PublikacjaContext. The global context of making numerous data produced by researchers available requires collecting and organising the data, assigning meaningful metadata, and presenting the data in a meaningful and homogeneous way. The BASECOL database, which collects inelastic rate coefficients for application to the interstellar medium and to circumstellar and cometary atmospheres, meets those requirements. Aims. We aim to present the...
-
Electrochemical impedance spectroscopy measurements - conductivity vs. temperature and conductivity vs. oxygen partial pressure - BaCe0.6Zr0.2Y0.1Tb0.1O3-δ
Dane BadawczeThe dataset consists of two main catalogs consisting of measurement data: of the electrical conductivity of the BaCe0.6Zr0.2Y0.1Tb0.1O3-δ (BCZYTb) sample as a function of temperature and of the electrical conductivity as a function of oxygen partial pressure (pO2). Measurements as a function of temperature were carried out in dry and wet air (pH2O ~...
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Linear impedance of 25Na2O–20CaO–5P2O5–50SiO2 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 25Na2O–20CaO–5P2O5–50SiO2 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
Linear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 30Bi2VO5.5-70SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 30Bi2VO5.5-70SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass measured with impedance spectroscopy method
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Dirac fermions and possible weak antilocalization in LaCuSb2
PublikacjaLayered heavy-metal square-lattice compounds have recently emerged as potential Dirac fermion materials due to bonding within those sublattices. We report quantum transport and spectroscopic data on the layered Sb square-lattice material LaCuSb2. Linearly dispersing band crossings, necessary to generate Dirac fermions, are experimentally observed in the electronic band structure observed using angle-resolved photoemission spectroscopy,...
-
CeIr3: superconductivity in a phase based on tetragonally close packed clusters
PublikacjaWe present the crystallographic analysis, superconducting and spectroscopic characterization, and theoretical modeling of CeIr3. Lattice parameters a = 5.2945(1) Å and c = 26.219(1) Å are found for the R-3m symmetry crystal structure, which are close to the literature values. CeIr3 is a moderate type-II superconductor (κ GL = 17, λ e–p = 0.65) below 2.5 K. Ce ions exhibit a strongly intermediate valence character as evidenced by...
-
Implementation of SiN thin film in fiber-optic sensor working in telecommunication range of wavelengths
PublikacjaMirrors are used in optical sensors and measurement setups. This creates a demand for mirrors made of new materials and having various properties tailored to specific applications. In this work, we propose silicon covered with a thin silicon nitride layer as a mirror for near-infrared measurements. SiN layer was deposited on a standard silicon wafer with a Low-Pressure Chemical Vapor Deposition furnace. Then, the created layer...
-
SnO2 nanoparticles embedded onto MoS2 nanoflakes - An efficient catalyst for photodegradation of methylene blue and photoreduction of hexavalent chromium
PublikacjaIn this work, a molybdenum disulfide/tin oxide (MoS2/SnO2) composite was successfully prepared via a hydrothermal method. The MoS2/SnO2 composite was used as a photocatalyst for photoreduction of hexavalent chromium and photodecomposition of methylene blue. It exhibited higher photocatalytic performance under simulated solar light irradiation than MoS2 itself. The obtained material was characterized by several spectroscopic and...
-
Absorption and fluorescence spectrum the Diamond™ nucleic acid dye applied to DNA and friction ridge analysis from fingerprint traces
Dane BadawczeThe results of a study of the spectroscopic properties of Diamond™ dye binding to reference DNA and to DNA from a fingerprint using a UV/VIs spectrophotometer and a spectrofluorimeter are presented.
-
The voltage across and current through the RC model object tested using pulse excitation in impedance spectroscopy measurement method
Dane BadawczeThe raw data (voltage across and current through RC model object ) obtained using pulse excitation EIS impedance spectroscopy measurement method. The data was acquired using 12-bit ADC (LTC1420) with sampling frequency changed in time segments. The 1V voltage pulse excitation duration was set to 0.1s and the total acqusition time was set to 1000s. For...
