displaying 1000 best results Help
Search results for: thermal degradation kinetics
-
Polyurethane/Silane-Functionalized ZrO2 Nanocomposite Powder Coatings: Thermal Degradation Kinetics
PublicationA polyurethane (PU)-based powder coating reinforced with vinyltrimethoxysilane (VTMS)-functionalized ZrO2 nanoparticles (V-ZrO2) for thermal stability was developed. Chemical structure, microstructure and thermal degradation kinetics of the prepared coatings were investigated. The peak of aliphatic C–H vibrating bond in the Fourier transform infrared (FTIR) spectrum of V-ZrO2 was a signature of VTMS attachment. Scanning electron...
-
Thermal degradation kinetics of poly(propylene succinate) prepared with the use of natural origin monomers
PublicationLinear biobased polyester polyols were prepared with the use of succinic acid and 1,3-pro- panediol (both with natural origin). Tetraisopropyl orthotitanate (TPT) was used as a catalyst. In order to determine the effect of various synthesis temperature conditions on the thermal degradation kinet- ics, nine sequences of temperature conditions were used during two-step polycondensation reaction. Thermogravimetric analysis was conducted...
-
Recycled Polyurethane as a Second Phase in Thermoset Blends and Its Effect on Thermal Degradation Kinetics Studies
PublicationA new approach is introduced in the modification of thermosetting polymer by using different amount of polyurethane of waste origin. The post consumer polyurethane foam coatings are degraded using glycolysis process and the recycled product is further converted into new polyurethane. The blending of recycled polyurethane with epoxy exhibits transparency and produces nanostructures. The effective interaction between two polymers...
-
Fully bio-based poly(propylene succinate) synthesis and investigation of thermal degradation kinetics with released gases analysis
PublicationOne of the most important information about polyesters is their thermal stability and phase transition tem- peratures. These characteristics give information about the promising behavior of the polyester during proces- sing. In this work, linear bio-based polyester polyols were prepared with the use of succinic acid and 1.3- propanediol (both with natural origin). As a polycondensation catalyst was used tetraisopropyl orthotitanate...
-
Thermal-Resistant Polyurethane/Nanoclay Powder Coatings: Degradation Kinetics Study
PublicationIn the present study, thermal degradation kinetics of polyurethane (PU) powder coatings reinforced with organo-modified montmorillonite (OMMT) was investigated. PU nanocomposites were prepared in different concentrations of 1, 3, and 5 wt.% of OMMT via the extrusion method. The microstructure of the nanocomposites was observed by scanning electron microscope (SEM) illustrating uniform dispersion of OMMT nano-clay platelets in the...
-
Bio based PUR-PIR foams thermal degradation (TG) and isoconversional kinetics
Open Research DataIn the present work, we perform a thorough thermogravimetric (TG) analysis of the bio-based polyurethane – polyisocyanurate (PUR-PIR) foams in both nitrogen and oxygen atmosphere. A sustainable element of the foam was a biopolyol obtained via acid-catalyzed liquefaction of Zostera Marina and Enteromorpha Algae biomass. Based on isoconversional analysis...
-
Phototransformation of Amlodipine: Degradation Kinetics and Identification of Its Photoproducts
PublicationNowadays, monitoring focuses on the primary compounds and does not include degradation products formed during various biological and chemical processes. Transformation products may have the same effects to human health and the environment or sometimes they can be more toxic than the parent compound. Unfortunately, knowledge about the formation of degradation products is still limited, however, can be very important for the environmental...
-
Degradation kinetics and mechanism of pentoxifylline by ultraviolet activated peroxydisulfate
PublicationDegradation of pentoxifylline (PTX) by sodium peroxydisulfate (SPDS) assisted by UV irradiation has been investigated in deionized water. The treatment was more favorable over direct photolysis or peroxydisulfate oxidation alone. The effects of various parameters, including different dosage of oxidant agent, PTX concentration, initial solution pH levels, and the presence of inorganic ions like chloride, nitrate and carbonate have...
-
Thermal degradation of poly(alkyl methacrylates)
Publication -
Thermal degradation of copolymers based on selected alkyl methacrylates
Publication -
Understanding the kinetics and atmospheric degradation mechanism of chlorotrifluoroethylene (CF2=CFCl) initiated by OH radicals
PublicationThe atmospheric degradation of chlorotrifluoroethylene (CTFE) by OH˙ was investigated using density functional theory (DFT). The potential energy surfaces were also defined in terms of single-point energies derived from the linked cluster CCSD(T) theory. With an energy barrier of −2.62 to −0.99 kcal mol−1 using the M06-2x method, the negative temperature dependence was determined. The OH˙ attack on Cα and Cβ atoms (labeled pathways...
-
The impact of addition of olive oil on thermal degradation of refined rapeseed oil
PublicationFats are an important component of the everyday diet and have a significant impact on the proper functioning of human organism. However, during the process of frying chemical transformations take place in the oil; hence fats characterised by high oxidative stability should be given preference. The aim of this work was to determine the quality of rapeseed oil, blended oil, and refined olive oil, all sourced from the domestic market....
-
Thermal degradation of butyl acrylate-methyl acrylate-acrylic acid-copolymers
Publication -
Thermal degradation of poly(alkyl methacrylates) and polyurethane pressure-sensitive adhesives
Publication -
Kinetics of the photosensitized degradation of benzyl 4-hydroxybenzoate in homogeneous aqueous solution under visible-light irradiation
Publication -
Isothermal Vulcanization and Non-Isothermal Degradation Kinetics of XNBR/Epoxy/XNBR-g-Halloysite Nanotubes (HNT) Nanocomposites
PublicationThe effect of several concentrations of carboxylated nitrile butadiene rubber (XNBR) functionalized halloysite nanotubes (XHNTs) on the vulcanization and degradation kinetics of XNBR/epoxy compounds were evaluated using experimental and theoretical methods. The isothermal vulcanization kinetics were studied at various temperatures by rheometry and differential scanning calorimetry (DSC). The results obtained indicated that the...
-
Thermal degradation of polylactic acid (PLA)/polyhydroxybutyrate (PHB) blends: A systematic review
PublicationPolylactic acid (PLA) and polyhydroxybutyrate (PHB) are two biopolyesters obtained from renewable resources like corn or sugar under bacterial fermentation. PLA is the most widely used biopolymer in diverse applications. Addition of PHB to PLA can improves the crystallinity of PLA, and thereby its mechanical strength. However, both PLA and PHB suffer from poor thermal stability, which limits their potential industrial application....
-
Thermal stability and degradation of selected poly(alkyl methacrylates) used in the polymer industry
Publication -
Application of Microextraction Techniques Including SPME and MESI to the Thermal Degradation of Polymers: A Review
Publication -
Enhancement of PUR/PIR foam thermal stability after addition of Zostera marina biomass component investigated via thermal analysis and isoconversional kinetics
PublicationIn the present work, a thorough thermogravimetric (TG) analysis of bio-based polyurethane–polyisocyanurate (PUR–PIR) foams in both nitrogen and oxygen atmosphere is performed. A sustainable element of the foam is a biopolyol obtained via acid-catalyzed liquefaction of Zostera marina and Enteromorpha Algae biomass. Based on isoconversional analysis and apparent activation energies, several conclusions are obtained. In contradiction...