TG analyses - content of SiO2 and TiO2 in polystyrene
Dane BadawczeTG analyses were performed for polystyrene spheres coating by SiO2 and then coating by SiO2-TiO2. Thermal analyses of polystyrene spheres only were also performed. The content of inorganic remaining was used for calculation the quantity of coating SiO2 and TiO2 in the polystyrene spheres.
-
SEM micrographs of the austenitic stainless steel corrosion in asphalt fumes
Dane BadawczeThe dataset contains the scanning electron microscopy (SEM) studies of the austenitic stainless steels: AISI 304, AISI 316, AISI 321 and duplex stainless steel AISI 2205. The samples were polished and exposed to the installation carrying asphalt fumes at elevated temperatures (approx. ~210-240 Celsius). The exposition duration was three months. Some...
-
Investigation of temperature changes using a microsphere-based fiber-optic sensor
Dane BadawczeInvestigation of temperature changes using a microsphere-based fiber-optic sensor with a 200 nm ZnO ALD coating for the purpose of validation the design of the sensor, measurement setup and method of examination of electric cell materials.
-
Application of optical microsphere in fiber optic sensors for measurement of electrochemical processes
Dane Badawczeinvestigation of the electrochemical processes using micro-sphere fiber-optic sensor with a zinc oxide (ZnO) coating applied by Atomic Layer Deposition method (ALD). The measurements were performed in 1M KNO3 during a decomposition of Bisphenol-A
-
The electrochemical impedance spectroscopy studies of cataphoretic-grown epoxy-based coatings
Dane BadawczeThe dataset contains electrochemical impedance spectroscopy spectra collected for epoxy-based cataphoretic coatings in order to determine the offered anti-corrosion protection. Particular spectra pertain to the coatings applied for the different magnitude of polarization potential imposed, namely 10V, 20V and 30V. The results were obtained within the...
-
Flow cytometry analysis of DNA DSBs in telomerase positive and negative cell lines after treatment with TXT2 and TXT4
Dane BadawczeFlow cytometry analysis of DNA DSBs in telomerase positive (A549, H460) and negative (NHBE2594, U2OS) cell lines after treatment with equitoxic concentrations of TXT2 and TXT4. MTX and DMSO were used as positive and negative controls, respectively.
-
Depth XPS profile of vanadium pentoxide
Dane BadawczeVanadium pentoxide sample was manufactured by sol-gel method and deposited on a substrate by spin coating technique. To determine depth profile of chemical composition of thin film, etching by Argon ion gun was used. Thin film was etched three times. Chemical composition was measured by XPS method.
-
Impedance spectroscopy of the lithium titanate doped by copper thin films
Dane BadawczeLithium titanate doped by copper thin films were derived by sol-gel method. Prepared gel was deposited by spin-coating technique. Samples with various content of Cu were measured by impedance spectroscopy method in a wide range of temperature, from -120 up to 150 deg.
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.5
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.4
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - microsphere inspection s.3
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
The influence of external interference on AFM imaging, the use of a protective helmet
Dane BadawczeThis collection is of purely practical importance, showing how the presence of external disturbances can adversely affect the quality of imaging with an atomic force microscope. For this reason, it is also advisable to provide a link to a workshop-like study [1] as well as a huge number of commercial solutions available after entering the keyword "AFM...
-
Microstructure of cross-sections of samples after laser treatment for the article entitled "Mechanical and corrosive properties of Ti13Nb13Zr alloy subjected to laser treatment with MWCNTs coatings"
Dane Badawcze -
Photocatalytic decomposition of ethylene on the TiO2-polystyrene spheres
Dane BadawczeData contain results from the measurements of the photocatalytic decomposition of ethylene under UV irradiation with using TiO2 coating on the expanded polystyrene spheres (EPS). EPS-SiO2-TiO2 and EPS-TiO2 were used as the photocatalytic beds in the fluidized bed reactor. Both, stationary and fluidized beds were tested. The comparison of ethylene decomposition...
-
Fuel cell noise data
Dane BadawczeMeasurement data of Hydrogen PEM fuel cels. The voltage fluctuations were measured over single cels of stack of 10 cels.
-
SEM micrographs of the topography of Cu-Sn-TiO2 nanocomposite coatings
Dane BadawczeThe dataset contains the scanning electron microscopy (SEM) micrographs of nanocomposite Cu-Sn-TiO2 coatings electrodeposited from oxalic acid bath containing Cu and Sn salts as well as TiO2 nanoparticles under various treatments: mechanical stirring, ultrasonic or none. The details of the electrodeposition process are presented in the readme file attached...
-
BET specific surface area measurements of silica-coated bismuth oxide (Bi2O3)/gadolinium oxide (Gd2O3) core-shell structures
Dane BadawczeThe BET specific surface area was measured using an N2 adsorption/desorption isotherm (Micromeritics ASAP 2460, Norcross, GA, USA).
-
A novel method for drop in drop edible oils encapsulation with chitosan using a coaxial technique
Dane BadawczeThe dataset present a novel one step method for oil encapsulation. In this coaxial system the oil constitutes the core of the capsule, while the chitosan solution is the polymer shell surrounding the core to provide separation of the core from the external environment. In comparison to other encapsulation methods, the presented technique is much simpler...
