Filtry
wszystkich: 14373
wybranych: 624
-
Katalog
- Publikacje 7238 wyników po odfiltrowaniu
- Czasopisma 14 wyników po odfiltrowaniu
- Wydawnictwa 6 wyników po odfiltrowaniu
- Osoby 854 wyników po odfiltrowaniu
- Wynalazki 70 wyników po odfiltrowaniu
- Projekty 106 wyników po odfiltrowaniu
- Laboratoria 5 wyników po odfiltrowaniu
- Zespoły Badawcze 47 wyników po odfiltrowaniu
- Aparatura Badawcza 7 wyników po odfiltrowaniu
- Kursy Online 3427 wyników po odfiltrowaniu
- Wydarzenia 106 wyników po odfiltrowaniu
- Dane Badawcze 2493 wyników po odfiltrowaniu
Filtry wybranego katalogu
Wyniki wyszukiwania dla: JAN PAWEŁ II
-
Conley-Morse graphs for a population model with harvesting. Case Ha-S1: Harvesting adults only, survival rates of juveniles and adults add up to 1
Dane BadawczeThis dataset contains selected results of rigorous numerical computations conducted in the framework of the research described in the paper "Global dynamics in a stage-structured discrete population model with harvesting" by E. Liz and P. Pilarczyk: Journal of Theoretical Biology, Vol. 297 (2012), pp. 148–165, doi: 10.1016/j.jtbi.2011.12.012.
-
Conley-Morse graphs for a population model with harvesting. Case Ha-Se: Harvesting adults only, equal survival rates of juveniles and adults
Dane BadawczeThis dataset contains selected results of rigorous numerical computations conducted in the framework of the research described in the paper "Global dynamics in a stage-structured discrete population model with harvesting" by E. Liz and P. Pilarczyk: Journal of Theoretical Biology, Vol. 297 (2012), pp. 148–165, doi: 10.1016/j.jtbi.2011.12.012.
-
Results of experimental research of hydraulic satellite motor
Dane BadawczeThe study of the flow rate in the motor and the torque on the motor shaft at low constant speed were carried out.The file contains measurement data of the torque on the motor shaft and the flow rate in the motor as a function of the angle of shaft rotation at various constant pressure drops in the motor.
-
A New Adaptive Method for the Extraction of Steel Design Structures from an Integrated Point Cloud
Dane BadawczeA new automatic and adaptive algorithm for edge extraction from a random point cloud was developed and presented herein. The proposed algorithm was tested using real measurement data. The developed algorithm is able to realistically reduce the amount of redundant data and correctly extract stable edges representing the geometric structures of a studied...
-
Calibration images under different lighting conditions - static for feature localisation
Dane BadawczeDataset description: Calibration images under different lighting conditions - static mode for feature detection
-
Terrestrial Laser Scan and Survey Images - 3D Model - Palm House - MP1 - Leica
Dane BadawczeDataset description: Raw images from photogrammetric and terresttial laser scaning survey. Object: Palm House in Gdansk Oliwa ParkLocation: Gdansk, Pomorskie, PolandDrone type: DJI Mavic Pro 1Flight plan: Circle | Point Of InterestTarget Product: 3D ModelDate: 06.11.2018Direct georeferencing: yesMetadata data: Yes/GPSGCP: NoCamera Name: DJI FC220Lasser...
-
Collective angst and collective action for progressive city policies: study2
Dane BadawczePaweł Adamowicz, the liberal mayor of Gdańsk, died on January 14, 2019, after being stabbed by a man who rushed onstage during a charity event. Three studies were carried out to analyze the predictors of willingness to engage in collective action for the support of the progressive city policies he initiated. Since we assumed that the time after the...
-
Frequency Response Functions for Sandvik CoroBore 825 XL boring tool, 733 mm
Dane BadawczeFrequency Response Functions (FRF) obtained for Sandvik CoroBore® 825 XL mounted at WHN 13-15 TOS VARNSDORF CNC machine at the minimum extension of the spindle adaptor. Tool set to bore a hole with a diameter 733mm
-
Nonlinear impedance as a function of A.C. voltage for glass 40Bi2VO5.5-60SrB4O7 annealed at 473 K for 3h and next fully crystallized measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties as a function of A.C. voltage for annealed at 473 K for 3h and next fully crystallized 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear and nonlinear impedance of iron containing silicate glasses
Dane BadawczeThe linear and nonlinear impedance ofglasses doped with iron oxide were measured. Glass samples (50 SiO2-50-xPbO-xFe2O3 in mol%) were prepared by the conventional melt quenching technique. The substrates were powdered in a mortar and melted in Al2O3 crucibles. The melting was conducted in air at 1623K. The melts were poured out on plate heated up to...
-
Linear and nonlinear impedance of alkali and iron doped silicate-lead glasses
Dane BadawczeLinear and nonlinear impedance was studied for lead-silicate glass samples doped with iron ions and alkaline oxides. The compositions of glasses were as follows: (in %mol) 50% SiO2, 25% PbO, 15% Fe2O3 and 15% one of alkaline oxides: Na2O, K2O, Li2O. All samples were prepared by the conventional melt quenching technique. The substrates were powdered...
-
Electrical properties of lead-borate glasses and glass-ceramics containing iron ions
Dane BadawczeElectrical properties were studied for borate-lead glasses and glass-ceramics doped with iron ions. Glass samples of composition of xFe2O3–(100 − x)(B2O3–2PbO) (2.5 b x b 37, in mol%) were prepared by the conventional melt quenching technique. The melting was conducted in alumina crucibles at the temperature of 1523 K. The melts were poured on a preheated...
-
Nonlinear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Linear impedance of vanadate glasses containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Nonlinear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe nonlinear impedance of vanadate glasses doped with BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated (573...
