study was to obtain conditions optimal for protein production with the use of prokaryotic cells. The constructed expression plasmids, designed in three different versions: encoding...
-
Overproduction of homoserine O-acetyltransferase (CaMet2p) native and His-tag versions.
Dane BadawczeEnzyme of fungal L-methionine biosynthetic pathway: homoserine O-acetyltransferase (Met2p) could be exploited as molecular target for antifungal chemotherapy. The goal of the study was to obtain conditions optimal for protein production with the use of prokaryotic cells. The constructed expression plasmids, designed in three different versions: encoding...
-
X-Ray photoemission spectroscopy measurements of the Nb-V-Sr-O ceramics
Dane BadawczeNiobium doped strontium vanadate based perovskite SrV1-xNbxO3-δ materials were prepared via conventional solid state reaction (SSR) method. For comparison, different samples with a various amount of niobium dopant in the structure were synthesized; x = 0; 0,2; 0,5; 0,8 and 1. Samples were sintered by two-steps: first under a pure hydrogen (purity >99.999%)...
-
Chemical composition analysis of the LSNO ceramics
Dane BadawczeThe chemical composition of a series of La-Sb-Nb-O ceramics manufactured by the solid-phase reaction method was analyzed. The samples with a various antimony content were measured by XPS method (OmicronNanotechnology UHV system). Analysis confirmed presence of elements: La, Sb, Nb.
-
Luminescence properties of TeOx-2%Eu1.5%Tb1.5%Dy thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-2%Eu1.5%Tb1.5%Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of rare-earth ions were added, the nitrates were used as a source of rare-earth...
-
Luminescence properties of TeOx-2%Eu1.5%Tb1.5%Tm thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-2%Eu1.5%Tb1.5%Tm thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of rare-earth ions were added, the nitrates were used as a source of rare-earth...
-
Luminescence properties of TeOx-1%Eu1.5%Tb2.5%Dy thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx-1%Eu1.5%Tb2.5%Dy thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. Next, the 5% mol of rare-earth ions were added, the nitrates were used as a source of rare-earth...
-
SEM micrographs of morphology evolution of VO2 and V2O3 thin films obtained at 1000°C
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of VO2 and V2O3 thin films obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials. The thin films were deposited on a silicon and quartz glass substrate and were annealing at 1000°C under an argon atmosphere.
-
SEM micrographs of vanadium oxide nanostructures obtained by V2O5 recrystallization at 1000°C
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of vanadium oxide nanostructures on quartz glass and silicon substrates obtained by recrystallization of V2O5 thin films at 1000°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
SEM micrographs of vanadium oxide nanostructures obtained by V2O5 recrystallization at 800°C
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of vanadium oxide nanostructures on quartz glass and silicon substrates obtained by recrystallization of V2O5 thin films at 800°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.
-
SEM micrographs of vanadium oxide nanostructures obtained by V2O5 recrystallization at 1200°C
Dane BadawczeThe DataSet contains the scanning electron microscopy (SEM) micrographs of vanadium oxide nanostructures on quartz glass and silicon substrates obtained by recrystallization of V2O5 thin films at 1200°C under synthetic air. The thin films were obtained by the sol-gel method. The information about sol synthesis is described in the Journal of Nanomaterials.