-
Experimental data of galvanic electric cells measurements
Dane BadawczeInternal temperature of an electric cell can be measured and monitored using microsphere-based fiber-optic sensors with thin ALD ZnO coating. Their compact size will allow to integrate them easily and effectively within the electric cells. Utilization of presented sensors allows to detect, in real time, damages to the structure of the sensor head that...
-
Optical Parameters Stability Over Time of Porous Phantoms Mimicking Tissues
Dane BadawczeOptical phantoms are used to validate optical measurement methods. The stability of their optical parameters over time allows them to be used and stored over long-term periods while maintaining their optical parameters. The aim of the presented research was to investigate the stability of fabricated porous phantoms, which can be used as a lung phantom...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 200 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 100 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated (100 nm) microsphere-based fiber-optic sensor - 300 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 100 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Initial geometries and MD trajectories of right- and left-handed G-quadruplexes
Dane BadawczeDataset contains initial geometries of 12 monomeric, 2-tetrad G-quadruplexes featuring three different loop lengths (T1, T2 and T3), adapted by the sequence GGTnGGTnGGTnGG where n=(1-3). For each loop length variant two directions of strand progression (clockwise (+) and anti-clockwise (-)) and two helicities (left-handed (LH) and right-handed (RH))...
-
XPS measurements of the iron elements covered by chromium
Dane BadawczeAnticorrosive coatings are an important issue in modern materials engineering. One of the most commonly used, for that coating materials, is chrome. Three metal elements were measured, named as Turcja, WB Tech and Nomet. Names were given according to producer of elements. XPS measurements of the Cr 2p region give an ansver concering on surface chemical...
-
The XPS studies revealing the surface chemistry of Cu-Sn-TiO2 nanocomposite coatings
Dane BadawczeThe dataset contains the X-Ray Photoelectron Spectroscopy (XPS) data of nanocomposite Cu-Sn-TiO2 coatings electrodeposited from oxalic acid bath containing Cu and Sn salts as well as TiO2 nanoparticles under various treatments: mechanical stirring, ultrasonic or none. The details of the electrodeposition process are presented in the descriptor file...
-
Impact of binary mixtures of Irgasan (triclosan) and Diclofenac on endocrine processes of the model organism Saccharomyces Cerevisiae (using XenoScreen YES/YAS test)
Dane BadawczeThe XenoScreen YES/YAS reagents and methodology is given in Kudłak et al. (2019) and in details in electronic supplementary material.
-
Impact of binary mixtures of diclofenac and on endocrine processes of the model organism Saccharomyces Cerevisiae (using XenoScreen YES/YAS test)
Dane BadawczeData shown in data set highlighte the results of the edorin processes of the diclofenac sodium salt mixture with Methylparaben. S cerevisiae is used as a model organism in the monitoring of endocrine disruptors in environmental and reference samples in Xenometrix® systems - XenoScreen®. Methylparaben have fungicide properties used in food preservative,...
-
Impedance spectra of RC model as a result of testing pulse excitation measurement method
Dane BadawczeThe impedance spectrum of RC model object obtained using pulse excitation EIS impedance spectrosocpy measurement method. The 1V voltage pulse excitation duration was set to 0.1s and the total acqusition time was set to 1000s. The object under test was built using RC components connected as Baunier model of anticorrosion coating with the following components...
-
Integrated circuit structure surface images obtained with contact capacitive imaging technique
Dane BadawczeThe measurements were done using NTEGRA Prima (NT-MDT) device. CSG 10Pt probe.
-
Luminescence properties of TeOx thin films annealing under an oxidizing atmosphere
Dane BadawczeThe DataSet contains the emission and excitation spectra of TeOx thin films. The material was obtained by the sol-gel method. The starting solution was prepared by mixing telluric acid (precursor) with thetraetylene glycol, water, and ethanol. The sol was obtained by vigorously stirring precursor solution at 50°C for 2h, then the temperature was raised...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 140 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 160 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 180 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 200 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-0optic sensor - 250 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 210 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 300 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 270 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 190 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 260 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 290 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
The voltage across and current through the RC model object tested using pulse excitation in impedance spectroscopy measurement method
Dane BadawczeThe raw data (voltage across and current through RC model object ) obtained using pulse excitation EIS impedance spectroscopy measurement method. The data was acquired using 12-bit ADC (LTC1420) with sampling frequency changed in time segments. The 1V voltage pulse excitation duration was set to 0.1s and the total acqusition time was set to 1000s. For...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 170 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 280 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 150 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 230 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 240 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...
-
Measurement spectrum obtained with the use of ZnO coated microsphere-based fiber-optic sensor - 220 Celsius degrees
Dane BadawczeApplication of a microsphere-based fiber-optic sensor with 200 nm zinc oxide (ZnO) coating, deposited by Atomic Layer Deposition (ALD) method, for temperature measurements between 100°C and 300°C, is presented. The main advantage of integrating a fiber-optic microsphere with a sensing device is the possibility of monitoring the integrity of the sensor...