-
Electrical properties of silicate-lead glasses containing nanostructures of iron oxides.
Dane BadawczeElectrical properties of silicate-lead glasses doped with different content of iron oxide was studied. The set of glass samples were prepared with the composition of (50 − 0.5x)SiO2–(50 − 0.5x)PbO–xFe2O3, where x = 2, 5, 10, 15, 20 and 25 (in mol%). All sampleswere prepared by the conventional melt quenching technique; the melting was conducted in...
-
Dielectric properties of barium-vanadate glasses
Dane BadawczeThe linear impedance of barium-vanadate glasses was measured. Samples of the composition of xBaO-(100-x)V2O5 where x= 30, 40 and 45 (in %mol) were prepared by the conventional melt quenching technique. Appropriate amounts of reagents: BaO (≥99.9%, P.P.H STANLAB Sp.J.) and V2O5 (≥99.9%, POCH) were thoroughly mixed in an agate mortar. The melting was...
-
Linear impedance of vanadate glass-ceramics containing BaTiO3
Dane BadawczeThe linear impedance of vanadate glass-ceramics containing BaTiO3 was measured. Samples of the composition of x[BaO,TiO2]–(80 − x)V2O5–20Bi2O3 where x = 5, 10 and 15 in mol% were prepared by a conventional melt quenching technique. The melting was performed in alumina crucibles at the temperature of 1273 K–1373 K. The melts were poured on a preheated...
-
Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 2.88 mm was measured at 693 K with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for fully crystallized 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties as a function of A.C. voltage for fully crystallized 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched Bi2VO5.5 glass-ceramic was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of as-quenched Bi2VO5.5 glass-ceramic was measured by impedance spectroscopy method.
-
Nonlinear impedance of 45Bi2VO5.5-55SrB4O7 fully crystallized glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 45Bi2VO5.5-55SrB4O7 fully crystallized glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of temperature and frequency for Bi2VO5.5 ceramic of thickness 2.52 mm was measured at different A.C. voltage with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties as a function of A.C. voltage for annealed and next fully crystallized 50Bi2VO5.5-50SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 glass-ceramic annealed at 423 K was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 glass-ceramic annealed at 423 K was measured by impedance spectroscopy method.
-
Linear impedance of as-quenched 40Bi2VO5.5-60SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated at 693 K was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic of thickness 2.88 mm measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic of thickness 2.88 mm was measured by impedance spectroscopy method.
-
Linear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(Bi2VO5.5)-50SrB4O7 glass was measured by impedance spectroscopy method.
-
D.C. electrical measurements of Bi2VO5.5 ceramic measured at high temperature region
Dane BadawczeD.C. electrical properties of Bi2VO5.5 ceramic was measured.
-
Linear impedance of strontium–borate glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of strontium–borate glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 1.63 mm was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 1.63 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of as-quenched glass 40Bi2VO5.5-60SrB4O7 after full crystallization was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of as-quenched glass 40Bi2VO5.5-60SrB4O7 afetr full crystallization was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 40Bi2VO5.5-60SrB4O7 annealed glass at 473 K for 3 h measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of 40Bi2VO5.5-60SrB4O7 glass annealed at 473 K for 3h was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic prepared by traditional melt quenching technique was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeNonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50(2Bi2O3-V2O5)-50SrB4O7 glass heat treated two times was measured by impedance spectroscopy method.
-
Linear impedance of 10Na2O–60P2O5–30CaO glass measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrical properties of 10Na2O–60P2O5–30CaO glass was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage for glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties as a function of A.C. voltage for annealed at 593 K and next fully crystallized 40Bi2VO5.5-60SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 3 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe nonlinear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 50Bi2VO5.5-50SrB4O7 annealed glass at 593 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 50Bi2VO5.5-50SrB4O7 annealed glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of 35Bi2VO5.5-65SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of 35Bi2VO5.5-65SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 5(2Bi2O3-V2O5)-95SrB4O7 glass measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties of 5(2Bi2O3-V2O5)-95SrB4O7 glass was measured by impedance spectroscopy method.
-
Linear impedance of 58(2Bi2O3-V2O5)-42SrB4O7 glass heat-treated for 10 hours at 693 K, measured with impedance spectroscopy method at low temperature region
Dane BadawczeThe linear electrcial properties of partially crystallized 58(2Bi2O3-V2O5)-42SrB4O7 glass was measured by impedance spectroscopy method.
-
Nonlinear impedance of glass 40Bi2VO5.5-60SrB4O7 annealed at 473 K for 3h and next fully crystallized was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrcial properties of glass 40Bi2VO5.5-60SrB4O7 annealed at 593 K and next fully crystallized was measured by impedance spectroscopy method.
-
Nonlinear impedance as a function of A.C. voltage of Bi2VO5.5 ceramic of thickness 4.03 mm was measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 4.03 mm was measured by impedance spectroscopy method.
-
Nonlinear impedance of Bi2VO5.5 ceramic of thickness 2.52 mm (after second heat-treatment at 913 K) was measured at high temperature range with impedance spectroscopy method
Dane BadawczeThe nonlinear electrical properties of Bi2VO5.5 ceramic of thickness 2.52 mm (after second heat-treatment at 913 K) was measured by impedance spectroscopy method.
-
Linear impedance as a function of A.C. voltage for 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat-treated at 813 K measured with impedance spectroscopy method at high temperature region
Dane BadawczeThe linear electrcial properties as a function of A.C. voltage of 50(2Bi2O3-V2O5)-50SrB4O7 glass-ceramic heat treated at 813 K was measured by impedance spectroscopy method.