-
Influence of sintering temperature of porous SrTi0.30Fe0.70O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperatures
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.30Fe0.70O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Influence of sintering temperature of porous SrTi0.50Fe0.50O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Influence of sintering temperature of porous SrTi0.65Fe0.35O3-d oxygen electrode on electrochemical impedance spectroscopy spectra measured at 800 °C
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.65Fe0.35O3-d oxygen electrodes sintered at different temperatures (800 °C; 900 °C and 1000 °C). Measure temperature was 800 °C (syntetic air, 40 ml min-1). Results converted to electrode surfaces area and dived by two electrodes.
-
Electrochemical impedance spectroscopy spectra measured at 700 °C on porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperatures
Dane BadawczeThis dataset contains results electrochemica impedance spectroscopy (EIS) of symmetrical cells with porous SrTi0.50Fe0.50O3-d oxygen electrodes sintered at different temperaturs (800 °C, 900 °C and 1000 °C). EIS spectra were measured at 700 °C with synthetic air flow (21% O2, 40 ml min-1). Results converted to electrode surfaces area and dived by two...
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K was measured by impedance spectroscopy method.
-
Linear impedance of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 2Si3N4–98(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 0.5Si3N4–99.5(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 annealed glass was measured by impedance spectroscopy method.
-
Linear impedance of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 1Si3N4–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Linear impedance of 1SiO2–99(40Na2O-20CaO-40P2O5) glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 1SiO2–99(40Na2O-20CaO-40P2O5) glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 593 K was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Synthesis of Phosphonated Carbon Nanotubes: New Insight into Carbon Nanotubes Functionalization
PublikacjaCarbon nanotubes were successfully functionalized for the first time in a free radical phosphonylation reaction. Three synthetic protocols were proposed. Carbon nanotubes and diethylphosphite reacted in the presence of known radical initiator, such as azobisisobutyronitrile, single electron oxidant—Mn(OAc)3, or under UV radiation. The functionalized material was fully characterized by means of spectroscopic methods, together with...
-
Reduced Graphene Oxide Joins Graphene Oxide To Teach Undergraduate Students Core Chemistry and Nanotechnology Concepts
PublikacjaNovel carbon nanomaterials such as reduced graphene oxide (rGO) and graphene oxide (GO) can be easily incorporated into the undergraduate curriculum to discuss basic chemistry and nanotechnology concepts. This paper describes a laboratory experiment designed to study the differences between GO and rGO regarding their physico-chemical properties (e.g. color, hydrophobicity, type of functional groups, electrical conductivity etc.)....
-
The influence of reactions conditions on aggregation of dyes used in biochemistry
PublikacjaSelf-association of dyes and related substances is a very important phenomenon in many fields of applied chemistry. It is also fundamental model reaction of many kinds of molecular interactions such as the micelle formation of amphiphilic substances and the binding of small organic molecules to macromolecules. In spite of many studies concerning the dimerization equilibria of dyes and related substances, the mechanism seems not...
-
Simultaneous opto-electrochemical monitoring of carbamazepine and its electro-oxidation by-products in wastewater
PublikacjaThe growing human impact on aquatic environments, due to the extensive use of pharmaceuticals and the release of persistent pollutants, makes it necessary to implement new widespread methods for the characterisation and quantification of such contaminants and relative degradation products. Carbamazepine, 5H-dibenzo[b,f]azepine-5-carboxamide, (CBZ) is a widely used anti-epileptic drug, characterised by its limited removal by conventional...
-
Maciej Jerzy Głowacki
OsobyMaciej Jerzy Głowacki jest absolwentem Politechniki Gdańskiej. Ukończył z wyróżnieniem studia inżynierskie na Wydziale Mechanicznym (2017) oraz studia magisterskie na Wydziale Elektroniki, Telekomunikacji i Informatyki (2018). Od 2014 roku jest nieprzerwanie zaangażowany w działalność badawczą prowadzoną w Katedrze Metrologii i Optoelektroniki. W pracy naukowej zajmował się m. in. nanoszeniem antybakteryjnych powłok hydroksyapatytowych...
-
Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 2.88 mm was measured at 693 K with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched glass 40Bi2VO5.5-60SrB4O7 after full crystallization was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of as-quenched glass 40Bi2VO5.5-60SrB4O7 afetr full crystallization was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of frequency for Bi2VO5.5 ceramic of thickness 2.88 mm was measured at high temperature range with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 fully crystallized glass at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 partially crystallized glass at 613 K measured with impedance spectroscopy method at high temperature region